Dissolution of gypsum rock in water is significant, which may result in hydrocarbon reservoir formation and evaporate deposits. However, the complexity of the gypsum dissolution process is still of interest because of its uncleanness that requires more critical analysis. The objectives of this experimental study are emphasis on the dissolution characteristics of gypsum rock under room temperature and by various types of water; namely: deionized, tap, fresh, acidic, well, and normal rainwatre. In addition, the influences of dissolution on gypsum rock's mechanical and physical characteristics. Gypsum rock was obtained from Agjalar area, in the southwest of Sulaymaniyah city, Northern Iraq. Experimental results show that well water is the most effective type to dissolve gypsum and cause significant reductions in the mechanical characteristics of gypsum rock.
Autorías: Jehan Faris Yousif, Read Idrees Mahmood. Localización: Utopía y praxis latinoamericana: revista internacional de filosofía iberoamericana y teoría social. Nº. 1, 2020. Artículo de Revista en Dialnet.
At a time when any tourist in the world wants a trip to reload his energy and enjoy peace and quiet and engage in adventures in a safe environment, terrorism comes to disturb him on that journey through operations aimed at the tourist and entertainment destinations, such as shops, restaurants, cafes and hotels Is the orbit of research) for many reasons. The security measures taken by hotels play an important and fundamental role in preventing or limiting these terrorist operations. At the same time, while some hotel administrations are constantly seeking to improve these measures to preserve the safety of their guests and visitors, In spite of the high number of attacks on hotels since 2001 and today. This research is intended to highlight
... Show MoreSlurry-infiltrated fibrous concrete (SIFCON) is a special type of concrete that has great strength, as well as high ductility. However, the unit weight is high, which exceeds the unit weight of fiber-reinforced concrete, because of the high fiber content. This research aims to verify the compressive and flexural strength, as well as the density of SIFCON when using two different fibers (steel and polyolefin). Sometimes mono type of fiber steel or polyolefin, sometimes by hybridizing two types of fiber steel + polyplefin. Volume fraction (6% for all species) was used. Hook-end steel fiber and polyolefin fiber are used. With hybridization, a total volume fraction of 6% was used, which
The experimental study showed the use of closed cavity wall (the thickness of the cavity 5cm) made a percentage reduction in the cooling load caused by heat gain from the wall by (21.5 %) compared with the conventional wall. also the thermal resistance of the closed cavity was an average (0.2 m2.oC/W).
The experimental results of the study showed that the use of closed cavity wall reduced the average temperature of the inner surface of the wall during the day, and that the reduction was an average (0.45 oC) when compared with the conventional wall , as well as the use of closed cavity wall reduced the temperature difference range of the inner surface of the wall during the day, and that the
... Show MoreOver the last few decades, fiber reinforced polymer (FRP) has been increasingly used in strengthening different structural concrete members. The main objective of this research is to study the influence of curvature on the performance of curved soffit reinforced concrete (RC) bridge girders that have been strengthened with carbon fiber reinforced polymers (CFRP). This experimental program was designed to evaluate the effect of concavity and soffit curvature on the CFRP laminate utilization and load capacity, compared to flat soffit RC beams strengthened with the same CFRP system. Accordingly, five beams, 2.7 m in length and having the same degree of soffit curvature (20 mm per 1 meter
The objective of this study is to determine the efficacy of class V Er:YAG laser (2940 nm) cavity preparation and conventional bur cavity preparation regarding Intrapulpal temperature rise during cavity preparation in extracted human premolar teeth. Twenty non carious premolar teeth extracted for orthodontic purposes were used and class V cavity preparation was applied both buccal and lingual sides for each tooth .Samples were equally grouped into two major groups according to cavity depth (1mm and 2mm). Each major group was further subdivided into two subgroupsof ten teeth for each (twenty cavities for each subgroup). TwinlightEr:YAG laser (2940 nm) with 500mJ pulse energy, P.R.R of 10 Hz and 63.69 J/cm2 energy density was used. The ana
... Show MoreThis paper reports on the experimental study, which conducted a series of triaxial tests for the asphalt concrete using hydrated lime as a mineral additive. Three HMA mixes, prepared by the specification for wearing, levelling and base layers, were studied under three different temperatures. The test results have demonstrated that, compared with the control mixes excluding HL, the permanent deformation resistance of the HL modified mixes has significant improvement. The deformation has been reduced at the same load repetition number, meanwhile the flow number has been considerably increased. The degree of improvement in permanent deformation resistance using HL is more pronounced at high stress deviation states and high temperature.
... Show MoreThe accelerating effect of 1,4- phenylenediamine (PDA) additions in 1M hydrochloric acid solution at temperature rang (20-60) C° has been studied by weight losses measurement during ranging time (1-260) h and by following the pb2+ concentration in solution after several times by using Atomic absorption spectroscopy (AAS) . The volume of hydrogen gas involving was followed also in presence and absence of (PDA) in the corrosive solution .Accelerating enhanced by adding (NaCl , NaBr , NaI ) was also investigated.
Abstract Twelve isolates of bacteria were obtained from samples of different soils and water amended with 100µg/ml of five heavy metals chlorides (i.e: Aluminum Al+2, Iron Fe+2, Lead Pb+2, Mercury Hg+2 and Zinc Zn+2). Four isolates were identified as Bacillus subtilis and B. subtilis (B2) isolate was selected for this study according to their resistance to all five heavy metals chlorides. The ability of B. subtilis (B2) isolate for growing in different concentration of heavy metals chlorides ranging from 200-1200 µg/ml was tested. The highest conc. that B. subtilis (B2) isolate tolerate was 1000 µg/ml for Al+2, Fe+2, Pb+2, and Zn+2and 300 µg/ml for Hg+2 for 24hour. The effect of heavy metals chlorides on bacterial growth for 72 hrs was
... Show More