This research studies the possibility of producing Bone China with available local and geological substitutes and other manufactured ones since it’s traditionally produced by Bone ash, Cornish stone, and China clay, while the substitutes are Kaolin instead of China clay and Feldspar potash instead of Cornish stone. Because of the unavailability of Feldspar in Iraq, it was substituted with the manufactured alternative Feldspar. Bone ash was prepared from cow bones with heating treatments, grinding and sifting. The alternative Feldspar was prepared by chemical analysis of the natural Feldspar potash with local materials that include Dwaikhla Kaolin, Urdhuma Silica sand, Potassium Carbonate, and Sodium Carbonate. The mixture was burned at (1250c○) before it was grinded. The mixture’s materials were sifted at (63µm). The samples were formed with slip casting by gypsum mold with a cut cone shape at (2×3×6 cm) to build a thickness of (3mm). The study materials consisted of two groups: Group 1 (BC.K.F) including Bone ash, Dwaikhla Kaolin, and the natural Feldspar, while Group 2 (BC.K.FR) had Bone ash, Dwaikhla Kaolin, and the manufactured alternative Feldspar. Every group included 8 recipes with the same percentages. The two groups were burned at (1220-1260c○), then tests were conducted: Chemical analyses, the outer appearance and color then the laboratory tests: the outer appearance, linear shrinkage, apparent porosity, water absorption, bulk density, hardness, scratching resistance, mineral analysis (XRD), color analyses, optical transmittance. After discussing and analyzing the results, it was concluded that the traditional materials substitutes gave matching and correspondent properties and specification of Bone China ceramic
The change in project cost, or cost growth, occurs from many factors, some of which are related to soil problem conditions that may occurs during construction and/or during site investigation period. This paper described a new soil improvement method with a minimum cost solution by using polymer fiber materials having a length of (3 cm) in both directions and (2.5 mm) in thickness, distributed in uniform medium dense .
sandy soil at different depths (B, 1.5B and 2B) below the footings. Three square footings has been used (5,7.5 and 10 cm) to carry the above investigation by using lever arm loading system design for such purposes.
These fibers were distributed from depth of (0.1B) below the footing base down to the investigated dep
Prostheses are used as an alternative to organs lost from the body. Flex-Foot Cheetah is considered one of the lower limb prostheses used in high-intensity activities such as running. This research focused on testing two samples of Flex-Foot Cheetah manufactured of two various materials (carbon, glass) with polyester and compare between them to find the foot with the best performance in running on the level of professional athlete. In the numerical analysis, the maximum principal stress, maximum principal elastic strain, strain energy; finally, the blade total deformation were calculated for both feet. In experimental work, the load-deflection test was done for foot to calculate the bending the results were very close to
... Show MorePorous materials play an important role in creating a sustainable environment by improving wastewater treatment's efficacy. Porous materials, including adsorbents or ion exchangers, catalysts, metal–organic frameworks, composites, carbon materials, and membranes, have widespread applications in treating wastewater and air pollution. This review examines recent developments in porous materials, focusing on their effectiveness for different wastewater pollutants. Specifically, they can treat a wide range of water contaminants, and many remove over 95% of targeted contaminants. Recent advancements include a wider range of adsorption options, heterogeneous catalysis, a new UV/H2O
This research studies the effect of addition of some nanoparticles
(MgO, CuO) and grain size (30,40nm) on some physical properties
(impact strength, hardness and thermal conductivity) for a matrix
blend of epoxy resin with SBR rubber. Hand –Lay up method was
used to prepare the samples. All samples were immersed in water for
9 weeks.
The Results showed decreased in the values of impact strength and
hardness but increased the coefficient of thermal conductivity.
Background: The microhardness of a composite resin is a vital parameter that is used to determine its clinical behavior. Measuring the microhardness of a composite resin has been used as an indirect method to assess its degree of conversion and extent of polymerization. The purpose of this in vitro study was to evaluate the effect of three curing distances (0, 2, and 4 mm) on the microhardness of the top and bottom surfaces of three types of flowable bulk-fill composite resins (smart dentin replacement, Opus bulk fill flow, and Tetric N). Material and method: Sixty-three specimens from the three types of composite resins (n=21) were fabricated using Teflon mold with a 4mm depth and a 5 mm internal diameter and cured for 20 seconds. For e
... Show MoreBackground: The aim of this study was to evaluate the effect of three types of light curing devices QTH, LED and Flashmax on the surface microhardness of three types of bulkfill composite resins; Filtek Bulkfill posterior composite ( 3M), Tetric Evo Ceram ( Ivoclar Vivadent) and Sonicfill composite ( Kerr) Materials and methods: Total number of 90 samples was prepared, 30 samples for each type of bulkfill composite, were divided into three main groups, group A: Filtek posterior bulkfil (3M), group B: Tetric Evo Ceram (Ivoclar Vivadent) and group C: contain Sonicfill composite (kerr). Which then divided into three subgroups (n= 10) (1) Samples cured by QTH system (2) Samples cured by LED system and (3) samples cured by Flashmax system the
... Show MoreThe tunnel’s stability during construction is a very important matter. Some methods have been proposed for stability evaluation, but the hazard warning levels (HWLs) are more applicable among these methods. Despite monitoring and applying HWLs, several collapses in Shibli twin tunnels in Iran have cast doubts on the accuracy of this criterion in the presence of water. In this study, the critical strains under different water contents were measured through uniaxial compressive strength tests on 11 different shale and marl samples. A comparison of laboratory tests and numerical results shows that the influence of the moisture content on the critical strain is negligible. In addition, the results show that there is no dir
... Show MoreObjective: To evaluate the effect of mouth rinses (Biofresh and ZAK) on the surface micro hardness
of two light cure restorative material (Tetric ceram ivoclar-vivadent) and (3M Z 250) dental
composite.
Methodology: The microhardness values of (sixty) composite specimens were measured at the top
surfaces after 24 hours of immersion in different solutions (Biofresh, Zak mouth wash and distilled
water as control). Comparison done using descriptive statistics (mean, SD, SEM, minimum and
maximum values) and inferential statistics (ANOVA and LSD) test.
Results: The biofresh mouth rinse which has high alcohol containing has less effect on
microhardness of tetric ceram than the zak &distiled water , while the effect
Steel fiber aluminum matrix composites were prepared by atomization technique. Different air atomization conditions were considered; which were atomization pressure and distance between sample and nozzle. Tensile stress properties were studied. XRF and XRD techniques were used to study the primary compositions and the structure of the raw materials and the atomized products. The tensile results showed that the best reported tensile strength observed for an atomization pressure equal to 4 mbar and sample to nozzle distance equal to 12 cm. Young modulus results showed that the best result occurred with an air atomization pressure equal to 8 mbar and sample to nozzle distance equal to 16cm