Biomimatic basic calcium phosphate ,known as Hydroxy apatite(HA), was
synthesised using calcium acetate and disodium phosphate dilute hot (boiling) solution of
both salts were added slowly to each other. A colloidal suspension formed was aged for few
days, then boiled for one hour to induced setting and coagulation of preapatite, and left to cool
until they reached room temperature.
The precipitate was filtered and washed with distilled water, then ethanol and dried.
The dried sample was calcined at 1100
o
C.The obtained solid lumps were then crushed
reground fine powder and analyzed for calcium to phosphorous ratio. X-ray analysis was
carried out to examine the solid sample. Chemical analysis for phosphorus and calcium had
been carried out using standard method.
The results proved that the calcined sample used in this investigation where Hydroxyapatite .
The accountants are preparing the financial statements under the Monetary Unit Stability Assumption without taking into consideration the changement of prices for the monetary unit. The income statement accounts containing different items of expenses and revenues. These items are not paid or obtained at one date, because the value of monetary unit is changing from one date to another , also the financial position contains different items of current and fixed assets, also contains different items of long-term liabilities and ownership rights, the continuity of applying historical cost principle will make the financial statements misleading, The adoption of financial analyst of these statements will affects
... Show MoreIn this work, prepared new ligand namely 5-(2,4-dichloro-phenyl)-1,3,4-oxadiazole-2-(3H)-thion, was obtained from the 2,4-dichlorobenzoyl chloride with hydrazine, after that reaxtion with CS2/KOH in methanol.
Breast cancer is the most common malignancy in female and the most registered cause of women’s mortality worldwide. BI-RADS 4 breast lesions are associated with an exceptionally high rate of benign breast pathology and breast cancer, so BI-RADS 4 is subdivided into 4A, 4B and 4C to standardize the risk estimation of breast lesions. The aim of the study: to evaluate the correlation between BI-RADS 4 subdivisions 4A, 4B & 4C and the categories of reporting FNA cytology results. A case series study was conducted in the Oncology Teaching Hospital in Baghdad from September 2018 to September 2019. Included patients had suspicious breast findings and given BI-RADS 4 (4A, 4B, or 4C) in the radiological report accordingly. Fine needle aspirati
... Show MoreHybrid architecture of ZnO nanorods/graphene oxide ZnO-NRs@GO synthesized by electrostatic self-assembly methods. The morphological, optical and luminescence characteristics of ZnO-NRs@GO and ZnO-NRs thin films have been described by FESEM, TEM, HRTEM, and AFM, which refers to graphene oxide have been coated ZnO-NRs with five layers. Here we synthesis ZnO-NRs@GO by simple, cheap and environmentally friendly method, which made it favorable for huge -scale preparation in many applications such as photocatalyst. ZnO-NRs@GO was applied as a photocatalyst Rodamin 6 G (R6G) dye from water using 532 nm diode laser-induced photocatalytic process. Overall degradation of R6G/ ZnO-NRs@GO was achieved after 90 minutes of laser irradiation while it ne
... Show MoreIn this work, porous silicon gas sensor hs been fabricated on n-type crystalline silicon (c-Si) wafers of (100) orientation denoted by n-PS using electrochemical etching (ECE) process at etching time 10 min and etching current density 40 mA/cm2. Deposition of the catalyst (Cu) is done by immersing porous silicon (PS) layer in solution consists of 3ml from (Cu) chloride with 4ml (HF) and 12ml (ethanol) and 1 ml (H2O2). The structural, morphological and gas sensing behavior of porous silicon has been studied. The formation of nanostructured silicon is confirmed by using X-ray diffraction (XRD) measurement as well as it shows the formation of an oxide silicon layer due to chemical reaction. Atomic force microscope for PS illustrates that the p
... Show MoreBiodiesel can be prepared from various types of vegetable oils or animal fats with the aid of a catalyst.
Calcium oxide (CaO) is one of the prospective heterogeneous catalysts for biodiesel synthesis. Modification
of CaO by impregnation on silica (SiO2) can improve the performance of CaO as catalyst. Egg shells and rice
husks as biomass waste can be used as raw materials for the preparation of the silica modified CaO catalyst.
The present study was directed to synthesize and characterize CaO impregnated SiO2 catalyst from biomass
waste and apply it as catalyst in biodiesel synthesis. The catalyst was synthesized by wet impregnation
method and characterized by x-ray diffraction, x-ray fluorescence, nitr
A new Macrocyclic Schiff base ligand Bis[4-hydroxy(1,2-ethylene-dioxidebenzylidene) pheylenediamine] [H2L] and its complexes with (Co(II) , Ni(II) , Cu(II) , Zn(II) and Cd(II)) are reported . The ligand was prepared in two steps,in the first step a solution of (o-phenylene diamine) in methanol react under reflux with (2,4-dihydroxybenzylaldeyed) to give an (intermediatecompound) [Bis-1,2 (2,4-dihydroxybenzylediene)pheylinediamine] which react in the second step with (1,2- dichloro ethane) giving the mentioned ligand.Then the complexes were synthesis of adding of corresponding metal salts to the solution of the ligand in methanol under reflux with 1:1 metal to ligand ratio. On the basis of, molar conductance, I.R., UV-Vis, chloride content a
... Show MoreObjective: The purpose of this work was to develop and optimize the emulgel formulation of piroxicam with two types of gelling agent chitosan and xanthan gum. The release profiles of prepared formulas were investigated. In addition, the rheology and stability of the best formula were investigated.Methods: Emulsified piroxicam was prepared to use oleic acid, tween 80 and PG with a ratio (3:10:10). In xanthan based emulgel, the xanthan gum (1% and 1.5%) was spread as powder on emulsified piroxicam with stirring until emulgel was formed. In chitosan-based emgels, Chitosan gel was added to emulsified piroxicam and stirring until the Emulgel was constructed. Chitosan gels were prepared by incorporating different concentration, 2%, 3%, 6%
... Show More