Boron Removal by Adsorption onto Different Oxides
...Show More Authors

A research was conducted to determine the feasibility of using adsorption process to remove boron from aqueous solutions using batch technique. Three adsorbent materials; magnesium, aluminum and iron oxide were investigated to find their abilities for boron removal. The effects of operational parameters on boron removal efficiency for each material were determined.
The experimental results revealed that maximum boron removal was achieved at pH 9.5 for magnesium oxide and 8 for aluminum and iron oxide. The percentage of boron adsorbed onto magnesium,aluminum and iron oxide reaches up to 90, 42.5 and 41.5% respectively under appropriate conditions. Boron concentration in effluent water after adsorption via magnesium oxide comply with the allowable
concentration according to WHO and the Iraqi drinking water guidelines, i.e. below 0.5 mg/l. Aluminum and iron oxide yield effluent water with boron concentration more than allowable limits. Accordingly,magnesium oxide is more suitable as adsorbent for boron removal from water; for its high adsorbent capacity and high removal ability for boron compared with aluminum and iron oxide.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Wed Aug 28 2019
Journal Name
Journal Of Engineering
Adsorption of Methylene Blue on Prepared Charcoal from Molasses Waste
...Show More Authors

Recently, important efforts have been made in an attempt to search for the cheapest and ecofriendly alternatives adsorbents. In the present work, waste molasses from Iraqi date palm (Zahdi) had been used as a provenance to produce charcoal for the removal of methylene blue (MB) dye from water. The optimum prepared charcoal was obtained at 150 C, by increasing temperature to 175 C, the charcoal had almost converted to ash. The obtained charcoal have been inspected for properties using scanning electron microscope (SEM), atomic force microscope (AFM), porosity and surface area. Adsorption data were optimized to Langmuir and Freundlich and adsorption parameters have been evaluated. The thermodynamic parameters like a change

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Fri Jul 12 2024
Journal Name
Biomass Conversion And Biorefinery
Chitosan-triphosphate/food grade algae/montmorillonite clay for adsorptive removal of methyl violet 2B dye removal: Behnken design optimization
...Show More Authors

View Publication
Scopus (3)
Crossref (3)
Scopus Clarivate Crossref
Publication Date
Sun Oct 27 2019
Journal Name
Journal Of Global Pharma Technology
Adsorption Thermodynamic Study of Congo Red Dye on Electrospun Nanofibers Mat of Polyacrylonitrile
...Show More Authors

The present study intends to prepare nanofibers mat of polyacrylonitrile by electrospinning technique and investigates their adsorption capacity to Congo red dye from the aqueous solution, after characterize it by different techniques such as FTIR, SEM, EDA, XRD and BET. The influence factors on adsorption were studied including adsorbent dosage, initial concentration, contact time, pH and ionic strength. The results confirmed that the increasing in pH decreases the adsorption capacity. So, the optimum adsorbent dosage, initial concentration and contact time were 0.006 g, 25 mg/L and 150 min respectively. The isotherm models of Freundlich and Langmuir were applied on the experimental adsorption data to evaluate the maximum capacity and ener

... Show More
Preview PDF
Publication Date
Fri Mar 01 2024
Journal Name
Baghdad Science Journal
Isotherms and Thermodynamic Parameters of Metoprolol Drug Adsorption on the Prepared Mesoporous Silica
...Show More Authors

In this study, mesoporous silica (MPS) is made using the sol-gel method from a cheap source (Na2SiO3) using the surfactant hydroxycetyl hydroxyethyl dimonium chloride as a template. The task is the adsorption-based removal of the medication metoprolol (MP) at concentrations between 10 and 50 ppm. Variables such as: contact time, dose of adsorbent, starting concentration of adsorbate, and adsorption temperature were studied which show the equilibrium time and adsorbent dose are 40 min and 0.05 g respectively. The Langmuir, Freundlich, Temkin, and Dubinin-Radushkevich isotherm models were fitted to the data obtained from the experiments. Comparing the outcomes showed that, of the four investigated isotherm models, the Freundlich equation m

... Show More
View Publication Preview PDF
Scopus (6)
Crossref (2)
Scopus Crossref
Publication Date
Sun Jul 31 2022
Journal Name
Iraqi Journal Of Science
Adsorption of Biebrich Scarlet Dye into Remains Chromium and Vegetable Tanned Leather as Adsorbents
...Show More Authors

Chromium tanned leather wastes (CTLW) and vegetable tanned leather wastes (VTLW) were used as adsorbent materials to remove the Biebrich scarlet dye (BS), as an anionic dye from wastewater, using an adsorption method. The effects of various factors, such as weight of leather waste, time of shaking, and the starting concentration of Biebrich scarlet dye, temperature and pH were studied. It described the adsorption process using Langmuir and Freundlich isotherm models. The obtained results agreed well with the Langmuir model, and the maximum adsorption capacities of CTLW and VTLW were 73.5294 and 78.1250 mg.g⁻¹, respectively, suggesting a monolayer adsorption process. The adsorption kinetic was found to follow a pseudo-second-order kinetic

... Show More
Scopus (15)
Crossref (8)
Scopus Crossref
Publication Date
Fri Mar 31 2017
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Equilibrium, Kinetic and Thermodynamic Study of Aniline Adsorption over Prepared ZSM-5 Zeolite
...Show More Authors

Aniline and its derivatives are common contaminants in various wastewaters and represent a serious worry for societies health and a challenge to ecologists due to their dangers effects on to the human health.

