In this work, the total linear attenuation coefficients µ(cm
-1
) were calculated and studied
for particulate reinforced polymer-based composites. Unsaturated polyester (UP) resin was
used as a matrix filled with different concentrations of Al, Fe, and Pb metal powders as
reinforcements. The effect of the metal powders addition at different weight percentages in
the range of (10,20,30,40,50)wt % and gamma energy on attenuation coefficients was studied.
The results show, as the metallic particulates content increase, the attenuation coefficients will
increase too, while it, were exhibited a decrease in their values when the gamma energy
increase.The total linear attenuation coefficients of gamma ray for 15 composites have been
calculated using the XCOM program (version 3.1) in the energy range of 0.1-20 MeV.
Anew Solar concentrator have been designed in this paper, this concentrators Were based on the total internal reflection in a prism, the prism angles has been calculated by depending on the solar incident ray angle in baghdad for a year. The optical design consist ofa triangular presume, Where the solar cells on one side of the prism Wh?le the prism head towered the south. The results show that there is an increasing in the solar ray concentrators and the cell area is reduced.
This research adopts the estimation of mass transfer coefficient in batch packed bed distillation column as function of physical properties, liquid to vapour molar rates ratio (L / V), relative volatility (α), ratio of vapour and liquid diffusivities (DV / DL), ratio of vapour and liquid densities (ρV / ρL), ratio of vapour and liquid viscosities (μV/ μL).
The experiments are done using binary systems, (Ethanol Water), (Methanol Water), (Methanol Ethanol), (Benzene Hexane), (Benzene Toluene). Statistical program (multiple regression analysis) is used for estimating the overall mass transfer coefficient of vapour and liquid phases (KOV and KOL) in a correlation which represented the data fairly well.
KOV = 3.3 * 10-10
... Show MoreBackground: Because of the demands for aesthetic orthodontic appliances have increased, aesthetic archwires have been widely used to meet patient's aesthetic needs. The color stability of aesthetic archwires is clinically important, any staining or discoloration will affect patient’s acceptance and satisfaction. This study was designed to evaluate the color stability of different types of aesthetic archwires after immersion into different types of mouth washes. Materials and methods: Four brands of nickel titanium coated aesthetic arch wires: Epoxy coated (Orthotechnology and G&H) and Teflon coated (Dany and Hubit) were evaluated after 1 week, 3 weeks and 6 weeks of immersion into two types of mouthwashes (Listerine with alcohol and
... Show MoreStudy the effect of doping V2O5 on polymers poly vinyl alcohol ( PVA), poly vinyl pyrrolidone (PVP) on the optical and structural properties for film prepared by using Casting method at thickness( 300±20)nm ,All the materials dissolved in distilled water by magnetic mixer for one hour .The optical parameters measured by using UV-VIS spectrometer ,and the structural parameters measured by X-ray diffraction .when measured the energy gap found that the value was decreases from 4.6 eV to 2.98 eV with doping .The refractive index ,extinction coefficient ,absorption coefficient ,real and imaginary dielectric constants of (PVA/PVP) are increasing with doping by V2O5 and wit
... Show MoreIn this study, aluminum alloyAA6061-T6 was joined by a hot press process with three types of material; polyamide PA 6.6 (nylon), 1% carbon nanotube/PA6.6 and 30% carbon fiber/PA6.6 composites. Three parameters were considered in the hot pressing; temperature (180, 200 and 220°C), pressure (2, 3, 4, 5 and 6 bar) and time of pressing (1, 2, 3, 4 and 5 minutes for 200ºC, and 0.25, 0.5, 0.75, 1 and 1.25 minutes for220ºC). Applied pressure has great effect on shear strength of the joint, corresponding to bonding time and temperature. Maximum shear strength was 8.89MPa obtained for PA6.6 at bonding conditions of 4 bar, 220ºC and 0.75 minute. For 30% carbon fiber/PA6,6 shear recorded was
The compound [K1] was synthesized from the reaction of dichloromethane with linear alkyl benzene (Lab9) using ethanol as a solvent, and from(chloro methyl)-4-nonylbenzene) [K1] it was possible to synthesize the compound Z(4-(nonan-3-yl)phenyl) methane amine) [K2] containing the amine group by synthesized from [K2] reaction with appropriate phenolic aldehydes and using Ethanol as a solvent in the preparation of vinyl chloride4-(((4-nonylbenzyl)imino)methyl)phenol-4-(((4-nonylbenzyl)imino methyl)benzene-1,3diol) [K3-K4] bases has been used. Preparation of a number of Phenolic polymers4-(2- hydroxy-3.5-dimethylbenzyl)-2-methyl-6-(((4-4-(2hyroxy-3, 5-dimethylbenzyl)-2-methyl-6(((4 nonylbenzyl) imino) methyl) benzene-phenolnonylbenzyl) imino) me
... Show MoreA theoretical calculation of the binding and excitation energies have been used at low – lying energies based on shell model and quantum theory. In this model, we evaluated the energies under assume Ni 28 56 30 as inert core with two nucleon extra, nucleons in the 2P3/2 , 1f 5/2 and 2P1/2 configuration. Modified Surface Delta Interaction (MSDI) and Reid's Potential (RP) theory for two body matrix elements are evaluated by using a Matlab program to calculate the energies of experimental and Reid single particle energies. Our results of the theoretical calculation have been compared with the experimental results, which show no good agreement with the experiment but have a good agreement wit
... Show MoreIn this research, damping properties for composite materials were evaluated using logarithmic decrement method to study the effect of reinforcements on the damping ratio of the epoxy matrix. Three stages of composites were prepared in this research. The first stage included preparing binary blends of epoxy (EP) and different weight percentages of polysulfide rubber (PSR) (0%, 2.5%, 5%, 7.5% and 10%). It was found that the weight percentage 5% of polysulfide was the best percentage, which gives the best mechanical properties for the blend matrix. The advantage of this blend matrix is that; it mediates between the brittle properties of epoxy and the flexible properties of a blend matrix with the highest percentage of PSR. The second stage
... Show MoreThe current work is concerned with preparing cobalt manganese ferrite (Co1-xMnxFe2O4) with different concentrations of cobalt and manganese (x=0.2, 0.4, and 0.6) and decorating it with polyaniline (PAni) for use in supercapacitive applications. The results of the X-ray diffraction (XRD) manifested a broad peak of PAni and a cubic structure of cobalt manganese ferrite having crystal size between 60 nm and 138 nm, which decreases with increasing concentration of Mn. The field emission scanning electron microscopy (FESEM) images evidenced that the PAni has nanofiber (NF) structures, according to the method of preparation, where the hydrothermal method was used. The magnetic properties of the prepared ferrite, as well as the prepared PAni/Co1-x
... Show More