This research studies the effect of adding five different percentages of polymer (2, 4, 6, 8, and 10% of cement weight) on cement mortar's fresh and hardened properties, which was cured at laboratory temperature for 7, 14, and 28 days. Workability increases with increasing polymer. The workability value was lowest (25.6 and 29.4) % in mixtures containing 2% and 4% of (SBR). Increasing polymer ratios significantly decreased mechanical properties (compressive and flexural strength). Therefore, the best results were at 2% SBR and 4% SBR at 28 days of age. An inverse relationship was recorded between the increase in SBR ratios and polymer-modified cement mortar's compressive and flexural strength values. In general, the highest improvement in the water absorption and dry density resulted in better results with a decrease in the proportion of the polymer for all specimens of cement mortar containing 4% SBR polymer relative to the reference mixture.
The important aspect of this unconventional approach is that eco-friendly, commercially available and straight forward method was used to prepared Silver Nanoparticles by using AgNO3 and curcumin solution as agent factor. The (TEM), (XRD), and (FTIR) was used to characterise these silver nanoparticles (AgNPs). Two types of bacterial isolates were used to indicate the antibacterial activity silver nanoparticles which prepared by curcumin solution, Gram negative like (Escherichia Coli E. Coli), & Gram positive (Stapha Urous). The results exhibit that silver nanoparticles synthesized by curcumin solution has effective antibacterial activities.
Recently, a great rise in the population and fast manufacturing processes were noticed. These processes release significant magnitudes of waste. These wastes occupied a notable ground region, generating big issues for the earth and the environment. To enhance the geotechnical properties of fine-grained soil, a sequence of research projects in the lab were conducted to analyze the impacts of adding sludge waste (SW). The tests were done on both natural and mixed soil with SW at various proportions (2%, 4%, 6%, 8%, and 10%) based on the dry mass of the soil used. The experiments conducted focused on consistency, compaction, and shear strength. With the addition of 10% of SW, the values of LL and PI decreased by 29.7% and 3
... Show MoreBackground: Polyetheretherketone (PEEK) is a promising implant material due to its superior biomechanical strength. However, due to its hydrophobic nature and lack of cellular adhesion properties, it has poor integration with bone tissue. Methods: A fractional CO2 laser was used with various parameters for surface texturing of PEEK substrate to enhance its surface properties. An optical microscope and field-emission scanning electron microscope (FESEM) were used to examine the surface morphology of untextured and laser-textured samples. Energy dispersive X-ray spectroscopy (EDX) was performed to determine the effect of the laser on the microstructure of PEEK. Surface microroughness, atomic force microscopy (AFM), and wettability were invest
... Show MoreObjective. Glass-ionomer and resin-modified glass-ionomer cements are versatile materials with the ability to form a direct bond with tooth tissues. The aim of this study was to formulate a novel class of dental bio-interactive restorative material (pRMGIC) based on resin-modified glass-ionomer cements via the inclusion of an organophosphorus monomer, ethylene glycol methacrylate phosphate, with a potential to improve the mechanical properties and also function as a reparative restorative material. Methods. pRMGIC was formulated with modification of the resin phase by forming mixes of ethylene glycol methacrylate phosphate (EGMP; 0–40%wt) and 2-hydroxyethyl methacrylate monomer into the liquid phase of a RMGIC (Fuji II LC, GC Corp.).
... Show MoreIn this work ,the modified williamos-Hall method was used to analysis the x-ray diffraction lines for powder of magnesium oxide nanoparticles (Mgo) .and for diffraction lines (111),(200),(220),(311) and (222).where by used special programs such as origin pro Lab and Get Data Graph ,to calculate the Full width at half maximum (FWHM) and integral breadth (B) to calculate the area under the curve for each of the lines of diffraction .After that , by using modified Williamson –Hall equations to determin the values of crystallite size (D),lattice strain (ε),stress( σ ) and energy (U) , where was the results are , D=17.639 nm ,ε =0.002205 , σ=0.517 and U=0.000678 respectively. And then using the scherrer method can by calculated the crystal
... Show MoreABSTRACT
A laboratory experiment was carried out during winter season of 2021 in the Seed Technology Laboratory- College of Agricultural Engineering Sciences/ University of Baghdad, to find out the allopathic effects of aerobic and terrestrial aqueous extracts of Artemisia vulgaris L. on the seed germination and seedling growth of linseed. A factorial experiment according to a completely randomized design (CRD)at three replicates was used; the first factor in clouded type of aqueous extract for two plant parts which were aerobic (stems and leaves) and terrestrial (root and rhizomes), while the second factor included five concentrations
... Show MoreWhen the depth of stressed soil is rather small, Plate Load Test (PLT) becomes the most efficient test to estimate the soil properties for design purposes. Among these properties, modulus of subgrade reaction is the most important one that usually employed in roads and concrete pavement design. Two methods are available to perform PLT: static and dynamic methods. Static PLT is usually adopted due to its simplicity and time saving to be performs in comparison with cyclic (dynamic) method. The two methods are described in ASTM standard.
In this paper the effect of the test method used in PLT in estimation of some mechanical soil properties was distinguished via a series of both test methods applied in a same site. The comparison of
... Show MoreThis study involves the design of 24 mixtures of fiber reinforced magnetic reactive powder concrete containing nano silica. Tap water was used for 12 of these mixtures, while magnetic water was used for the others. The nano silica (NS) with ratios (1, 1.5, 2, 2.5 and 3) % by weight of cement, were used for all the mixtures. The results have shown that the mixture containing 2.5% NS gives the highest compressive strength at age 7 days. Many different other tests were carried out, the results have shown that the carbon fiber reinforced magnetic reactive powder concrete containing 2.5% NS (CFRMRPCCNS) had higher compressive strength, modulus of rupture, splitting tension, str
... Show More