Normal concrete is weak against tensile strength, has low ductility, and also insignificant resistance to cracking. The addition of diverse types of fibers at specific proportions can enhance the mechanical properties as well as the durability of concrete. Discrete fiber commonly used, has many disadvantages such as balling the fiber, randomly distribution, and limitation of the Vf ratio used. Based on this vision, a new technic was discovered enhancing concrete by textile-fiber to avoid all the problems mentioned above. The main idea of this paper is the investigation of the mechanical properties of SCC, and SCM that cast with 3D AR-glass fabric having two different thicknesses (6, 10 mm), and different layers (1,2 layers). As well as micro-steel fiber with 1.25% volume fraction was used. Sixteen rectangular reinforced concrete beam specimens have been tested to study the behavior of their flexural strength. The results concluded that utilizing 3D-TFs with mortar mixture gave significantly higher enhancement for the load-carrying capacity than the concrete mixture. The utilization of 3D-TFs and micro-steel fiber together in the SCM mix gave better results. The stiffness of the specimens was improved with increasing the thickness and the number of textile fiber layers.
The primary purpose of this paper is to introduce the, N-coprobabilistic normed space, coprobabilistic dual space of N-coprobabilistic normed space and give some facts that are related of them.
This study assessed the effect of co-substitution of strontium (Sr) and magnesium (Mg) ions into the hydroxyapatite (HA) coating which was deposited on Ti–6Al–4V dental alloys by an electrochemical deposition process. The deposited layers were examined using energy-dispersive X-ray spectroscopy, scanning electron microscopy, Fourier transform infrared spectroscopy, atomic force microscopy and X-ray diffraction. The corrosion behavior of Ti–6Al–4V alloys in an artificial saliva environment was studied through potentiodynamic polarization technique and electrochemical impedance spectroscopy. The results indicated that the substituted Sr and Mg ions in HA improved the HA coating, where the protection efficiency percentage (PE%) for Ti
... Show MoreBackground: An injury to both the primary and permanent teeth and the supporting structures is one of the most common dental problems seen in children. Splinting is usually difficult or impossible to perform in the primary dentition (due to diminutive room size and lack of patient cooperation). Healing must, therefore, occur despite mobility at the fracture line, usually resulting in interposition of connective tissue. In some instances, infection will occur in the coronal pulp. The present study reported a case of trauma to the anterior primary teeth and alveolar bone in a four year old child. The trauma has caused fracture to the crowns and roots of the primary anterior teeth. The following case was managed in a procedure that may prov
... Show MoreBackground: White spot lesion is the first visible sign of dental caries that is characterized by demineralized lesion underneath an intact surface. Several studies demonstrated that they could be treated using noninvasive techniques like the use of fluoride or casein phospho-peptide and amorphous calcium phosphate. Improvement in aesthetic outcomes by covering the demineralized enamel is one of the advantages of the use of resin infiltration and opal-ustre microabrasion, which are two new techniques that had been used for treatment of white spot lesion. The purpose of this study was to evaluate the impact of resin infiltration and microabrasion in the microhardness of the artificial white spot lesions at various depths. Material and method
... Show MorePolish Academy of Sciences