In this work, we are Study the effect of annealing temperature on the structure of a-Ge films doped with Sb and the electrical properties of a-Ge:Sb/c-Si heterojunction fabricated by deposition of a-Ge:Sb film on c-Si by using thermal evaporation. Electrical properties of aGe:Sb/c-Si heterojunction include I-V characteristics in dark at different annealing temperatures and C-V characteristics and with the C-V characteristics suggest that the fabricated heterojunction was abrupt type, built in potential determined by extrapolation from 1/C2-V curve and show that the built - inpotential (Vbi) for the Ge:Sb/Si system increases with the increase of annealing temperatures
Stable isotopes 18O/16O and 13C/12C in the carbonate rocks of the Mishrif Formation are examined here to define the depositional characters in the basin includes paleo temperatures and paleo depth. The Mishrif formation (Cenomanian – Early Turonian) has extensive distribution in Iraq and Middle East. Mishrif Formation composed of organic detrital limestone. Four boreholes in four oilfields, Noor – well (11), Amarah – well (14), Buzurgan – well (24), Halfaya – well (8), in south east of Iraq have been studied. The studied samples have negative δ18O isotope values studied well, with Average (-4.11‰), (-4.47‰), (-4.48‰), (-4.18‰) in the studied wells res
... Show MoreThe activation and reaction energies of the C-C and C-H bonds cleavage in pyrene molecule are calculated applying the Density Functional Theory and 6-311G Gaussian basis. Different values for the energies result for the different bonds, depending on the location of the bond and the structure of the corresponding transition states. The C-C bond cleavage reactions include H atom migration, in many cases, leading to the formation of CH2 groups and H-C≡C- acetylenic fragments. The activation energy values of the C-C reactions are greater than 190.00 kcal/mol for all bonds, those for the C-H bonds are greater than 160.00 kcal/mol. The reaction energy values for the C-C bonds range between 56.497 to 191.503 kcal/mol. As for the C-H cleavage rea
... Show MoreThe UN organization is considered one of the most important organizations at the international level. It has accomplished multiple tasks and roles of many different issues and events that hit the developing and advanced world countries. It has performed a series of procedures and laws that have had an impact on ending the wars and conflicts that plagued some countries and continued for a period of time in the past. Moreover, it has improved the level of the international relations between a number of countries due to the problems and incidents took place between them. It has relied on finding solutions and treatments for humanitarian problems such as the preservation of the environment, preventing the spread of epidemics and diseases Thi
... Show MoreThe (NiTsPc) thin films operating by vacuum evaporation technique are high recital and good desirable for number of applications, were dumped on glass substrates at room temperature with (200±20nm) thickness and doped with Al at different percentage (0.01,0.03) besides annealing the sample with 200˚C for 1 hours . The stimuluses of aluminum dopant percentage on characterization of the dropped (Ni Ts Pc) thin films were studied through X-ray diffraction in addition from the attained results, were all the films have polycrystalline in nature, as well the fallouts of XRD aimed at film illustrations polycrystalline, depending on the Al ratio doping, the results, SEM exposed the surface is regularly homogeneous. Utilizing first-ideolog
... Show MoreIn this work, the influence of the annealing temperature on the optical properties of the thin films Cadmium Sulphide (CdS) has been studied. Thin films of Cadmium Sulphide (CdS) were made using the Physical Vapor Deposition (PVD) method. The optical properties of annealing temperatures (as deposited, 200, 250, and 300 ) were scrupulous. The UV/VIS spectrophotometer investigated optical parameters such as transmission, the coefficient of absorption and energy gap of the films for the range (400-110 nm) as an assignment of the annealing temperature. The optical properties were calculated as a function of annealed temperature: absorption, transmission, reflection, band gap, coefficient of absorp
... Show MoreIn this study, Mn-Ni Ferrite was prepared by using two composites of manganese ferrite ( MnFe2o4 ) and Nicle Ferrite ( NiFe2O4) tested by X-Ray diffraction (XRD) method. The dielectric constant (ðœ€Ì…) and the dielectric loss tangent (ð‘¡ð‘Žð‘› ð›¿) were studied for the ferrite system prepared at different frequencies (100, 200… and 5000 kHz). It was found that the values of (ðœ€Ì…) and (ð‘¡ð‘Žð‘› ð›¿) decrease with the increase of frequencies.
The structural, optical properties of cupper indium gallium selenite (CuIn1-xGaxSe) have been studied. CuIn1-xGaxSe thin films for x=0.6 have been prepared by thermal evaporation technique, of 2000±20 nm thickness, with rate of deposition 2±0.1 nm/sec, on glass substrate at room temperature. Heat treatment has been carried out in the range (373-773) K for 1 hour. It demonstrated from the XRD method that all the as-deposited and annealed films have polycrystalline structure of multiphase. The optical measurement of the CIGS thin films conformed that they have, direct allowed energy gap equal to 1.7 eV. The values of some important optical parameters of the studied films such as (absorption coefficient, refractive index, extinction coeffici
... Show MoreThe CdSe pure films and doping with Cu (0.5, 1.5, 2.5, 4.0wt%) of thickness 0.9μm have been prepared by thermal evaporation technique on glass substrate. Annealing for all the prepared films have been achieved at 523K in vacuum to get good properties of the films. The effect of Cu concentration on some of the electrical properties such as D.C conductivity and Hall effect has been studied.
It has been found that the increase in Cu concentration caused increase in d.c conductivity for pure CdSe 3.75×10-4(Ω.cm)-1 at room temperatures to maximum value of 0.769(Ω.cm)-1 for 4wt%Cu.All films have shown two activation energies, where these value decreases with increasing doping ratio. The maximum value of activation energy was (0.319)eV f