In this research, thin films of CdO: Mg and n-CdO: Mg/ p-Si heterojunction with thickness (500±50) nm have been deposited at R.T (300 K) by thermal evaporation technique. These samples have been annealed at different annealing temperatures (373 and 473) K for one hour. Structural, optical and electrical properties of {CdO: Mg (1%)} films deposited on glass substrate as a function of annealing temperature are studied in detail. The C-V measurement of n-CdO: Mg/ p-Si heterojunction (HJ) at frequency (100 KHz) at different annealing temperatures have shown that these HJ were of abrupt type and the builtin potential (Vbi) increase as the annealing temperature increases. The I-V characteristics of heterojunction prepared under dark case at different annealing temperatures show that the values of ideality factor and potential barrier height increase with the increase of annealing temperature.
The influence of different thickness (500, 1000, 1500, and 2000) nm on the electrical conductivity and Hall effect measurements have been investigated on the films of copper indium gallium selenide CuIn1-xGaxSe2 (CIGS) for x= 0.6.The films were produced using thermal evaporation technique on glass substrates at R.T from (CIGS) alloy. The electrical conductivity (σ), the activation energies (Ea1, Ea2), Hall mobility and the carrier concentration are investigated and calculated as function of thickness. All films contain two types of transport mechanisms of free carriers, and increase films thickness was fond to increase the electrical conductivity whereas the activation energy (Ea) would vary with f
... Show More
The aim of the work is synthesis and characterization of new bidentate chalcone ligand type (NO):[(E)-1-(3-aminophenyl)-3-(4-chlorophenyl) prop-2-en-1-one] [H2L], from the reaction of 3-amino acetophenone with 4-chloro benzaldehyde to produce the ligand [H2L], the reaction was carried out in ethanol as a solvent under stirring. The prepared ligand [H2L] was characterized by FT-IR, UV-Vis spectroscopy, 1H, 13C-NMR spectra, Mass spectra, (C.H.N) and melting point. The complexes of ligand [H2L] were prepared with metal ion M(Π).Where M(Π) = (Mn ,Co ,Ni and Cu) at reflux ,using ethanol as a solvent and KOH as a base with molecular formula [M (H2L)2] +2 where: H2L= (C15H12NOCl). All the complexes were characterized by spectroscopic met
... Show MoreThe current work reports a new Schiff base [N1-benzylidenebenezene-1,2-diamine(L) = C20H16N2] has been synthesized from benzaldehyde (C6H5CHO) and O- aminoaniline (O-C6H4(NH2)2. Metal mixed ligand complexes of the Schiff base were prepared from chloride salts of Zn(II), Cd(II) and Hg(II) in ethanol and 8-hydroxyquinoline(8HQ)(C9H7NO) containing sodium hydroxide. All the complexes were characterized on the basis of their; FT-IR and U.V spectra, melting point, molar conductance, and determination of the percentage of the metal in the complexes by flame (AAS). In the all complexes, (8HQ) behaves as a bidentate ligand as primary ligand through –-OH phenolic group and –N groups of pyridine group. Also, the prepared ligand (L) was bidentate i
... Show MoreThe aim of the work is the synthesis and characterization of the tridentate Schiff base (HL) containing (N and O) as donor atoms type (ONO). The ligand is: (HL) phenyl 2-(2-hydroxybenzylidenamino)benzoate . This ligand was prepared by the reaction of (phenyl 2-aminobenzoate) with salicylaldehyde under reflux in ethanol and few drops of glacial acetic acid which gave the ligand (HL). The prepared ligand was characterized by (FT IR,UV–Vis) spectroscopy, Elemental analysis of carbon, hydrogen and nitrogen (C.H.N.) and melting point. The ligand was reacted with some metal ions under reflux in ethanol with (1 metal :2 ligand )mole ratio which gave complexes of the general formula: [M(L)2]Cl , M = Cr III La III and , Pr III Products were found
... Show MoreOlmesartan medoxomil (OM) has low bioavailability and limited solubility. To enhance bioavailability, fast dissolving films (FDF) with mixed micelles of soluplus (SPL) and solutol HS15 (STL H15) were developed using solvent casting. The optimised formula, FM2, used polyvinyl alcohol (PVA) and showed high entrapment efficiency, rapid disintegration, and significant improvement in OM bioavailability compared to the market tablet (Olmetec®). FM2 also demonstrated stability and potential for enhanced drug delivery.
The newly synthesized Schiff base ligand (E)-2-((2-phenylhydrazono)methyl)naphthalen-1-ol (phenyl hydrazine derivative), is allowed to react with each of the next mineral ion: Ni2+, Cu2+, Zn2+andCd2+successfully resulting to obtain new metal complexes with different geometric shape. The formation of Schiff base complexes and also the origin Schiff base is indicated using LC-Mass that manifest the obtained molar mass, FT-IR proved the occurrence of coordination through N of azobenzene and O of OH by observing the shifting in azomethines band and appearing of M-N and N-O bands. Moreover, we can also detect by such apparatus, the presence of aquatic water molecule inside the coordination sphere. UV-Vis spectra of all resultants reveale
... Show MoreThe influence of different thickness (500,750, and 1000) nm on the structure properties electrical conductivity and hall effect measurements have been investigated on the films of copper indium selenide CuInSe2 (CIS) the films were prepared by thermal evaporation technique on glass substrates at RT from compound alloy. The XRD pattern show that the film have poly crystalline structure a, the grain size increasing with as a function the thickness. Electrical conductivity (σ), the activation energies (Ea1,Ea2), hall mobility and the carrier concentration are investigated as function of thickness. All films contain two types of transport mechanisms of free carriers increase films thickness. The electrical conductivity increase with thickness
... Show MoreCuInSe2 (CIS)thin films have been prepared by use vacuum thermal evaporation technique, of 750 nm thickness, with rate of deposition 1.8±0.1 nm/sec on glass substrate at room temperature and pressure (10-5) mbar. Heat treatment has been carried out in the range (400-600) K for all samples. The optical properties of the CIS thin films are been studied such as (absorption coefficient, refractive index, extinction coefficient, real and imaginary dielectric constant)by determined using Measurement absorption and transmission spectra. Results showed that through the optical constants we can made to control it is wide applications as an optoelectronic devices and photovoltaic applications.