Preferred Language
Articles
/
jih-422
Synthesis Of Nanostructured TiO2 Thin Films By Pulsed Laser Deposition (PLD) And The Effect Of Annealing Temperature On Structural And Morphological Properties
...Show More Authors

  In this work, nanostructured TiO2 thin films were grown by pulsed laser deposition (PLD) technique on glass substrates. TiO2 thin films then were annealed at 400-600 °C in air for a period of 2 hours. Effect of annealing on the structural and morphological were studied. Many growth parameters have been considered to specify the optimum conditions, namely substrate temperature (300 °C), oxygen pressure (10-2 Torr), laser fluence energy density (0.4 J/cm2), using double frequency Q-switching Nd:YAG laser beam (wavelength 532nm), repetition rate  (1-6 Hz) and the pulse duration of 10 ns. The results of the X-ray test show that all nanostructures tetragonal are polycrystalline. These results show that grain size increase from 19.5 nm to 29.5 with the increase of annealing temperature. The XRD results also reveal that the deposited thin film, annealed at 400 °C of TiO2 have anatase phase. Thin films annealed at 500 °C and 600 °C have mixed anatase and rutile phases.  Full Width at Half Maximum (FWHM) values of the (101) peaks of these films decrease from 0.450° to 0.301° with the increase of annealing temperature.  Surface morphology of the thin films have been studied by using atomic force microscopes (AFM). AFM measurements confirmed that the films have good crystalline and homogeneous surface. The Root Mean Square (RMS) value of thin films surface roughness are increased with the increase of annealing temperature

View Publication Preview PDF
Quick Preview PDF
Publication Date
Mon Nov 06 2017
Journal Name
International Conference On Technologies And Materials For Renewable Energy, Environment And Sustainability, Tmrees17, 21-24 April 2017, Beirut Lebanon
HgBa2 Can-1CunO2n+2+δ Superconducting thin films Prepared by Pulsed Laser Deposition
...Show More Authors

In the present work, HgBa2Can-1CunO2n+2+δ superconducting thin films with (100) nm thickness were (n=1, 2 and 3) prepared by Pulsed Laser Deposition technique on glass substrate at R.T (300) K, have been synthesize. The effect of Cu content on the structural, surface morphology, optical and electrical properties of HgBa2Can-1CunO2n+2+δ films were investigated and analyzed. The results of XRD analysis show that all samples are polycrystalline structure with orthorhombic phase, the change of Cu concentration in samples produce changes in the mass density, lattice parameter and the ratio (c/a). AFM techniques were used to examine the surface morphology of HgBa2Can-1CunO2n+2+δ superconducting films, the study showed the values of surface rou

... Show More
Publication Date
Mon Apr 24 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect of Annealing Temperatures on the Structural and Optical Properties of ZnO and ZnO:Al Thin Films Prepared By Thermal Evaporation Technique
...Show More Authors

 We studied the changing of structural and optical properties of pure and Aluminum-doped ZnO thin films prepared by thermal evaporation technique on glass substrates at thickness (800±50)nm with changing of annealing temperatures ( 200,250,300 )℃ for one hour. The investigation of (XRD) indicates that the pure and doped ZnO thin films were polycrystalline of a hexagonal wurtzite structure with preferred orientation along (002) plane. The grain size was decreased with doping before annealing, but after annealing the grain size is increasing with the increase of annealing temperature for pure film whereas for the doped films with ratios 1 %, 2 % we found that the grain size is larger than that before annealing. The grain size

... Show More
View Publication Preview PDF
Publication Date
Mon Apr 24 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Influence of the Annealing Temperature on optical Properties of (CuInSe2) Thin Films
...Show More Authors

  The Influence of annealing temperature on the optical properties of (CuInSe2) thin films was studied. Thermal evaporation in vacuum technique has been used for films deposited on glass substrates, these films were annealed in vacuum at (100C°, 200C°) for (2 hours). The optical properties were studied in the range (300-900) nm. The obtained results revealed a reduction in energy band gap with annealing temperature . optical parameters such as reflectance, refractive index, extinction coefficient, real and imaginary parts of the dielectric constant, skin depth and optical conductivity are investigated before and after annealing. It was found that all these parameters were affected by annealing temperature.
 

