The work is concerned with the characterization of as cast films of neat and UV-stabilized nylon 6,6 by employing FTIR measurements. Band assignment is made for neat and UVstabilized nylon 6,6 using FTIR spectra confirm their molecular structure. UV-stabilizer added to nylon 6,6 has caused reduction in the absorbance of the vibrational bands and thus stabilizes the behavior of the polymer in the end and uses specially in harsh environment.
In this paper, a miniaturized 2 × 2 electro-optic plasmonic Mach– Zehnder switch (MZS) based on metal–polymer–silicon hybrid waveguide is presented. Adiabatic tapers are designed to couple the light between the plasmonic phase shifter, implemented in each of the MZS arms, and the 3-dB input/output directional couplers. For 6 µm-long hybrid plasmonic waveguide supported by JRD1 polymer (r33= 390 pm/V), a π-phase shift voltage of 2 V is obtained. The switch is designed for 1550 nm operation wavelength using COMSOL software and characterizes by 2.3 dB insertion loss, 9.9 fJ/bit power consumption, and 640 GHz operation bandwidth
A thin CdS Films have been evaporated by thermal evaporation technique with different thicknesses (500, 1000, 1500 and 2000Å) and different duration times of annealing (60, 120 180 minutes) under 573 K annealing temperature, the vacuum was about 8 × 10-5 mbar and substrate temperature was 423 K. The structural properties of the films have been studied by X- ray diffraction technique (XRD). The crystal growth became stronger and more oriented as the film thickness (T) and duration time of annealing ( Ta) increases.
Copper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show MoreIn this work, we study the effect of doping Sn on the structural and optical properties of pure cadmium oxide films at different concentrations of Tin (Sn) (X=0.1,0.3 and 0.5) .The films prepared by using the laser-induced plasma at wavelength of laser 1064 nm and duration 9 ns under pressure reached to 2.5×10-2 mbar. The results of X-ray diffraction tests showed that the all prepared films are polycrystalline. As for the topography of the films surface, it was measured using AFM , where the results showed that the grain size increases with an increase in the percentage of doping in addition to an increase in the average roughness. The optical properties of all films have also been studied through the absorbance s
... Show MoreThe optical energy gap(Eopt) and the width of the tails of localized states in the band gap (?E) for Se:2%Sb thin films prepared by thermal co-evaporation method as a function of annealing temperature are studied in the photon energy range ( 1 to 5.4)eV.Se2%Sb film was found to be indirect transition with energy gap of (1.973,2.077, 2.096, 2.17) eV at annealing temperature (295,370,445,520)K respectively. The Eopt and ?E of Se:2%Sb films as a function of annealing temperature showed an increase in Eopt and a decrease in ?E with increasing the annealing temperature. This behavior may be related to structural defects and dangling bonds.
Alloys of Bi2[Te1-x Sex]3 were prepared by melting technique with different values of Se percentage (x=0,0.1,0.3,0.5,0.7,0.9 and 1). Thin films of these alloys were prepared by using thermal evaporation technique under vacuum of 10-5 Torr on glass substrates, deposited at room temperature with a deposition rate (12nm/min) and a constant thickness (450±30 nm). The concentrations of the initial elements Bi, Te and Se in the Bi2 [Te1-x Sex]3 alloys with different values of Se percentage (x), were determined by XRF,The morphological and structural properties were determined by AFM and XRD techniques. AFM images of Bi2[Te1-x Sex]3 thin films show that the average diameter and the average surface roughness inc
... Show MoreThe V2O5 films were deposited on glass substrates which produce using "radio frequency (RF)"power supply and Argon gas technique. The optical properties were investigated by, UV spectroscopy at "radio frequency" (RF) power ranging from 75 - 150 Watt and gas pressure, (0.03, 0.05 and 0.007 Torr), and substrate temperature (359, 373,473 and 573) K. The UV-Visible analysis shows that the average transmittance of all films in the range 40-65 %. When the thickness has been increased the transhumance was decreased from (65-40) %. The values of energy band gap were lowered from (3.02-2.9 eV) with the increase of thickness the films in relation to an increase in power, The energy gap decreased (2.8 - 2.7) eV with an increase in the pressure and
... Show MorePeroxidase is a class of oxidation-reduction reaction enzyme that is useful for accelerating many oxidative reactions that protect cells from the harmful effects of free radicals. Peroxidase is found in many common sources like plants, animals and microbes and have extensive uses in numerous industries such as industrial, medical and food processing. In this study, P. aeruginosa was harvested to utilize and study its peroxidases. P. aeruginosa was isolated from a burn patient, and the isolate was verified as P. aeruginosa using staining techniques, biochemical assay, morphological, and a sensitivity test. The gram stain and biochemical test result show rod pink gram-ne
... Show More