The waste material problem in today's world has become a major topic affecting all sectors of human life. Researchers are interested in providing solutions for each kind of waste material. Waste glass is one of the waste materials whose amounts increase daily. This article deals with two types of modified cement mortar with glass granular in the masonry wall to find their effect on the wall's property (direct tensile, flexural, and compressive bond strength). Seven different mixes were prepared according to the used glass granular ratio (three mixes contained white glass with 15, 20, and 25% while three of them contained green glass granular 5, 10, and 15%, and the last mix was a controlled mix which contains no glass granular).Based on the obtained result, the used white glass granular provides optimum compression and direct tensile bond strength when 20% of sand is replaced with white glass granular; optimum direct tensile bond value was obtained, which increased by 1.4% and increased compressive strength by 13.08% compared to control mortar. Green glass granular provides optimum compression and direct tensile bond strength when 10% of sand is replaced, direct tensile strength by 1.02%, and increased compressive strength by 3.7% compared to control mortar. The increase of the used waste glass granular in the mortar decreases flexural bond strength, and the amount of decrease depends on the chemical glass compositions.
With the increase in industry and industrial products, quantities of waste have increased worldwide, especially plastic waste, as plastic pollution is considered one of the wastes of the modern era that threatens the environment and living organisms. On this basis, a solution must be found to use this waste and recycle it safely so that it does not threaten the environment. Therefore, this research used plastic waste as an improvement material for clay soil. In this research, two types of tests were conducted, the first of which was a laboratory test, where the undrained shear strength (cohesion), compression index (Cc), and swelling index (Cr) of the improved and unimproved soils were calculated (plastic was added in pr
... Show MoreLandfill and incineration are the most common and widely used methods to dispose of solid wastes; both of these techniques are considered the main sources of pollution in the world due to the harmful toxic emissions that are considered an environmental problem. Because of the large areas used by landfills, they are not always considered an economical method. With the increase in the production of solid materials, solid wastes increase the pressure on incinerators and landfills, making the environmental pollution hazard more serious. Instead, these waste materials can be used in some other applications. One of the most important of these applications is asphalt pavements, which are the most used types of pavements in the
... Show More|
مجلة العلوم الاقتصادية والإدارية المجلد 18 العدد 69 الصفحات 318- 332 |
From the sustainability point of view a combination of using water absorption polymer balls in concrete mix produce from Portland limestone cement (IL) is worth to be perceived. Compressive strength and drying shrinkage behavior for the mixes of concrete prepared by Ordinary Portland Cement (O.P.C) and Portland limestone cement (IL) were investigated in this research. Water absorbent polymer balls (WAPB) are innovative module in producing building materials due to the internal curing which eliminates autogenous shrinkage, enhances the strength at early age, improve the durability, give higher compressive strength at early age, and reduce the effect of insufficient external curing. Polymer balls (WAPB) had been used in the mixes of thi
... Show MoreTight reservoirs have attracted the interest of the oil industry in recent years according to its significant impact on the global oil product. Several challenges are present when producing from these reservoirs due to its low to extra low permeability and very narrow pore throat radius. Development strategy selection for these reservoirs such as horizontal well placement, hydraulic fracture design, well completion, and smart production program, wellbore stability all need accurate characterizations of geomechanical parameters for these reservoirs. Geomechanical properties, including uniaxial compressive strength (UCS), static Young’s modulus (Es), and Poisson’s ratio (υs), were measured experimentally using both static and dynamic met
... Show MoreBack ground: Glass ionomer materials lack resistance to wear and pressure and are susceptible to moisture during the initial stages of setting and dehydration. So this study was done to assess diametral tensile strength and microhardness of glass ionomer reinforced by different amounts of hydroxyapatite. Materials and methods: In this study a hydroxyapatite material was added to glass monomer cement at different ratios: 10%, 15%, 20%, 25% and 30% (by weight). The diametral tensile strength test described by the British standard specification for zinc polycarboxylate cement was used in this study and the microhardness test was performed using Vickers microhardness testing machine and the microhardness values were calculated and statistical c
... Show MoreThis research paper aims at studying the effect of adopting the corporate social responsibility on marketing performance indicators, where the study adopted the descriptive method for theoretical concepts, in addition to the statistical approach by using the SPSS v25 program to analyze the questionnaire and test the hypotheses of the study. The results showed that there is a positive correlation between social responsibility and marketing performance indicators, and the study found that it is better for NAFTAL Company to mix the environmental and social responsibilities in order to improve its marketing performance. Also, the study recommended that Naftal should adopt the four responsibilities equally, correctly and make its work
... Show MoreErbium, as optical probe, doped silicate sol-gel glass with
different Er concentrations was formed by wet chemical synthesis
method using ethanol, water and tetraethaylorthosilicate
[Si(OC2H5)4] precursor. Erbium ions were incorporated into silica
sol-gel matrix via dissolution of Erbium chloride solution into the
initial Si(OC2H5)4 precursor sol. Aluminum (Al) as a co-dopant was
added to the final precursor in the form of Aluminum chloride
(AlCl3) solution. The prepared samples were analyzed using atomic
absorption analysis, X-ray diffraction and spectroscopic tests. The
experimental results concerned with the transmission spectra suggest
that the final samples have a good transparency and homogeneity.
A