View Publication Preview PDF
Publication Date
Thu Jan 01 2015
Journal Name
Journal Of The College Of Basic Education
Effect of Annealing Temperature on the Structure and Optical Properties of CdS: Cu Thin Films Prepard By Thermal Vacuum Evaporation
...Show More Authors

Publication Date
Mon Apr 20 2020
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Annealing Influence on Nanostructure's Optical Properties CdS Thin Films Prepared by Physical Vapor Deposition Technique
...Show More Authors

    In this work, the influence of the annealing temperature on the optical properties of the thin films Cadmium Sulphide (CdS) has been studied. Thin films of Cadmium Sulphide (CdS) were made using the Physical Vapor Deposition (PVD) method. The optical properties of annealing temperatures (as deposited, 200, 250, and 300  ) were scrupulous. The UV/VIS spectrophotometer investigated optical parameters such as transmission, the coefficient of absorption and energy gap of the films for the range (400-110 nm) as an assignment of the annealing temperature. The optical properties were calculated as a function of annealed temperature: absorption, transmission, reflection, band gap, coefficient of absorp

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Thu Dec 28 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
The Effect of Annealing Temperature on the Optical Properties of the a-Ge: As Thin Films
...Show More Authors

a-Ge: As thin films have prepared by thermal evaporation teclmique, then they were annealing at various temperatures within the

range (373-473)  K.   The  result of  X-ray di ffraction spectrum  was showing  that  all  the  specimens  remained  in  amorphous structure before and after annealing  process. This paper studied the effect of annealing  temperature as  a  function of  wavelength on  the optical energy gap and optical constants for the a-Ge:As thin  films . Results have showed that there was an increasing in the optical energy gap

{Egopt) values with the in ,;rcasing of the annealing temperatures within

... Show More
View Publication Preview PDF
Publication Date
Fri Mar 31 2023
Journal Name
2nd International Conference On Mathematical Techniques And Applications: Icmta2021
Annealing effect on structural and optical properties of Sb2S3 thin film
...Show More Authors

The effect of annealing on the structural and optical properties of Antimony trisulfide (Sb2S3) is investigated. Sb2S3 powder is vaporized on clean glass substrates at room temperature under high vacuum pressure to form thin films. The structural research was done with the aid of X-ray diffraction (XRD) and atomic force microscopy (AFM). The amorphous to the polycrystalline transformation of these thin films was shown by X-ray diffraction analysis after thermal annealing. These films' morphology is explained. The absorption coefficient and optical energy gap of the investigated films are calculated using transmission spectra. Both samples have strong absorption in the visible spectrum, according to UV-visible absorption spectra. The optical

... Show More
View Publication Preview PDF
Scopus (5)
Crossref (2)
Scopus Crossref
Publication Date
Wed May 10 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
The Study of Annealing and Dopping Effect of Zn on Structural and Optical Properties for CdTe Thin Films
...Show More Authors

In this research thin films of (CdTe) have been prepared as pure and doped by Zn
with different ratios (1,2,3,4,5)% at thickness (400+25)nm with deposition rate (2±0.1)nm,
deposited on glass substrate at R.T. by using thermal evaporation in vacuum . All samples
were annealed at temperature (523,573,623,673)K at 1h.
The structural prop erties of all prepared thin films, doped and undoped have been
studied by using XRD. The analysis reveals that the structures of the films were
polycrystalline and typed cubic with a preferred orientation along (111) plane for the
undoped films with (2,3)% of zinc , and shifting (2ÆŸ) for doped films . The annealing films
at temperature 573 K and Zn:3% show decreasing in

... Show More
View Publication Preview PDF
Publication Date
Sun Jun 01 2014
Journal Name
Baghdad Science Journal
The Effect of annealing temperature on the optical properties of (Cu2S)100-x( SnS2 )x thin films
...Show More Authors

Thin films of (Cu2S)100-x( SnS2 )x at X=[ 30,40, &50)]% with thickness (0.9±0.03)µm , had been prepared by chemical spray pyrolysis method on glass substrates at 573 K. These films were then annealed under low pressure of(10-2) mbar ,373)423&473)K for one hour . This research includes , studying the the optical properties of (Cu2S)100-x-(SnS2)x at X=[ 30,40, &50)]% .Moreover studying the effect of annealing on their optical properties , in order to fabricate films with high stability and transmittance that can be used in solar cells. The transmittance and absorbance spectra had been recorded in the wavelength range (310 - 1100) nm in order to study the optical properties . It was found that these films had direct optical band

... Show More
View Publication Preview PDF
Crossref
Publication Date
Thu Jun 08 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
The Effect of the (Se) percentage on Compositional, Morphological and structural properties of Bi2(Te1-xSex)3 thin films
...Show More Authors

  Alloys of Bi2[Te1-x Sex]3 were prepared by melting technique with different values of  Se percentage (x=0,0.1,0.3,0.5,0.7,0.9  and 1). Thin films of these alloys were prepared by using thermal evaporation technique under vacuum of 10-5 Torr on glass substrates, deposited at room temperature with a deposition rate (12nm/min) and a constant thickness (450±30 nm). The concentrations of the initial elements Bi, Te and Se in the Bi2 [Te1-x Sex]3 alloys with different values of Se percentage (x), were determined by XRF,The morphological and structural properties were determined by AFM and XRD techniques.  AFM images of Bi2[Te1-x Sex]3 thin films  show that the average diameter and the average surface roughness inc

... Show More
View Publication Preview PDF
Crossref