In this work , impact strength and the water absorption ratio of powders of white and brown local chicken eggshell reinforced epoxy with different volume fractions ( 1 , 2 , 3 , 4 and 5 % ) were studied . The experimental results show that composite filled by ( 1 % Vol . )of white eggshell powder exhibited maximum impact strength and high resistance to tape water , so we choose this volume fraction to use the epoxy composite in coating . Optical microscopic observations are taken to develop a better understanding of the phenomena taking place in the material system at microscopic level .
The study aimed to investigate the effect of using the intructional computer individually or through the cooperative groups on the achievement of the ninth grade students in mathematics compared to the traditional method. The experimental method adapted three groups out of three schools were chosen, two groups of the students where applied the computer method. The comtrol group used the simple random method, and it used the diagnostic test as tool for the study.The result showed that there is a statistically significant difference between the mean scores of the experimental groups and the control group on the post-test for the two experimental groups.
In this work optical window for infrared region was prepared by using Aluminum Oxide (Al2O3)material as antireflection coating on ZnSe substrate which covers the atmospheric window 3-5µm. the maximum transition was 97% at a wavelength 0f 4.4µm.
The nonlinear refractive index and the nonlinear absorption coefficient of unmodified and functional poly(methyl methacrylate) PMMA films were studied before and after the addition of the filler by the z-scan technique, using a Q-switched Nd:YAG laser at two wavelengths: 532 nm and 1064 nm, and at three input energies (13, 33 and 53) mJ. Both linear and nonlinear refractive indices and absorption coefficients of polymer films were studied by using UV-VIS spectrophotometer. The results show that the creation of functional PMMA from unmodified PMMA will increase the nonlinear optical properties in the functional PMMA/copper matrix more than in the unmodified PMMA/copper matrix. Hence, the functional PMMA appears promising as a useful third
... Show MoreThe effects of reinforcing polymers with glass and graphite particles on enhancing their flexural properties are investigated. Five composites were fabricated using the same polymer matrix material with different volume fractions of reinforcement particles. They comprise glass particles and graphite particles each having volume fractions of 20% and 30% as well as a hybrid composite having 10% glass and 10% graphite. Three-point bending tests using a Universal Testing Machine were carried out on specimens of the above mentioned composites, as well as specimens of the polymer matrix material to determine their flexural properties. The experimental test results indicate that the flexural stiffness of all the composites wer
... Show MoreThe ceramic composite with different proportions of clay and silica was prepared with a grain size of 70 μm and the weight percentage was selected for four groups (clayx silica100-x) were x q15, 25, 30 and 50. In this manuscript, for each pressured sample, a sintering procedure was carried out for 3 hours under static air and at various sintering temperatures (1000, 1100, 1200, 1400)°C. After sintering, the density, porosity, water absorption, compression strength and thermal conductivity were measured. The best results were obtained using a mixture of 15% clay and 85% silica which were sintering at 1400°C for three hours under air.
This paper aims to study the damage generated due to creep-fatigue interaction behaviors in solid polyamide 6,6 and its composites that include 1%wt of carbon nanotubes or 30% wt short carbon fiber prepared by an injection technique. The investigation also includes studying the influence of applied temperatures higher than the glass transition temperatures on mechanical properties. The obtained results showed that the addition of reinforcement materials increased all the mechanical properties, while the increase in test temperature reduced all mechanical properties, especially for polyamide 6,6. The creep-fatigue interaction resistance also improved due to the addition of reinforcement materials by inc
... Show MoreIn this study, polyester composites reinforced with pistachio shells powder (P.) with an average
diameter (150 – 200 μm) with different weight ratios (0.5%, 1%, 1.5%, 2%, and 2.5%) were
prepared to the resin. The Shore D hardness, thermal conductivity (K), and the glass transition
temperature (Tg) of the samples were examined. The results showed that the Shore D hardness
increases with the increase of the reinforcement ratio and its maximum value is (87.55) at (2.5%
P.) While the value of hardness at (0%) is (86.5). The thermal conductivity increases slightly with
the increase in the percentage of reinforcement and its maximum value is (0.213253 W/ m. K) at
(2.5% P.), while the value of K at (0% P.)
This research estimates the effect of independent factors like filler (3%, 6%, 9%, 11% weight fraction), normal load (5N, 10N, 15N), and time sliding (5,7 , 9 minutes) on wear behavior of unsaturated polyester resin reinforced with jute fiber and waste eggshell and, rice husk powder composites by utilizing a statistical approach. The specimens polymeric composite prepared from resin unsaturated polyester filled with (4% weight fraction) jute fiber, and (3%, 6%, 9%, 11% weight fraction) eggshell, and rice husk by utilizing (hand lay-up) molding. Dry sliding wear experiments were carried utilizing a standard (pin on disc test setup) following a well designed empirical schedule that depends on Taguchi’s experimental design L9 (MINIT
... Show MoreThis research studyies wear rate of composite materials by using Epoxy Resin and Polyurethane Rubber as a matrix of weigt percentage (90:10) (Ep/Pu) and reinforced by PVC fibers and Aluminum fibers two dimension knitted mat with fractional volume(15 %), in different conditions like: lab conditions and after submerge the samples in water for different periods of time. . four kinds of materials were prepared: (Ep+pu), (Ep+Pu+PVC), (Ep+Pu+Al.F), (Ep+Pu+PVC+Al. F) .And the results have shown that the best wear resistance are for the hybrid composite material (Ep + Pu+ PVC + Al. F) and wear rate of all samples increased when it was submerged in water