Wires are commonly used for the construction of orthodontic appliances and occasionally as wrought clasps and rests on partial dentures. The corrosion resistance is the most important properties of dental alloy. Corrosion process reported to cause a numerous adverse effects on both living tissue and restoration .The conditions in the mouth are very suitable for the occurrence of corrosion. The main objective of this study was to evaluate the corrosion behavior of different gauges of stainless steel wire in artificial saliva .Four gauges of dental stainless steel wire used in orthodontic and removable partial denture were used in this study 0.6mm.,0.7mm.,0 .8mm.&1.0mm.).The specimens were divided according to gauge in to four groups(A,B,C,&D ) ,ten specimens in each group .Each wire was cut by using wire cutter to get wire with (1cm) in length .Artificial saliva of Fusayama Meyer type was used as the testing solution .Sensitive electronic balance was used to weight the sample before immersion in solution and recording the results.This this represents the first weight(W1).Each specimen was put inside a test tube , and held using dental floss in a way that the specimen was fully immersed in the solution from all sides . The specimens then were put inside an incubator ,which was adjusted at 37±2 and left for 14 days .At the end of immersion period ; the specimens were removed from the solution and then allowed to dry and were balanced then the results were recorded .This represents the second weight (W2) .After obtaining the (W1)&(W2) the corrosion rate was calculated . The results before and after immersion showed that the 0.6 mm.& 0.7mm stainless steel wire gave the highest and more corrosion resistance value than 0.8mm&1.0mm.stainless steel wire . The result showed there is a statistical significance between (W1&W2) of 0.8mm stainless steel wire and highly significant between (W1&W2) of 1.0mm. stainless steel wire . The comparison of the results after calculating results in corrosion rate formula showed that the 1.0mm stainless steel wire more corrosion resistance followed by 0.8mm wire ,from 0.6mm& 0.7 mm wire .
Objective(s): The aim of this study is to compare the impact strength of a heat cured denture-base acrylic resin
reinforced with metal wire and glass fibers.
Methodology: Forty five specimens were prepared from pink heat cure acrylic resin. Specimens were grouped into;
group-I (control group) which consists of 15 specimens with no reinforcement, group-II which consists of 15 specimens
reinforced with metal wire, and group-III consists of 15 specimens reinforced with glass fibers. Specimens were tested
by using charpy impact machine.
Results: The result showed that there was a highly significant difference in impact strength value among the testing
groups at (P < 0.001).
Conclusion: The impact str
... Show MoreThe corrosion inhibition of low carbon steel in1N HCl solution in the presence of peach juice at temperature (30,40,50,and 60)°C at concentration ( 5, 10, 20, 30, 40and 50 cm3/L)were studied using weight loss and polarization techniques. Results show that the inhibition efficiency was increased with the increase of inhibitor concentration and increased with the increase of temperature up to 50ºC ,above 50ºC (i.e. at 60 ºC) the values of efficiency decreases. Activation parameters of the corrosion process such as activation energies, Ea, activation enthalpies, ΔH, and activation entropies, ΔS, were calculated. The adsorption of inhibitor follows Langmuir isotherm. Maximum inhibition efficiency obtained was a bout 91% at 50ºC in the
... Show MoreCorrosion of steel reinforcement is one of the biggest problems facing all countries in the world like bridges in the beach area and marine constructions which lead to study these problems and apply some economical solutions. According to the high cost of repair for these constructions, were studied the effect of using kind of chemical compounds sodium nitrite(NaNO2) and sodium silicate(Na2SiO3) as corrosion inhibitors admixture for steel bars that immersed partially in electrolyte solution (water + sodium chloride in 3% conc.) (Approximately similar to the concentration of salt in sea water). The two inhibitors above added each one to the electrolyte solution at concentrations (0.5%, 1% and 2%) for both
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreThe present investigation aims to study the effect of heat treatment by quenching in different quenching media (salt water, water and oil) following by tempering on wear resistance of EN25 steel. EN25 steel is an alloy of medium carbon low alloy steel which is used for many applications requiring high tensile strength and wear resistance such as connecting rods, adapters and in power sectors extensively. The specimens are machined to 20 mm in length and 10 mm in diameter. This study is done by two stages: The first stage is done by austenitizing EN25 steel to 850 for 1 hr by quenching the specimens in three different quenching media and then tempered at 300 in air. While the second stage is performed by wear
... Show MoreThis research involves study effect of chloride ions in concentration range (0.01 – 0.50 mol.dm-3) on the corrosion behavior of Al-Zn alloy in basic media of 1x10-3 mol.dm-3 NaOH at pH=11 and four different temperatures in the range (298-313 K). Cathodic and anodic Tafel slopes (bc &ba) and transfer coefficients (αc & αa) were calculated and the results interprets according to the variation of the rate – determining steps. The results also indicate that the chloride ions are bonded chemically in the interface as an initial step of formation of different mixed oxohydroxy – and chloro complexes. Polarization resistance (Rp) is calculates
... Show MoreThis study investigates the implementation of Taguchi design in the estimation of minimum corrosion rate of mild-steel in cooling tower that uses saline solution of different concentration. The experiments were set on the basis of Taguchi’s L16 orthogonal array. The runs were carried out under different condition such as inlet concentration of saline solution, temperature, and flowrate. The Signal-to- Noise ratio and ANOVA analysis were used to define the impact of cooling tower working conditions on the corrosion rate. A regression had been modelled and optimized to identify the optimum level for the working parameters that had been founded to be 13%NaCl, 35ᴼC, and 1 l/min. Also a confirmation run to establish the p
... Show MoreIn present work an investigation for precise hole drilling via continuous wave (CW) CO2 laser at 150 W maximum output power and wavelength 10.6 μm was achieved with the assistance of computerized numerical controlled (CNC) machine and assist gases. The drilling process was done for thin sheets (0.1 – 0.3 mm) of two types of metals; stainless steel (sst) 321H, steel 33 (st). Changing light and process parameters such as laser power, exposure time and gas pressure was important for getting the optimum results. The obtained results were supported with computational results using the COMSOL 3.5a software code.
Corrosion experiments were carried out to investigate the effect of several operating parameters on the corrosion rate and corrosion potential of carbon steel in turbulent flow conditions in the absence and presence of sodium benzoate inhibitor using electrochemical polarization technique. These parameters were rotational velocity (0 - 1.57 m/s), temperature (30oC – 50oC), and time. The effect of these parameters on the corrosion rate and inhibition efficiency were investigated and discussed. It was found that the corrosion rate represented by limiting current increases considerably with increasing velocity and temperature and that it decreased with time due to the formation of corrosion product layer. The corrosion potential shifted t
... Show More