This Investigation aims to study the effect of adding Steel fibers with different volume fractions Vf (o.5, 0.75, and 1% by volume of concrete) with aspect ratio 100 on mechanical properties of concrete, and also
finding the influence of petroleum products (Kerosene and Diesel) on mechanical properties of Steel Fiber Reinforced Concrete (SFRC).
The experimental work consists of two groups: group one consists of specimens (cubes and prisms) plain and concrete reinforced with steel fiber exposed to continuous curing with water. Group two consists of
specimens (cubes and prisms) plain and concrete reinforced with steel fiber exposed to kerosene and diesel after curing them in water for 28 days before exposure. The results of all tests refer that the specimens (plain and reinforced concrete with steel fiber with different volume fraction) exposed to kerosene were better than the specimens (plain and reinforced concrete with steel fiber with different volume fraction) exposed to diesel.
Cooling towers is one of the most important unit in industry, they are used to dispose heat from cooling media used in the integrated units. The choice of the cooling media plays recently an important rule due to fresh-water scarcity. The use of saline as a cooling media become of growing interest, but the corrosion problem has to be taken in consideration. In this study the simultaneous effect of cooling tower operation parameters on the corrosion rate of mild-steel is considered. The role of NaCl content is found to be pronounced more than the working solution temperature and flowrate. The corrosion of mild-steel in these studied factors had shown an interesting result especially with the NaCl% content. Firstly, there was an increase in t
... Show MoreWater absorbent polymers (WAP) are new component in producing building materials. They provide internal curing which reduces autogenous cracking, eliminates autogenous shrinkage, mortar strength increased, enhance early age strength to withstand strain, improve the durability, introduce higher early age compressive strength, have higher performance and reduce the effect of insufficient external curing. This research used different percent of polymer balls to choose the percent that provides good development in compressive strength with time for both water and air curing. The water absorption polymer balls in this research have the ability to absorb water and after usage in concrete they spill out the water (internal curing) and shri
... Show MoreMoisture damage is a primary mode of distress occurring in hot mix asphalt (HMA) pavements in Iraq. Because of the loss of bond, or stripping, caused by the presence of moisture between the asphalt and aggregate, which is a problem in some areas and can be severe in some cases, it is requires to evaluate the design asphalt mixture to moisture susceptibility. Many factors such as aggregate characteristics, asphalt characteristics, environment, traffic, construction practices and drainage can contribute to stripping. Asphalt concrete mixes were prepared at their optimum asphalt content by superpave system and then tested to evaluate their engineering properties, which include tensile strength, resilient modulus, and perman
... Show MoreThis study dealt with the management strategy as an independent variable and the integrated industrial distribution as a variable. The study aimed at finding the integrated industrial distribution that fits with the management strategy in providing the needs of the firm on the one hand and reducing the cost of management that is reflected in increasing its profits.
The researcher selected the data from (130) decision makers in the corporation and used the questionnaire as a tool for collecting data and used a set of statistical tools and tools suitable for the nature of information and were processed using the data analysis system (SPSS version 24) Based on the analysis of the responses of the sample and the test of correlation and
Background: Numerous methods have been described for achievement of Intermaxillary fixation in the treatment of fractures of facial skeleton. Conventional methods like Erich arch bars and eyelet wires are currently the most common methods for achieving intermaxillary fixation (IMF), however, they have their own disadvantages. Since 1989, IMF using intraoral self-tapping IMF screws has been introduced for treatment of mandibular fractures. The aim of this study was to evaluate the efficacy, advantages, disadvantages and potential complications associated with using of self-tapping IMF screws in the treatment of mandibular fractures. Material and Methods: Twenty patients with favorable mandibular fractures, attended to Oral and Maxillofacial
... Show MoreThis research examines the use of vibratory treatments to reduce residual stresses in small welded parts. In this experimental investigation, a post weld vibration treatment was applied to T- A106 steel pipe fitting specimens to study the effect of the treatment on the residual stress and the hardness of the material. The vibratory stress relief treatment was carried out at different vibration frequency. The results have demonstrated that post-weld vibratory stress relief of small size fittings is possible and residual stress may be relieved, and the treatment may be an alternative method for heat treatment especially when unchange in dimensions and material stability are required.
The effect of applied current on protection of carbon steel in 0.1N NaCl solution (pH=7) was investigated under flow conditions (0-0.262 m/s) for a range of temperatures (35-55°C) using rotating cylinder electrode. Various values of currents were applied to protect steel from corrosion, these were Iapp.=Icorr., Iapp.=2Icorr. and Iapp.=2.4Icorr. under stationary and flow conditions. Corrosion current was measured by weight loss method. The variation of protection potential with time and rotation velocity at various applied currents was assessed. It is found that the corrosion rate of carbon steel increases with rotation velocity and
has unstable trend with temperature. The protection current required varies with temperature and it inc
The performance of asphalt concrete pavement has affected by many factors, the temperature is the most important environmental one which has a large effect on the structural behavior of flexible pavement materials. The main cause of premature failure of pavement is the rutting, Due to the viscoelastic nature of the asphalt cement, rutting is more pronounced in hot climate areas because the viscosity of the asphalt binder which is
inversely related to rutting is significantly reduced with the increase in temperature resulting in a more rut susceptible paving mixtures. The objective of this study is to determine the effect of temperatures variations on the permanent deformation parameters (perm
Many tools and techniques have been recently adopted to develop construction materials that are less harmful and friendlier to the environment. New products can be achieved through the recycling of waste material. Thus, this study aims to use recycled glass bottles as sustainable materials.
Our challenge is to use nano glass powder by the addition or replacement of the weight of the cement for producing concrete with enhanced strength.
A nano recycled glass p
Waste materials might be utilized in various applications, such as sustainable roller compacted concrete pavements (RCCP), to lessen the negative environmental consequences of construction waste. The impacts of utilizing (brick, thermostone, granite, and ceramic) powders on the mechanical characteristics of RCCP are investigated in this study. To achieve this, the waste materials were crushed, grounded, and blended before being utilized as filler in the RCCP. After the mixes were prepared, compressive strength, splitting tensile strength, flexural strength, water absorption, density, and porosity were all determined. According to the research results, adding some of these powders, mainly brick and granite powder, enhances the mechanical
... Show More