The Effect of Zirconium Silicate Nanopowder Reinforcement on Some Mechanical and Physical Properties of Heat Cured Poly (Methyl Methacrylate) Denture Base Materials
...Show More Authors

Background: Polymethylmethacrylate (PMMA) has relatively unsatisfactory mechanical properties such as low flexural strength and impact strength also dimensional instability. Material and method: Zirconium silicate nanoparticles were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 1% and 1.5% by weight then mixed with powder using conventional procedure, (150) samples were prepared and divided into three groups, each group consisted of (50) samples, the first group prepared from PMMA without addition (control), another group with the addition of 1% wt Zrsio4 nanoparticles (experimental) and the third one with 1.5% wt Zrsio4 nanoparticles (experimental). Each group was divided into 5 sub-groups according to the test performed. The tests conducted impact strength, transverse strength, indentation hardness (shore D), surface roughness, water sorption and solubility. The size, shape and distribution of nanofiller were estimated using scanning electron microscope (SEM) .The results were statistically analyzed using ANOVA and LSD test. Result: Highly significant increase in impact strength, transverse strength and surface hardness occurred with the incorporation of 1.5% wt Zirconium silicate nanofiller but non-significant increase in impact strength, significant increase in transverse strength and highly significant increase in surface hardness occurred with the incorporation of 1% wt Zrsio4 nanofiller. Non-significant increase in surface roughness with both 1% and 1.5% wt Zrsio4 . Highly significant decrease in water sorption and solubility with 1.5% wt Zrsio4 nanofiller and non-significant decrease in water sorption and solubility with 1% wt Zrsio4 compared with control group. Conclusion: The maximum increase in impact strength, transverse strength, and surface hardness was observed in denture base nano composite containing 1.5% Zrsio4. In addition, highly significant decrease in water sorption and solubility and non-significant increase in surface roughness was also noticed.

View Publication Preview PDF
Quick Preview PDF
Publication Date
Fri Jun 01 2018
Journal Name
Journal Of The College Of Languages (jcl)
Отражение женского пола в качестве женщины в русских фразеологических единицах на фоне арабского языка Reflection of Feminine Gender as represented by Women in Russian Idioms in Comparison with Arabic
...Show More Authors

Аннотация

Взгляд на пол как на комплексное социальное отношение означает,что роль женщины в истории следует рассматривать не просто как новый для исторической науки предмет исследования, а как обойденный вниманием ученых вопрос об отношениях между людьми или группами людей.

Женщина играет особую и важную  роль в обществе , даже скажут ,что она половина нашего общества ,поэтому она яв

... Show More
View Publication Preview PDF
Publication Date
Thu Jan 23 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Shear bond strength of stainless steel brackets bonded to porcelain surface treated with 1.23% acidulated phosphate fluoride gel compared to hydro fluoric acid with silane coupling agent (In vitro comparative study)
...Show More Authors

Background: With the increasing demands for adult orthodontics, a growing need arises to bond attachments to porcelain surfaces. Optimal adhesion to porcelain surface should allow orthodontic treatment without bond failure but not jeopardize porcelain integrity after debonding.The present study was carried out to compare the shear bond strength of metal bracket bonded to porcelain surface prepared by two mechanical treatments and by using different etching systems (Hydrofluoric acid 9% and acidulated phosphate fluoride 1.23%). Materials and Methods: The samples were comprised of 60 models (28mm *15mm*28mm) of metal fused to porcelain (feldspathic porcelain). They were divided as the following: group I (control): the porcelain surface left u