Roller compacted concrete (RCC) is a concrete of no slump, no reinforcement, no finishing, and compacted using vibratory roller. When compared with conventional concrete, it contains less water content
when compared to traditional concrete. The RCC technique achieves significant time and cost savings during the construction of concrete. This study demonstrates the preparation of RCC slab of (38 ×38× 10) cm
samples by using roller compactor which is manufactured in local markets. The Hydrated lime additive is used to study the mechanical and physical properties of that RCC slab samples. This investigation is divided
into two main stages: The First stage consists of hammer compaction method with two gradation of aggregate, dense and gap graded aggregate, using five percentages of cement content (10, 12, 14, 16, and 18) as a percentage of the total aggregate content. This stage is carried out for selecting the maximum dry density, optimum moisture content, and optimum cement content which is utilized in RCC slab samples
construction, a total of 49 cylinder samples sized (10 cm diameter and 11.6 cm high) are prepared. The Second stage is classified into two sub stages; the first one consists of constructing RCC slab samples using roller compaction, 12% cement as a percentage of total aggregate weight has been used according to the data obtained from first stage, this group presents reference mixes without additives. While the second sub stage presents RCC mix with hydrated lime additive and with the same gradation of mixes compact by hammer compaction method, hydrated lime was implemented as (5, 10, 12, and 15) percentage
as a partial replacement of cement content. Both of physical and mechanical properties of RCC are studied using cores, sawed cubes, and sawed beams obtained from RCC slab samples. The properties studied were porosity, absorption, and compressive strength, splitting tensile strength and flexural strength by using third point loading method. The results show that hydrated lime improved the overall properties of RCC as compared to reference mix. Mixes with 5% lime give the optimum values for most of strength properties. Dense graded mixes with hydrated lime show superior properties as compared to gap graded mixes.
Flexible pavements are subjected to three main distress types: fatigue crack, thermal crack, and permanent deformation. Under severe climate conditions, thermal cracking particularly contributes largely to a considerable scale of premature deterioration of pavement infrastructure worldwide. This challenge is especially relevant for Europe, as weather conditions vary significantly throughout the year. Hydrated lime (HL) has been recognized as an effective additive to improve the mechanical properties of asphalt concrete for pavement applications. Previous research has found that a replacement of conventional limestone dust filler using hydrated lime at 2.5% of the total weight of aggregates generated an optimum improvement in the mec
... Show MoreMoisture induced damage can cause a progressive deterioration in the performance of asphalt pavement by the loss of adhesion between asphalt binder and aggregate surface and/or loss of cohesion within the binder in the presence of water. The objective of this paper is to improve the asphalt mixtures resistance to moisture by using hydrated lime as an anti-stripping additive. For this purpose, two types of asphalt binder were utilized; asphalt grades (40-50) and (60-70) with one type of aggregate of 19.0 mm aggregate nominal maximum size, and limestone dust as a mineral filler. Marshall method was adopted to find the optimum asphalt content. Essentially, two parameters were determined to evaluate the moisture susceptibili
... Show MoreRoller-Compacted Concrete is a no-slump concrete, with no reinforcing steel, no forms, no finishing and wet enough to support compaction by vibratory rollers. Due to the effect of curing on properties and durability of concrete, the main purpose of this research is to study the effect of various curing methods (air curing, 7 days water curing, and permanent water curing) and porcelanite (local material used as an Internal Curing agent) with different replacement percentages of fine aggregate (volumetric replacement) on some properties of Roller-Compacted Concrete and to explore the possibility of introducing practical Roller-Compacted Concrete for road pavement with minimum requirement of curing. Specimens were sawed fro
... Show MorePremature failure in asphalt concrete pavement has been the main concern for pavement construction companies and engineers in recent years because of the large rise in traffic volume and loads and the temperature extremes in the summer and winter. The use of modifiers in asphalt concrete mixtures has attracted much attention to increase the performance and lifespan of pavements. As nanotechnology developed, several researchers concentrated on how these materials can help increase pavement serviceability by minimizing rutting and moisture damage. This study evaluates the Hydrated Lime (HL) effect by two methods (wet and dry hydrated lime) on the durability of the warm mix asphalt. The first method, HL, has been supplemented to the as
... Show MorePermanent deformation, fatigue and thermal cracking are the three typical distresses of flexible pavement. Using hydrated lime (HL) into the conventional limestone mineral additive has been widely practiced, including in Europe, to improve the mechanical properties of hot mix asphalt (HMA) concrete and as the result the durability of the constructed pavement. Large number of experimental studies have been reported to find the optimum addition of HL for the improvement on HMA concrete mechanical properties, moisture susceptibility and fatigue resistance. Pavement in service is under complex thermomechanical stress-strain conditions due to coupled atmospheric and surrounding environment temperature variation and the traffic loading. To predic
... Show MoreRecently, some of Iraq's newly constructed asphalt concrete pavements showed premature failures with significant negative impacts on roadway safety and the economy. Using Nano hydrated lime (NHL) in pavement construction could be one of the possible steps to improve pavement durability. This article discusses how NHL affects the durability of hot mix asphalt. NHL was added in two methods to the asphalt concrete mixture for the wearing course. The first is the dry method, i.e., on the aggregate, whereas the second is the wet addition method, i.e., to the bitumen. The percentages were tried for each additional method; 1, 2, and 3% by weight of aggregate for the dry method and 0.5, 1, and 1.5% by weight of asphalt concrete for the wet
... Show MoreTo decrease the impact on the environment of building waste, the recycled aggregate may be used in various sustainable engineering applications, such as roller compacted concrete pavement (RCCP). This research examined how using recycled aggregate as a partial replacement for natural aggregate as coarse or fine affected the mechanical properties of roller-compacted concrete pavement. The recycled aggregate was crushed and sieved to coarse and fine aggregate before being used in the roller-compacted concrete pavement. Compressive strength, splitting tensile strength, and flexural strength were all evaluated after the samples were prepared at 28 and 90 days of curing. According to the study's findings, the partial replacem
... Show MoreRecently, increasing material prices coupled with more acute environmental awareness and the implementation of regulation has driven a strong movement toward the adoption of sustainable construction technology. In the pavement industry, using low temperature asphalt mixes and recycled concrete aggregate are viewed as effective engineering solutions to address the challenges posed by climate change and sustainable development. However, to date, no research has investigated these two factors simultaneously for pavement material. This paper reports on initial work which attempts to address this shortcoming. At first, a novel treatment method is used to improve the quality of recycled concrete coarse aggregates. Thereafter, the treated recycled
... Show MoreIn the recent years, some of the newly constructed asphalt concrete pavements in Baghdad as well as other cities across Iraq showed premature failures with consequential negative impact on both roadway safety and economy. Frequently, load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some poorly drained sections are the main failure types found in those newly constructed road.
In this research, hydrated lime was introduced into asphalt concrete mixtures of wearing course in two methods. The first one was the addition of dry lime on dry aggregate and the second one was the addition of dry lime on saturated surface dry aggregate moisturized by 2.0 to 3.0 percent of wa
... Show MorePrevious experimental studies have suggested that hot mixed asphalt (HMA) concrete using hydrated lime (HL) to partially replace the conventional limestone dust filler at 2.5% by the total weight of all aggregates showed an optimum improvement on several key mechanical properties, fatigue life span and moisture susceptibility. However, so far, the knowledge of the thermal response of the modified asphalt concrete and thermal influence on the durability of the pavement constructed are still relatively limited but important to inform pavement design. This paper, at first, reports an experimental study of the tensile fatigue life of HMA concrete mixes designed for wearing layer application. Tests were conducted under three different temperatur