The thin films of cadmium oxide (CdO) were deposited using the SILAR (Successive ionic layer absorption and reaction) method at various deposition cycles. CdO thin films were made on glass substrates at a temperature of 95°C, using a cadmium acetate source material and an ammonium hydroxide solution. One of the main criteria that impact the quality of thin films is the number of deposition cycles. The size of the crystals decreases with the increase in the number of cycles from 33.7 nm at the immersion cycle 10 to 22.7 nm at the immersion cycle 20, as shown by the X-ray diffraction results. The optical band gap energy of the films reduces as the number of deposition cycles increases, while the transmittance of the Cadmium oxide film increases as the dipping cycle increases. FTIR analytics of the sample showed that the transmittance increases with the immersion cycles. The thickness of the sample measured by the Michelson method increases with the increase in sedimentation.
The toxic lead additives to gasoline are no longer used in many countries around the world. Many other countries are now phasing out the lead in gasoline. Although the lead fuel is still in use in Iraq, several plans are considered to phase out the lead. The use of organic compounds to replace the lead additives in gasoline is considered now as an option in Iraqi refineries. The main objective of this project was preparation of premium gasoline, by blending of gasoline with Alternative additives (alcohol, aromatic) to enhancing octane number of Al-Doura gasoline pool. Improved gasoline was tested by ASTM standard method which includes octane number measuring by CFR engine analyzer. Gasoline pool RON (80) was used and selective components
... Show MoreABSTRACTObjective: The objective of this study is to develop a controlled release matrix tablet of candesartan cilexetil to reduce the frequency of administration,enhance bioavailability and improve patient compliance; a once daily sustained release formulation of candesartan cilexetil is desirable.Methods: The prepared tablets from F1 to F24 were evaluated with different evaluation parameters like weight variation, drug content, friability,hardness, thickness and swelling ability. In vitro release for all formulas were studied depends on the type and amount of each polymer, i.e. (16 mg,32 mg and 48 mg) respectively beside to the combination effect of polymers on the release of the drug from the tablet.Results: In vitro release show
... Show MoreZinc Oxide (ZnO) thin films of different thickness were prepared
on ultrasonically cleaned corning glass substrate, by pulsed laser
deposition technique (PLD) at room temperature. Since most
application of ZnO thin film are certainly related to its optical
properties, so the optical properties of ZnO thin film in the
wavelength range (300-1100) nm were studied, it was observed that
all ZnO films have high transmittance (˃ 80 %) in the wavelength
region (400-1100) nm and it increase as the film thickness increase,
using the optical transmittance to calculate optical energy gap (Eg
opt)
show that (Eg
opt) of a direct allowed transition and its value nearly
constant (~ 3.2 eV) for all film thickness (150
In this work, lead oxide (PbO) thin films were deposited using D.C. sputtering method on a surface of glass substrates and then thermally annealed at a temperature of 473K with annealing times of (1,2 and 3) hours. The structural, morphological, and optical properties of films were determined using X-ray diffraction (XRD), atomic force microscopy (AFM), FT-IR, and UV-Visible spectroscopy. The structure studies confirmed that PbO films are polycrystalline structures in an orthorhombic phase with average grain size (24.51, 29.64, 46.49, 16) nm with increasing annealing time. From AFM, the roughness of the film surface (3.26, 1.76, 1.61, 1.79) nm as the film annealing time increases. The optical band gap values of the PbO thin fi
... Show MoreIn this paper, Zinc oxide were deposited on a glass substrate at room temperature (RT) and two annealing temperatures 350ºC and 500ºC using laser induced plasma technique. ZnO nanofilms of 200nm thickness have been deposited on glass substrate. X-RAY diffraction (XRD), atomic force microscopy and UV-visible spectrophotometer were used to analyze the results. XRD forms of ZnO nanostructure display hexagonal structure with three recognized peaks (100), (002), and (101) orientations at 500ºC annealing temperature. The optical properties of ZnO nanostructure were determined spectra. The energy gap was 3.1 eV at 300 oC and 3.25eV at 500ºC annealing temperature.
Tin Selenide (SnSe) Nano crystalline thin films of thickness 400±20 nm were deposited on glass substrate by thermal evaporation technique at R.T under a vacuum of ∼ 2 × 10− 5 mbar to study the effect of annealing temperatures (as-deposited, 100, 150 and 200) °C on its structural, surface morphology and optical properties. The films structure was characterized using X-ray diffraction (XRD) which showed that all the films have polycrystalline in nature and orthorhombic structure, with the preferred orientation along the (111) plane. These films was synthesized of very fine crystallites size of (14.8-24.5) nm, the effect of annealing temperatures on the cell parameters, crystallite size and dislocation density were observed.
... Show MoreThe importance of this research is due to its importance goals, Which are about the attempt of researchers to investigate the probability of depending on businesses, environments to transform organizations, performance in away that enhance the leading role of organizations in their environments , and through views of a number of the staff working in the foundation of technical institutes in Mosul. .
After deciding the methodology of the study that ,in one hand ,performs the goals of the study , and achieving a suitable theoretical framework to present the concepts of businesses, environments and the leadin
... Show MoreHybrid architecture of ZnO nanorods/graphene oxide ZnO-NRs@GO synthesized by electrostatic self-assembly methods. The morphological, optical and luminescence characteristics of ZnO-NRs@GO and ZnO-NRs thin films have been described by FESEM, TEM, HRTEM, and AFM, which refers to graphene oxide have been coated ZnO-NRs with five layers. Here we synthesis ZnO-NRs@GO by simple, cheap and environmentally friendly method, which made it favorable for huge -scale preparation in many applications such as photocatalyst. ZnO-NRs@GO was applied as a photocatalyst Rodamin 6 G (R6G) dye from water using 532 nm diode laser-induced photocatalytic process. Overall degradation of R6G/ ZnO-NRs@GO was achieved after 90 minutes of laser irradiation while it ne
... Show More