Wires are commonly used for the construction of orthodontic appliances and occasionally as wrought clasps and rests on partial dentures. The corrosion resistance is the most important properties of dental alloy. Corrosion process reported to cause a numerous adverse effects on both living tissue and restoration .The conditions in the mouth are very suitable for the occurrence of corrosion. The main objective of this study was to evaluate the corrosion behavior of different gauges of stainless steel wire in artificial saliva .Four gauges of dental stainless steel wire used in orthodontic and removable partial denture were used in this study 0.6mm.,0.7mm.,0 .8mm.&1.0mm.).The specimens were divided according to gauge in to four groups(A,B,C,&D ) ,ten specimens in each group .Each wire was cut by using wire cutter to get wire with (1cm) in length .Artificial saliva of Fusayama Meyer type was used as the testing solution .Sensitive electronic balance was used to weight the sample before immersion in solution and recording the results.This this represents the first weight(W1).Each specimen was put inside a test tube , and held using dental floss in a way that the specimen was fully immersed in the solution from all sides . The specimens then were put inside an incubator ,which was adjusted at 37±2 and left for 14 days .At the end of immersion period ; the specimens were removed from the solution and then allowed to dry and were balanced then the results were recorded .This represents the second weight (W2) .After obtaining the (W1)&(W2) the corrosion rate was calculated . The results before and after immersion showed that the 0.6 mm.& 0.7mm stainless steel wire gave the highest and more corrosion resistance value than 0.8mm&1.0mm.stainless steel wire . The result showed there is a statistical significance between (W1&W2) of 0.8mm stainless steel wire and highly significant between (W1&W2) of 1.0mm. stainless steel wire . The comparison of the results after calculating results in corrosion rate formula showed that the 1.0mm stainless steel wire more corrosion resistance followed by 0.8mm wire ,from 0.6mm& 0.7 mm wire .
Background: The final stage of endodontic therapy is complete obturation of the root canal system to provide as perfect as possible at the cementodentinal junction of the apical foramen. The purpose of this in vitro study was to evaluate the sealing ability of injection molded thermoplasticized gutta percha and lateral condensation techniques with and without the use of sealers. Materials and Methods: Forty freshly extracted adult human maxillary central incisors with complete formed apices were utilized in this study. The teeth were randomly divided into four groups for evaluation of the apical seal. Group (1) lateral condensation gutta percha technique without sealer, (2) lateral condensation gutta percha technique with sealer, (3) Inject
... Show MoreIntroduction: We aimed to assess the impact of adhesive and wires types on the tensile bond strength of fixed lingual retainers. Methods: A total of 160 intact bovine teeth were collected, cleaned, stored in 25% sodium hypochlorite, and randomly assigned to two groups based on the adhesive type: a two-step adhesive and a one-step adhesive. Each group was further divided into four subgroups based on the type of lingual retainer wire, which included (A) 8-strand braided stainless steel wire, (B) three-strand titanium retainer wire, (C) stainless steel chain, and (D) fiber-reinforced retainer. A tensile bond strength test was conducted using a universal testing machine at a controlled speed of 10 mm/min. Result: The 8-strand braided stainles
... Show MoreBackground: The most widely used material for fabrication of denture base is poly methyl methacrylate, despite its popularity, the main problems associated with it as a denture base material are poor strength particularly under fatigue failure inside the patient mouth, impact failure outside the patient mouth, which are the main causes for fracture of denture, several studies was done to increase mechanical properties of denture base. The present study was conducted to evaluate and compare the effect of addition single walled carbon nanotubes in different concentrations to polymethyl methacrylate on some mechanical properties (surface hardness, surface roughness, impact strength and transverse strength). Materials and methods: Forty eight
... Show MoreObjective: To evaluate and compare the effect of mechanical surface treatment (groove, aluminum oxide particles)
with 45 degree bevel type of joint on tensile bond strength of acrylic specimens repaired by two curing methods
(microwave and water both).
Methodology: Eighty specimens (80) were prepared from pink heat cure acrylic resin. They were divided into two
main groups (40 specimen repaired by microwave energy and 40 specimens repaired by water bath method).Each
group can be divided into four subgroups of ten according to the surface treatment. The control group A was left
intact, group B received no surface treatment, group C and D received surface treatment by (groove, 50 m aluminum
oxide particles). Specimens
Background: Acrylic resin polymer s used in prosthodontic treatment as a denture base material for several decades. Separation and debonding of artificial teeth from denture bases present a laboratory and clinical problem affect patient and dentist. The aim of this study is to evaluate the effect of oxygen plasma and argon plasma treatment of acrylic teeth and thermocycling on bonding strength to hot cured acrylic resin denture base material. Materials and Methods: Sixty denture teeth (right maxillary central incisor) are selected. The denture teeth are waxed onto the beveled surface of rectangular wax block according to Japanese standard for artificial teeth. The control group consisted of 20 denture teeth specimen without any treatment.
... Show MoreBraces in straight bridge systems improve the lateral-torsional buckling resistance of the girders by reducing the unbraced length, while in horizontally curved and skew bridges, the braces are primary structural elements for controlling deformations by engaging adjacent girders to act as a system to resist the potentially large forces and torques caused by the curved or skewed geometry of the bridge. The cross-frames are usually designed as torsional braces, which increase the overall strength and stiffness of the individual girders by creating a girder system that translates and rotates as a unit along the bracing lines. However, when they transmit the truck’s live load forces, they can produce fatigue cracks at their connection
... Show MoreAim: This study aimed to assessing orthodontic knowledge and attitude among general dentists and non-orthodontic specialists. Background: Early detection of orthodontic disorders is essentialin motivating patients to intervene prior to long term complications when the disorders are not recongised. Methods: A questionnaire was distributed amongst dentistsother than orthodontists. This questionnaire consisted of three sections. The first one aimed to collect demographic, educational level and practice type information. Further two sections consisted of closed-end questions designed to evaluateknowledge and attitude of orthodontics. Results: A total of 313 responses to the survey were submitted. No significant correlation was observed, e
... Show MoreBackground: The microorganisms can impend the life of health care professional and particularly the dental practitioners. They can be transmitted by different ways like airborne and droplet transmission. The current study was carried out to identify whether the arch wires that received from the manufactures are free from microbial contamination and to determine the bacterial species attached to the arch wires. Materials and Methods: This study involved eighty samples, consisted of two types of arch wires (nitinol and stainless-steel) from four companies (3M, G&H, Jiscop, OrthoTechnology). These wires inserted in a plane tube that contains 10 -ml of (Tris [tris(hydroxymethyl)aminomethane] and EDTA (ethylenediaminetetraacetic acid) tri