Test results of six half-scale reinforced concrete flat plates connections with an opening in the vicinity of the column are reported. The test specimens represent a portion of a slab bounded by the lines of contraflexure around the column. The tests were designed to study the effect of openings on the punching shear behavior of the slab-column connections. The test parameters were the location and the size of the openings. One specimen had no opening and the remaining five had various arrangements of openings around the column. All specimens were cast with normal density concrete of approximately 30 MPa compressive strength. The openings in the specimens were square, with the sides parallel to the sides of the column. Three sizes of openings were used: the same size as the column (150 x 150 mm), 67 percent of the column size (100 x 100mm), and 150 percent of the column size (225×225mm). Due to the presence of the openings, the specimens showed a decrease in punching shear capacity ranged between 11.43% and 29.25% with respect to the control solid slab. Also, the stiffness decreased between 0.31% and 83.00%, depending on the size and location of these openings with respect to the column.
Warm asphalt mixture (WMA) and reclaimed asphalt pavement (RAP) are the most memorable sustainable materials in world of asphalt concrete pavements . This research aims to study the warm asphalt mixture for different types of filler materials such as ordinary cement and limestone dust. Beside, this research focused on the test of emulsified asphalt properties by evaluating the performance of warm asphalt mixture by Marshall Stability properties as well as moisture sensitivity. The results of this experiment provided many important points. First, The cationic emulsified asphalt is suitable with RAP aggregate for production warm asphalt mixtures .Second, The effective mixing procedure for warm asphalt mixtures consists hea
... Show MoreConventional concretes are nearly unbendable, and just 0.1 percent of strain potential makes them incredibly brittle and stiff. This absence of bendability is a significant cause of strain failure and has been a guiding force in the production of an elegant substance, bendable concrete, also known as engineered cement composites, abbreviated as ECC. This type of concrete is capable of displaying dramatically increased flexibility. ECC is reinforced with micromechanical polymer fibers. ECC usually uses a 2 percent volume of small, disconnected fibers. Thus, bendable concrete deforms but without breaking any further than conventional concrete. This research aims to involve this type of concrete, bendable concrete, that will give solut
... Show MoreReinforcing asphalt concrete with polyester fibers considered as an active remedy to alleviate the harmful impact of fatigue deterioration. This study covers the investigation of utilizing two shapes of fibers size, 6.35 mm by 3.00 mm and 12.70 mm by 3.00 mm with mutual concentrations equal to 0.25 %, 0.50 % and 0.75 % by weight of mixture. Composition of asphalt mixture consists of different optimum (40-50) asphalt cement content, 12.50 mm nominal aggregate maximum size with limestone dust as a filler. Following the traditional asphalt cement and aggregate tests, three essential test were carried out on mixtures, namely: Marshall test (105 cylindrical specimens), indirect tensile strength test (21 cylindrical specimens)
... Show MoreAs human societies grow, the problem of waste management becomes one of the pressing issues that need to be addressed. Recycling and reuse of waste are effective waste management measures that prevent pollution and conserve natural resources. In this study, the possibility of using glass waste as an alternative was used as a partial weight substitute for fine aggregates with replacement ratios of 10, 20, 30, and 40% by the weight, and formed into test models (15 cm * 15 cm ) cube and (15 cm * 30 cm) cylinder, then matured and tested their strength compression and tensile strength at the age of 7 and 28 days and compared with a reference or conventional concrete with a mixing ratio (1: 1.5: 3) as well as testing its worka
... Show MoreConcrete pavements are essential to modern infrastructure, but their low tensile and flexural strengths can cause cracking and shrinkage. This study evaluates fiber reinforcement with steel and carbon fibers in various combinations to improve rigid pavement performance. Six concrete mixes were tested: a control mix with no fiber, a mix with 1% steel fiber (SF1%), a mix with 1% carbon fiber (CF1%), and three hybrid mixes with 1% fiber content: 0.75% steel /0.25% carbon fiber (SF0.75CF0.25), 0.25% steel /0.75% carbon fiber (SF0.25CF0.75), and 0.5% steel /0.5% carbon fiber ((SF0.5CF0.5). Laboratory experiments including compressive, flexural, and splitting tensile strength tests were conducted at 7, 28, and 90 days, while Finite Element Analys
... Show MoreThe introduction of concrete damage plasticity material models has significantly improved the accuracy with which the concrete structural elements can be predicted in terms of their structural response. Research into this method's accuracy in analyzing complex concrete forms has been limited. A damage model combined with a plasticity model, based on continuum damage mechanics, is recommended for effectively predicting and simulating concrete behaviour. The damage parameters, such as compressive and tensile damages, can be defined to simulate concrete behavior in a damaged-plasticity model accurately. This research aims to propose an analytical model for assessing concrete compressive damage based on stiffness deterioration. The prop
... Show MoreMoisture-induced damage is one of the primary causes of premature distress in asphalt pavements, leading to reduced service life and increased maintenance costs. Although nanomaterials have shown potential in enhancing asphalt performance, the underlying composite interaction mechanisms among nanomaterials, asphalt binder, and aggregate phases under moisture exposure are still not fully understood. In addition, comparative evaluations under consistent experimental conditions remain limited. This study investigates the influence of five nanomaterials: nano-silica (NS), nano-alumina (NA), nano-titanium dioxide (NT), nano-zinc oxide (NZ), and carbon nanotubes (CNT) on the physical and mechanical properties of asphalt binders and mixtur
... Show MoreBackground: The longevity of any prosthesis depends on the materials from which it was fabricated, that is why, defects in the material properties may reduce the service life of prosthesis and necessitate its replacement. The aim of this study was to evaluate the effect of adding different concentrations of Polyamide-6 (Nylon-6) on the tear and tensile strength of A-2186 RTV silicone elastomer. Materials and Methods: 80 samples were fabricated by the addition of 0%, 1%, 3% and 5% by weight PA-6 micro-particles powder to A-2186 platinum RTV silicone elastomer. The study samples were divided into four (4) groups, each group containing 20 samples. One control group was prepared without PA-6 micro particles and three experimental groups were pr
... Show More