ZSM-5 zeolite was prepared from locally available materials (kaolin and rice husk) for adsorption of aniline from synthetic wastewater. Characterization of the prepared zsm-5, kinetics and thermodynamic of the adsorption process were investigated.

The characterization results of the prepared zsm-5 zeolite showed that the surface area was 270.1 m2/g and pore volume 0.21828 cm3/g. The silica to alumina ratio (Si/Al) was 166. 47 and the sodium content was 11 wt. %. The atomic force microscope (AFM)

... Show More
View Publication Preview PDF
Publication Date
Sun Jul 09 2023
Journal Name
Journal Of Engineering
Dynamic Behavior of Pb(II) and Cr(III) Biosorption onto Dead Anaerobic Biomass in Fixed-Bed Column, Single and Binary Systems
...Show More Authors

The biosorption of lead (II) and chromium (III) onto dead anaerobic biomass (DAB) in single and binary systems has been studied using fixed bed adsorber. A general rate multi- component model (GRM) has been utilized to predict the fixed bed breakthrough curves for single and dual- component system. This model considers both external and internal mass transfer resistances as well as axial dispersion with non-liner multi-component isotherm (Langmuir model). The effects of important parameters, such as flow rate, initial concentration and bed height on the behavior of breakthrough curves have been studied. The equilibrium isotherm model parameters such as maximum uptake capacities for lead (II) and chromium (III) were found to be 35.12 and

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Wed Mar 18 2020
Journal Name
Baghdad Science Journal
In Vitro Bioremediation: A Development Process of Cadmium and Mercury Removal by Environmental Biotechnologies of UV-Mutated Escherichia coli K12 and Bacillus subtilis 168
...Show More Authors
  1. coli K12 and B. subtilis 168 were investigated for their cadmium and mercury tolerance abilities. They were developed by UV mutagenesis technique to increase their tolerances either to cadmium or mercury, and their names then were designated depend on the name and concentration of metals. E. coli K12 Cd3R exhibited bioremediation amount of 6.5 mg Cd/g dry biomass cell. At the same time, its wild-type (E. coli K12 Cd3) was able to remove 5.2 mg Cd/g dry biomass cell in treatment of 17 mg Cd /L within 72 hours of incubation at 37 °C (pH=7) in vitro assays. The results show that E.coli K12 Hg 20 was able to remove 0.050 µg Hg/g dry biomass cell
... Show More
View Publication Preview PDF
Scopus (12)
Crossref (6)
Scopus Clarivate Crossref
Publication Date
Sat Mar 30 2019
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Removal of Manganese Ions (Mn2+) from a Simulated Wastewater by Electrocoagulation/ Electroflotation Technologies with Stainless Steel Mesh Electrodes: Process Optimization Based on Taguchi Approach
...Show More Authors

This study depicts the removal of Manganese ions (Mn2+) from simulated wastewater by combined electrocoagulation/ electroflotation technologies. The effects of initial Mn concentration, current density (C.D.), electrolysis time, and different mesh numbers of stainless steel screen electrodes were investigated in a batch cell by adopting Taguchi experimental design to explore the optimum conditions for maximum removal efficiency of Mn. The results of multiple regression and signal to noise ratio (S/N) showed that the optimum conditions were Mn initial concentration of 100 ppm, C.D. of 4 mA/cm2, time of 120 min, and mesh no. of 30 (wire/inch). Also, the relative significance of each factor was attained by the analysis

... Show More
View Publication Preview PDF
Crossref (5)
Crossref
Publication Date
Sat Mar 30 2019
Journal Name
Iraqi Journal Of Chemical And Petroleum Engineering
Removal of Manganese Ions (Mn2+) from a Simulated Wastewater by Electrocoagulation/ Electroflotation Technologies with Stainless Steel Mesh Electrodes: Process Optimization Based on Taguchi Approach
...Show More Authors

This study depicts the removal of Manganese ions (Mn2+) from simulated wastewater by combined electrocoagulation/ electroflotation technologies. The effects of initial Mn concentration, current density (C.D.), electrolysis time, and different mesh numbers of stainless steel screen electrodes were investigated in a batch cell by adopting Taguchi experimental design to explore the optimum conditions for maximum removal efficiency of Mn. The results of multiple regression and signal to noise ratio (S/N) showed that the optimum conditions were Mn initial concentration of 100 ppm, C.D. of 4 mA/cm2, time of 120 min, and mesh no. of 30 (wire/inch). Also, the relative significance of each factor was attained by the analysis of variance (ANO

... Show More
View Publication Preview PDF
Crossref (5)
Crossref