The thermal degradation of cable ties of polyamide (PA6,6) neat and UV stabilized was investigated by thermogravimetry (TG) and its derivative (DTG) at several heating rates between 5 and 80 oC min-1 in helium atmosphere. High heating rates signal novel peaks in the DTG curves that indicate melting temperature of PA6,6. The kinetic parameters calculated via isoconversion and nonisothermal data using the Flynn-Wall-Ozawa, Kissinger and CoatsRedfern methods showed comparable activation energy values. Exposure of the ties to outdoor environment causes pre-mature stress cracking and brittle failure due to prevalence of crosslinking reaction occurring in the polymer chains
Polyaromatic hydrocarbons (PAHs) are a group of aromatic compounds that contain at least two rings. These compounds are found naturally in petroleum products and are considered the most prevalent pollutants in the environment. The lack of microorganism capable of degrading some PAHs led to their accumulation in the environment which usually causes major health problems as many of these compounds are known carcinogens. Xanthene is one of the small PAHs which has three rings. Many xanthene derivatives are useful dyes that are used for dyeing wood and cosmetic articles. However, several studies have illustrated that these compounds have toxic and carcinogenic effects. The first step of the bacterial degradation of xanthene is conducted by d
... Show MoreThe major objectives of this research are to analyze the behavior of road embankments
reinforced with geotextiles constructed on soft soil and describe the finite element analysis by using
ANSYS program ver. (5.4). The ANSYS finite element program helps in analyzing the stability of
geo- structure (embankment) in varied application of geotextiles reinforcement to enhance the best
design for embankment.
The results of analysis indicate that one of the primary function of geotextiles reinforcement was to
reduce the horizontal displacement significantly. With the inclusions of reinforcement, the horizontal
displacement reduced by about (81%), while the vertical displacement reduced by (32%). The effect
of geotextiles
Isolated Bacteria from the roots of barley were studied; two stages of processes Isolated and screening were applied in order to find the best bacteria to remove kerosene from soil. The active bacteria are isolated for kerosene degradation process. It has been found that Klebsiella pneumoniae sp. have the highest kerosene degradation which is 88.5%. The optimum conditions of kerosene degradation by Klebsiella pneumonia sp. are pH5, 48hr incubation period, 35°C temperature and 10000ppm the best kerosene concentration. The results 10000ppm showed that the maximum kerosene degradation can reach 99.58% after 48 h of incubation. Higher Kerosene degradation which was 99.83% was obtained at pH5. Kerosene degradation was found to be maximum at 3
... Show MoreIsolated Bacteria from the roots of barley were studied; two stages of processes Isolated and screening were applied in order to nd the best bacteria to remove kerosene from soil. The acve bacteria are isolated for kerosene degradaon process. It has been found that Klebsiella pneumoniae sp. have the highest kerosene degradaon which is 88.5%. The opmum condions of kerosene degradaon by Klebsiella pneumonia sp. are pH5, 48hr incubaon period, 35°C temperature and 10000ppm the best kerosene concentraon. The results 10000ppm showed that the maximum kerosene degradaon can reach 99.58% aer 48 h of incubaon. Higher Kerosene degradaon which was 99.83% was obtained at pH5. Kerosene degradaon was found
... Show MoreCopper (1) oxide nanoparticles together with matrix polymers of polyvinyl alcohol (PVA) and polyaniline (PANI) composite films were synthesized, as these materials are of importance in optoelectronic applications. Nanoparticles of Cu2O were produced by chemical precipitation. Polymerization of aniline was carried out through polymerization in an acidic medium. Structural, thermal, and optical properties of PVA+PANI/Cu2O nanocomposite were inspected by x-ray diffraction (XRD), scanning electron microscopy (SEM), fourier-transform infrared (FTIR), differential scanning calorimeter (DSC) and ultraviolet-visible spectroscopy (UV-Vis spectroscopy). X-ray diffraction peaks at 29.53°, 36.34°, and 42.22° indicated the
... Show MoreAbstract
Paraffin wax is utilized for the heat storage applications taking advantage from the high stored latent heat during the phase change (from solid to fluid) period. What isn't right with this procedure is that the wax has a little heat transfer rate because of its low thermal conductivity. The thermal conductivity improvement of the paraffin wax has been examined utilizing nano-material with high thermal conductivity. In the recent study, (Al2O3) nanoparticles with weights of 1, 2, and 3% of the paraffin wax were added to the paraffin wax. The Iraqi paraffin wax accessible at the local markets was utilized as a phase change material (PCM).
Many properties of the
... Show More