A reseach is carried out by using Alumina material type α-Al2O3 which has partical size 63μm doped with different percentage weight of MgO (0.1%,0.3%and0.5%) and by using dry press method to prepare the samples ,A force press 50KN used and sintering to 1500oC with soaking time of 6 hours. The physical properties were studied such as "Bulk density ,Porosity and water absorption "also the mechanical properties such as (hardness,compressive strength ), the result shows that the best ratio of maginsa(MgO) added to Alumina (Al2O3)is 0.5%and this worked to improve Physical and mechanical properties .
Two simple methods for the determination of eugenol were developed. The first depends on the oxidative coupling of eugenol with p-amino-N,N-dimethylaniline (PADA) in the presence of K3[Fe(CN)6]. A linear regression calibration plot for eugenol was constructed at 600 nm, within a concentration range of 0.25-2.50 μg.mL–1 and a correlation coefficient (r) value of 0.9988. The limits of detection (LOD) and quantitation (LOQ) were 0.086 and 0.284 μg.mL–1, respectively. The second method is based on the dispersive liquid-liquid microextraction of the derivatized oxidative coupling product of eugenol with PADA. Under the optimized extraction procedure, the extracted colored product was determined spectrophotometrically at 618 nm. A l
... Show More