The structural properties of ternary chalcopyrite AgAlSe2 compound alloys and thin films that prepared by the thermal evaporation method at room temperature on glass substrate with a deposition rate (5±0.1) nm s-1 for different values of thickness (250,500 and 750±20) nm, have been studied, using X-ray diffraction technology. As well as, the optical properties of the prepared films have been investigated. The structural investigated shows that the alloy has polycrystalline structure of tetragonal type with preferential orientation (112), while the films have amorphous structure. Optical measurement shows that AgAlSe2 films have high absorption in the range of wavelength (350-700 nm). The optical energy gap for allowed direct transition were evaluated, which decreases with film thickness increasing, i.e. it decreases from 2.5 eV to 2.2 eV when thickness varies from 250±20 nm to 750±20 nm.
Tensile , thermal, and barrier properties of polylactide PLA-based
nanocomposite films that were prepared by solvent casting method with
polyethylene glycol (PEG), and alumina were studied. PLA/PEG blend showed
decrease in tensile strength and Young modulus but increased in elongation in
PLA/PEG and increased in crystalline of PLA but decrease in glass transition
temperature with the increasing of PEG concentration . A nano blend composites of
PLA/PEG/alumina (50/50/4) when compared to PLA/PEG blend indicated that
tensile strength , Young modulus and glass transition temperature (Tg) increased
with adding alumina nano particles, concentration and barrier properties
improvement due to its nucleating and reinforc
Abstract: Tin oxide thin films were deposited by direct current (DC) reactive sputtering at gas pressures of 0.015 mbar – 0.15 mbar. The crystalline structure and surface morphology of the prepared SnO2 films were introduced by X-ray diffraction (XRD) and atomic force microscopy (AFM). These films showed preferred orientation in the (110) plane. Due to AFM micrographs, the grain size increased non-uniformly as the working gas pressure increased.
In dental and medical applications, poly-methyl methacrylate (PMMA) has been widely accepted due to the excellent biocompatibility and easy fabrication. Yet, some of the physical and mechanical characteristics of this compound are considered inferior. Seven groups of PMMA nano-composite samples were reported to be fabricated at laboratory temperature . These samples could be used in manufacturing the complete or partial maxillary denture base. The aim of this research is to prepare nano-composite materials which consist of PMMA as a matrix material and two different types of powder (prepared nanoparticles of SnO2 and natural egg shell powder (ESP)) as strengthening materials. The selected additives were used in many cases as p
... Show MoreThis study involves the design of 24 mixtures of fiber reinforced magnetic reactive powder concrete containing nano silica. Tap water was used for 12 of these mixtures, while magnetic water was used for the others. The nano silica (NS) with ratios (1, 1.5, 2, 2.5 and 3) % by weight of cement, were used for all the mixtures. The results have shown that the mixture containing 2.5% NS gives the highest compressive strength at age 7 days. Many different other tests were carried out, the results have shown that the carbon fiber reinforced magnetic reactive powder concrete containing 2.5% NS (CFRMRPCCNS) had higher compressive strength, modulus of rupture, splitting tension, str
... Show MoreThe major target of this paper is to study a confirmed class of meromorphic univalent functions . We procure several results, such as those related to coefficient estimates, distortion and growth theorem, radii of starlikeness, and convexity for this class, n additionto hadamard product, convex combination, closure theorem, integral operators, and neighborhoods.
The calcination treatments and a binder of poly acrylic acid PAA (1wt%)
effects on kaolinite particles were investigated through dielectric properties at
1MHz ,quantitative analysis of X-ray diffraction and microstructure. The calcinated
samples at 850°C/3hr and fired at 1350°C/2hr were revealed decrease in broadening
(Full Width at half maximum) FWHM and increase of dielectric constant.
Nanostructured tin dioxide (SnO2) thin films were prepared by thermal oxidation of Sn, which were ground and embedded in methanol then it was deposited on a glass substrate utilizing casting method. The deposited films were examined for their morphology, and crystal structure by transmission electron microscopy (TEM) scanning electron microscopy (SEM), and X-ray diffraction (XRD) technique. In most cases, it was found that SnO2 thin films had a tetragonal phase, predominantly grown on preferred (110) and (200) planes. The deposited thin films have grain size was about 82 nm. The sensing properties of SnO2against NO2 gas were studied as a function of working temperature and time under optimal co
... Show MoreThe aim of this work is to evaluate some mechanical and physical
properties (i.e. the impact strength, hardness, flexural strength,
thermal conductivity and diffusion coefficient) of
(epoxy/polyurethane) blend reinforced with nano silica powder (2%
wt.). Hand lay-up technique was used to manufacture the composite
and a magnetic stirrer for blending the components. Results showed
that water had affected the bending flexural strength and hardness,
while impact strength increased and thermal conductivity decreased.
In addition to the above mentioned tests, the diffusion coefficient
was calculated using Fick’s 2nd law.
The primary purpose of this paper is to introduce the, N-coprobabilistic normed space, coprobabilistic dual space of N-coprobabilistic normed space and give some facts that are related of them.
A comprehensive practical study of typical mechanical properties of welded Aluminum alloy AA7020-T6 (Al-Mg-Zn), adopting friction stir welding (FSW) technique and conventional metal inert gas (MIG) technique, is well achieved in this work for real comparison purposes. The essences of present output findings were concentrated upon the FSW samples in respect to that MIG ones which can be summarized in the increase of the ultimate tensile strength for FSW was 340 MPa while it was 232 MPa for MIG welding, where it was for base metal 400 MPa. The minimum microhardness value for FSW was recorded at HAZ and it was 133 HV0.05 while it was 70 HV0.05 for MIG weld at the welding metal. The FSW produce 2470 N higher than MIG welding in the bending t
... Show More