Preferred Language
Articles
/
jih-1946
Thickness Influence on Structural and Optical Properties of ZnO Thin Films Prepared by Thermal Evaporation

  A thermal evaporation technique was used to prepare ZnO thin films. The samples were prepared with good quality onto a glass substrate and using Zn metal. The thickness varied from (100 to 300) ±10 nm. The structure and optical properties of the ZnO thin films were studied. The results of XRD spectra confirm that the thin films grown by this technique have hexagonal wurtzite, and also aproved that ZnO films have a polycrystalline structure. UV-Vis measurement, optical transmittance spectra, showed high transmission about 90% within visible and infrared range. The energy gap is found to be between 3.26 and 3.14e.V for 100 to 300 nm thickness respectivly. Atomic Force Microscope AFM (topographic image ) shows the grain size increased in the range (91.29 -110.11)nm.

 

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Wed Mar 30 2022
Journal Name
Iraqi Journal Of Science
Effect of Fe-Doping on the Properties of CdO Thin Films Prepared by Pulsed Laser Deposition

     Pure and iron-doped cadmium oxide ((CdO)1-xFex) thin films at different ratios were prepared using  pulsed laser deposition technique. The X-ray diffraction showed a polycrystalline structure for all samples associated with cubic CdO structure. Another phase appeared at the highest ratio corresponding to the cubic Fe phase. Crystallinity was enhanced and crystalline size increased with increasing Fe ratio. AFM measurements showed that increase of  Fe ratio led to an increase in the average particle diameter. In addition, the distribution of particle size became wide and of irregular behaviour, as well as increasing of the average roughness and the root-mean-square roughness. Increasing the Fe ratio caused

... Show More
Scopus Crossref
View Publication Preview PDF
Publication Date
Sun Feb 26 2012
Journal Name
Ibn Al-haitham Journal For Pure And Applied Science
Study the Effect of Annealing Temperature on the Structural, Optical and Electrical Properties of ZnS Thin Films

The structural, optical and electrical properties of ZnS films prepared by vacuum evaporation technique on glass substrate at room temperature and treated at different annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction studies show that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (111). The optical properties investigated which include the absorbance and transmittance spectra, energy band gab, absorption coefficient, and other optical constants. The results showed that films have direct optical transition. The optical band gab was found to be in the range t

... Show More
Publication Date
Fri Nov 29 2019
Journal Name
Iraqi Journal Of Physics
ZnO Characterization of ZnO/GaAs heterojunction: ZnO thin films

ZnO thin films have been prepared by pulse laser deposition technique at room temperatures (RT). These films were deposited on GaAs substrate to form the ZnO/GaAs heterojunction solar cell. The effect of annealing temperatures at ( RT,100, 200)K on structural and optical properties of ZnO thin films has been investigated. The X-ray diffraction analysis indicated that all films have hexagonal polycrystalline structure. AFM shows that the grains uniformly distributed with homogeneous structure. The optical absorption spectra showed that all films have direct energy gap. The band gap energy of these films decreased with increasing annealing temperatures.  From the electrical properties, the carriers have n-type conductivity.  From

... Show More
Crossref
View Publication Preview PDF
Publication Date
Mon Jun 01 2020
Journal Name
Iraqi Journal Of Physics
Optical and structural properties of synthesized ZnO nanorods through chemical bath deposition on various substrates

Chemical bath deposition was used to synthesize ZnO nanorods (NRs) on glass and fluorine_doped tin oxide (FTO) substrates. X-ray diffraction was performed to examine the crystallinity of ZnO nanorod. Results showed that ZnO NRs had a wurtzite crystal structure. Field emission scanning electron microscopy images showed that glass sample had rod-like structure distribution with (50 nm) diameter and average length of approximately (700 nm), whereas the FTO-coated glass sample had 25 nm diameter and average length of approximately 950 nm. The direct optical transition band gaps of the glass and FTO_coated glass samples were( 4 and 4.43 eV), respectively. The structural and optical properties of the synthesized ZnO p

... Show More
Crossref
View Publication Preview PDF
Publication Date
Wed May 10 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Annealing Effect on the Optical Properties of (ZnO)x (CdO)1-x Films Obtained by Spray Pyrolysis

The effect of the annealing on the optical transmission , absorp tion coefficient,
dielectric constants (ε
r
),( ε
i
) ,Skin depth and the optical ener gy gap of (ZnO)x(CdO)1-x thin
films with (x=0.05) deposited on preheated glass substrates at a temperature of (450 C°) by
chemical pyrolysis technique were performed . These f ilms show direct allowed inter band
transition that influenced by annealing at ( 450 C°) for two hours . And it also found that the
optical ener gy gap has been increased fro m about (2.50 eV) before annealing to about (2.65
eV) after annealing , fro m the analysis of the absorp tion and transmission sp ectra in the
wavelength range (380-900nm) . The results show t

