The work reported in this study focusing on the abrasive wear behavior for three types of pipes used in oil industries (Carbone steel, Alloy steel and Stainless steel) using a wear apparatus for dry and wet tests, manufactured according to ASTM G65. Silica sand with
hardness (1000-1100) HV was used as abrasive material. The abrasive wear of these pipes has been measured experimentally by measuring the wear rate for each case under different sliding speeds, applied loads, and sand conditions (dry or wet). All tests have been conducted using sand of particle size (200-425) µm, ambient temperature of 34.5 °C and humidity 22% (Lab conditions).
The results show that the material loss due to abrasive wear increased monotonically with the applied load at constant sliding speed and constant grit size due to increasing depth of penetration in both dry and wet sand which agrees with Archard´s equation. Sliding speed show insignificant effect on the wear loss of metals at constant load and constant grit size in both dry and wet sand. Wet sand results show higher wear losses than dry sand (20-70) % due to micro abrasion – corrosion wear and high slurry concentration.
The investment government expenditure is considered the fundamental of enhancing the economic activity as it has become a mean for achieving capital accumulation in all economic sectors, The Iraqi economy is characterized of being yield unilateral depending petroleum revenues as an essential resource of financing government expenditure , as the contribution of petroleum sector in GDP is large in proportions to other economic sectors contribution.
The relationship between investing government expenditure, and non-oil GDP is about to be not existent during the
... Show MoreAn optoelectronic flow-through detector for active ingredients determination in pharmaceutical formulations is explained. Two consecutive compact photodetector’s devices operating according to light-emitting diodes-solar cells concept where the LEDs acting as a light source and solar cells for measuring the attenuated light of the incident light at 180˚ have been developed. The turbidimetric detector, fabricated of ten light-emitting diodes and five solar cells only, integrated with a glass flow cell has been easily adapted in flow injection analysis manifold system. For active ingredients determination, the developed detector was successfully utilized for the development and validation of an analytical method for warfarin determination
... Show MoreThe study entitled (Anthropometric Treatments of the Study Seat Units Used in Elementary stages) highlighted the relations between the sizes of dimensions of the study seats and the different anthropometric sizes of the students. The study problem is manifested in the following question: what are the anthropometric treatments used in the design of the study seats in the elementary stages? The research aims at finding design treatments for the anthropometric variables of the study seats used in the elementary stages, because the study seats have to do with preserving students health and safety through providing an ideal seating mechanism compatible with the anthropometric variables which enhances comfort, safety and focus in the mo
... Show MoreBackground: Chief complaint of patients attending dental clinic represents the first step towards treatment plan. However, most of patients are not aware but the extent and severity of periodontal disease, which could be also, misdiagnose by the dentist. Aim of the study: To investigate whether reported chief complaint(s) are consistent with oral hygiene status Materials and methods: Records of 1102 patients, attending periodontics clinics in the college of dentistry/ university of Baghdad, were used to determine ten most commonly reported chief complaints. Sample of patients was further subdivided according to gender and age. In addition, plaque and gingival index were recorded to determine oral hygiene status. Results: Patients mostly
... Show MoreUnlike welding, soldering does not involve melting the work pieces. Soldering is a process in which two or more items are joined together by melting and putting a filler metal (solder) into the joint. Failure in the solder joint may make the system components lose their functions. Electrical wiring and electronic components are joined to devices and printed circuit boards using soldering. Soldering and brazing are both used in the assembly of musical instruments. Lead-tin alloy solder employed in the current investigation which has a diameter of 4 mm and a density of 11.0103 kg/m3 with continuous heat flux heating from the domain's left side and complete insulation on the other side. The melting of PCM was simulated using the ANSYS
... Show More