The waste material problem in today's world has become a major topic affecting all sectors of human life. Researchers are interested in providing solutions for each kind of waste material. Waste glass is one of the waste materials whose amounts increase daily. This article deals with two types of modified cement mortar with glass granular in the masonry wall to find their effect on the wall's property (direct tensile, flexural, and compressive bond strength). Seven different mixes were prepared according to the used glass granular ratio (three mixes contained white glass with 15, 20, and 25% while three of them contained green glass granular 5, 10, and 15%, and the last mix was a controlled mix which contains no glass granular).Based on the obtained result, the used white glass granular provides optimum compression and direct tensile bond strength when 20% of sand is replaced with white glass granular; optimum direct tensile bond value was obtained, which increased by 1.4% and increased compressive strength by 13.08% compared to control mortar. Green glass granular provides optimum compression and direct tensile bond strength when 10% of sand is replaced, direct tensile strength by 1.02%, and increased compressive strength by 3.7% compared to control mortar. The increase of the used waste glass granular in the mortar decreases flexural bond strength, and the amount of decrease depends on the chemical glass compositions.
This research of using Feldspar in the production self compacting concrete (SCC) ( 5,10,15 )% as partial replacement by weight of cement .In this research some of fresh properties of SCC ( slump flow used V-funnel test and filling ability used ( U- box test ) for concrete mixes and also some of the harden properties of SCC ( compressive and flexural tests ). The research results showed that negative effect of Feldspar on the fresh properties of self compacting concrete but the positive effect of Feldspar on the harden properties of self compacting concrete .
The compound chalcon originally is extracted form some plant and herbs, the studies of the antiviral activity of this compound were done in two cell line cultures the L2OB and RD, the compound relatively non toxic to both cell lines of the concentration of 32?g/ml or less ,the compound have significantly anti poliovirus activity in both L2OB cell line and RD cell line, we find that the concentration of 0.03 ?g/ml or more inhibit the 100TCDID50 of the poliovirus .The therapeutic index(TI)used in this study to evaluate the drug activity ,( TI is the ratio of dose of drug which is just toxic to the cells to the does which is just inhibit the viral multiplication, if this index more than one the margin of safety of drug is according great ) .In
... Show MoreHigh temperature superconductors with a nominal composition HgBa2Ca2Cu3O8+δ
for different values of pressure (0.2,0.3, 0.5, 0.6, 0.9, 1.0 & 1.1)GPa were prepared by
a solid state reaction method. It has been found that the samples were semiconductor
P=0.2GPa.while the behavior of the other samples are superconductor in the rang
(80-300) K. Also the transition temperature Tc=143K is the maximum at P is equal to
0.5GPa. X-ray diffraction showed a tetragonal structure with the decreasing of the
lattice constant c with the increasing of the pressure. Also we found an increasing of
the density with the pressure.
An experimental and computational study is conducted to analyze the thermal performance of heat sinks and to pick up more profound information in this imperative field in the electronic cooling. One important approach to improve the heat transfer on the air-side of the heat exchanger is to adjust the fin geometry. Experiments are conducted to explore the impact of the changing of diverse operational and geometrical parameters on the heat sink thermal
performance. The working fluid used is air. Operational parameters includes: air Reynolds number (from 23597 to 3848.9) and heat flux (from 3954 to 38357 W/m
2 ). Conformational parameters includes: change the direction of air flow and the area of conduct
This paper deals with prediction the effect of soil re-moulding (smear) on the ultimate bearing capacity of driven piles. The proposed method based on detecting the decrease in ultimate bearing capacity of the pile shaft (excluding the share of pile tip) after sliding downward. This was done via conducting an experimental study on three installed R.C piles in a sandy clayey silt soil. The piles were installed so that a gap space is left between its tip and the base of borehole. The piles were tested for ultimate bearing capacity according to ASTM D1143 in three stages. Between each two stages the pile was jacked inside the borehole until a sliding of about 200mm is achieved to simulate the soil re-moulding due to actual pile driving. The re
... Show MoreAtotal of 75 different clinical samples were collected from different hospitals in Baghdad Biochemical and morphological characterization tests showed that forty isolates were identified as Staphylococcus aureus Antibiotic susceptibility tests of all isolates towards ten antibiotics were carried out and results showed that many isolates (97.5 %) were resistant to ?-lactam antibiotic , 70 % were resistant to Tetracyclinee , 62.5% were resistant to co-trimoxazole , 60 % were resistant to ciprofloxacin , 55% were resistant both of chloramphenicol and erythromycin , 52.5% were resistant to gentamicin , 35% were resistant to rifampicin , 10% were resistant to vancomycin . According to the above results the S.aureus I1 which is isolated
... Show MoreThe present work aimed to study the SiO2μPs, and NPs effect on the biodegradability of St/PVA blends. The samples were prepared by casting method as PVA, St/PVA blends with different concentrations (30, 40, 50, and 60 %). FTIR test was carried out for the samples preparation. The results proved some changes which might be related to changing in crystallinity of St/PVA matrix as well as physical incorporation of SiO2 μPs, and NPs addition. The enzymatic test and water uptake results proved that increase in weight loss with increases of starch ratio. The lowest weight loss was PVA; the highest weight loss is 60% St/PVA whereas the lowest weight loss is 30%St/PVA for blends involved. SiO2μPs (753.7 nm), and NPs (263.1 nm) were added at d
... Show MoreThis paper deals with prediction the effect of soil remoulding (smear) on the ultimate bearing capacity of driven piles. The proposed method based on detecting the decrease in ultimate bearing capacity of the pile shaft (excluding the share of pile tip) after sliding downward. This was done via conducting an experimental study on three installed R.C piles in a sandy clayey silt soil. The piles were installed so that a gap space is left between its tip and the base of borehole. The piles were tested for ultimate bearing capacity
according to ASTM D1143 in three stages. Between each two stages the pile was jacked inside the borehole until a sliding of about 200mm is achieved to simulate the soil remoulding due to actual pile driving. T