... Show More
View Publication Preview PDF
Publication Date
Sun Oct 27 2019
Journal Name
Iraqi Journal Of Science
Studying the Effect of Annealing on Optical and Structure Properties of Zno Nanostructure Prepared by Laser Induced Plasma

In this paper, Zinc oxide were deposited on a glass substrate at room temperature (RT) and two annealing temperatures 350ºC and 500ºC using laser induced plasma technique. ZnO nanofilms of 200nm thickness have been deposited on glass substrate. X-RAY diffraction (XRD), atomic force microscopy and UV-visible spectrophotometer were used to analyze the results. XRD forms of ZnO nanostructure display hexagonal structure with three recognized peaks (100), (002), and (101) orientations at 500ºC annealing temperature. The optical properties of ZnO nanostructure were determined spectra. The energy gap was 3.1 eV at 300 oC and 3.25eV at 500ºC annealing temperature.

Scopus (24)
Crossref (16)
Scopus Crossref
View Publication Preview PDF
Publication Date
Sun Mar 01 2009
Journal Name
Baghdad Science Journal
The structure and optical properties of CdSe:Cu Thin Films

A polycrystalline CdSe thin films doped with (5wt%) of Cu was fabricated using vacuum evaporation technique in the substrate temperature range(Ts=RT-250)oC on glass substrates of the thickness(0.8?m). The structure of these films are determined by X-ray diffraction (XRD). The X-ray diffraction studies shows that the structure is polycrystalline with hexagonal structure, and there are strong peaks at the direction (200) at (Ts=RT-150) oC, while at higher substrate temperature(Ts=150-250) oC the structure is single crystal. The optical properties as a function of Ts were studied. The absorption, transmission, and reflection has been studied, The optical energy gap (Eg)increases with increase of substrate temperature from (1.65

... Show More
Crossref
View Publication Preview PDF
Publication Date
Tue Jun 01 2021
Journal Name
Iraqi Journal Of Physics
Effect of Transition Metal Dopant on the Electrical Properties of ZnO-TiO2 Films Prepared by PLD Technique

In this article, the influence of group nano transition metal oxides such as {(MnO2), (Fe2O3) and (CuO)} thin films on the (ZnO-TiO2) electric characteristics have been analyzed. The prepared films deposited on glass substrate laser Nd-YAG with wavelength (ℷ =1064 nm) ,energy of (800mJ) and number of shots (400). The density of the film was found to be (200 nm) at room temperature (RT) and annealing temperature (573K).Using DC Conductivity and Hall Effect, we obtained the electrical properties of the films. The DC Conductivity shows that that the activation energies decrease while the σRT at annealing temperature with different elements increases the formation of mixed oxides. The Hall effect, the elec

... Show More
Crossref
View Publication Preview PDF
Publication Date
Sat Dec 20 2014
Journal Name
International Journal Of Current Engineering And Technology
The Effect of Sb Dopant and Annealing Temperature on the Structural and Optical Properties of GeSe Thin Films

The pure and Sb doped GeSe thin films have been prepared by thermal flash evaporation technique. Both the structural and optical measurement were carried out for as deposited and annealed films at different annealing temperatures.XRD spectra revealed that the all films have one significant broad amorphous peak except for pure GeSe thin film which annealed at 573 K, it has sharp peak belong to orthorhombic structure nearly at 2θ=33o . The results of the optical studies showed that the optical transition is direct and indirect allowed. The energy gap in general increased with increasing annealing temperature and decreased with increase the ratio of Sb dopant. The optical parameters such as refractive index, extinction coefficient and r

... Show More
Publication Date
Wed May 10 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
The Study of Annealing and Dopping Effect of Zn on Structural and Optical Properties for CdTe Thin Films

In this research thin films of (CdTe) have been prepared as pure and doped by Zn
with different ratios (1,2,3,4,5)% at thickness (400+25)nm with deposition rate (2±0.1)nm,
deposited on glass substrate at R.T. by using thermal evaporation in vacuum . All samples
were annealed at temperature (523,573,623,673)K at 1h.
The structural prop erties of all prepared thin films, doped and undoped have been
studied by using XRD. The analysis reveals that the structures of the films were
polycrystalline and typed cubic with a preferred orientation along (111) plane for the
undoped films with (2,3)% of zinc , and shifting (2ÆŸ) for doped films . The annealing films
at temperature 573 K and Zn:3% show decreasing in

... Show More
View Publication Preview PDF