This study is concerned with the effect of Deep Cryogenic Treatment (DCT) at liquid nitrogen temperature (-196 o C) on the mechanical properties and performance of low carbon steel (A858). The tests specimens were divided in to two groups, the first group was subjected to the conventional heat treatment of normalizing, and the second group was also normalized then subjected to (DCT). The results have shown that after (DCT), the Hardness, Tensile properties and the impact energy absorbed were all slightly increased. However the fatigue test showed some positive improvement in fatigue limit by 20(N/mm2 ), and the volume wear rates at different loads were significantly decreased after (DCT). The changes in microstructure due to (DCT) were clearly noticeable, the grain boundaries were no longer visible, and the Pearlite isles globalization was obvious.
The most significant function in oil exploration is determining the reservoir facies, which are based mostly on the primary features of rocks. Porosity, water saturation, and shale volume as well as sonic log and Bulk density are the types of input data utilized in Interactive Petrophysics software to compute rock facies. These data are used to create 15 clusters and four groups of rock facies. Furthermore, the accurate matching between core and well-log data is established by the neural network technique. In the current study, to evaluate the applicability of the cluster analysis approach, the result of rock facies from 29 wells derived from cluster analysis were utilized to redistribute the petrophysical properties for six units of Mishri
... Show MoreA thin CdS Films have been evaporated by thermal evaporation technique with different thicknesses (500, 1000, 1500 and 2000Å) and different duration times of annealing (60, 120 180 minutes) under 573 K annealing temperature, the vacuum was about 8 × 10-5 mbar and substrate temperature was 423 K. The structural properties of the films have been studied by X- ray diffraction technique (XRD). The crystal growth became stronger and more oriented as the film thickness (T) and duration time of annealing ( Ta) increases.
Copper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show MoreThe zirconia ceramic restoration (ZCR) is used as substitutes for the metal-ceramic restoration. Clinical studies demonstrating of ZCRs showed a high fracture incidence of veneering layer than metal-ceramic restorations. This attributed to the low bond strength of zirconia to veneering ceramic as a result of lacking of glass content in its matrix. Surface treatment was proposed to improve the bonding strength between zirconia and veneering ceramic. Several studies revealed that some treatment such as airborne particle abrasion (APA) is responsible for generating chipping of veneering ceramic. The study aimed to develop a new zirconia coatings to increase bonding strength between zirconia substrate and veneering porcelain. Three groups of 15
... Show MoreTin oxide films (SnO2) of thickness (1 ?m) are prepared on glass substrate by post oxidation of metal films technique. Films were irradiated with Nd:YAG double frequency laser of wavelength (532 nm) pulses of three energies (100, 500, 1000) mJ. The optical absorption, transmission, reflectance, refractive index and optical conductivity of these films are investigated in the UV-Vis region (200-900) nm. It was found that the average transmittance of the films is around (80%) at wavelength (550 nm) and showed high transmission (? 90 %) in the visible and near infrared region. The absorption edge shifts towards higher energies, which is due to the Moss-Burstien effect and it lies at (4 eV). The optical band gap increased with increasing of ene
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreBeta-irradiation effects on the microstructure of LDPE samples have been investigated
using Positron Annihilation Lifetime Technique (PALT). These effects on the orthopositronium
(o-Ps) Lifetime t3, the free positron annihilation lifetime 2 t , the free-volume
hole size (Vh) and the free volume fraction (fh) were measured as functions of Beta
irradiation - dose up to a total dose of 30.28 kGy.
The results show that the values of t3, Vh and fh increase gradually with increasing Beta
dose up to a total dose of 1.289 kGy, and reach a maximum increment of 17.4%, 32.8% and
5.86%, respectively, while t2 reachs maximum increment of 211.9% at a total dose of 1.59
kGy. Above these doses, the values show nonlinear changes u
An experimental investigation of the variation of argon discharge current with a glow and afterglow time intervals of a square discharge voltage was carried out at low pressure (6-11 mbar). The discharge was created between two circular metal electrodes of diameter (7.5 cm), separated horizontally by a distance (10 cm) at the two ends of a Pyrex cylindrical tube. A composite of two Gaussian functions has been suggested to fit and explain the variation graphs clearly. It is shown that the necessary times of glow and afterglow needed to attain a maximum discharge current are (70 us) and (60 us), respectively. The discharge current is observed to drop to the lowest value when the two times are serially longer than (85 us) and (72 u
... Show More