Background: Ceramic veneers represent the treatment of choice in minimally invasive esthetic dentistry; one of the critical factors in their long term success is marginal adaptation. The aim of the present study is to evaluate the marginal gap of ceramic veneers by using two different fabrication techniques and two different designs of preparation. Material and methods: A typodont maxillary central incisor used in the preparation from which metal dies were fabricated, which were in turn used to make forty stone dies. The dies divided into four experimental groups, each group had ten samples: A1: prepared with butt-joint incisal reduction and restored with IPS e.max CAD, A2: prepared with overlapped incisal reduction and restored with IPS e.max CAD. B1: prepared with butt-joint incisal reduction restored with IPS e.max press. B2: prepared with overlapped incisal reduction and restored with IPS e.max press. The marginal gap was measured with direct view technique using digital microscope at a magnification of 230x. Measurements were recorded for four surfaces for each sample and the maximum value was taken to represent that sample. Results: The data were analyzed with two-way ANOVA and independent samples t-tests. These tests revealed highly significant effects of both the preparation design and the technique of fabrication on the marginal gap (p=0.00), with CAD/CAM veneers, group A1 recorded the least marginal gap and pressing group, B2 showed the highest gap values. There was no significant effect of the interaction between the two parameters on the marginal gap. Conclusion: the CAD/CAM veneers with butt joint incisal reduction produced the most accurate margins while the least favorable combination was the pressable ceramic veneers with overlapped incisal reduction.
Effects of Ozonated Water on Micro Leakage between Enamel and Fissure Sealants Prepared by Different Etching Technique (An in vitro Study), Baraa M Jabar*, Muna S Khalaf
Background: Esthetic treatment is the options of patient seeking orthodontic treatment. Therefore this study was conducted to measure the concentration of Aluminum, Nickel, Chromium and Iron ions released from combination of monocrysralline brackets with different arch wires immersed in artificial saliva at different duration, to evaluate the corrosion point on different parts of the orthodontic appliances before and after immersion in artificial saliva, and to evaluate the corrosion potential of each group of the orthodontic appliances. Material and methods: Eighty orthodontic sets prepared. Each set represents half fixed orthodontic appliance, from the central incisor to the first molar, for the maxillary arch, each set consisted of molar
... Show MoreBackground: Ideal root canal obturation depends on many factors; one of them is good sealing of root canal without pores. The aim of this study was to determine the radiographic density of GuttaFlow® 2 with different obturation techniques using spiral computed tomography. Materials and Methods: Forty palatal roots of permanent maxillary first molar were used in this study. Following working length determination, root canal was prepared using rotary PROTAPER universal system. They were randomly divided into four groups of 10 roots each, the groups are Conventional lateral condensation with Apexit Plus sealer, Conventional lateral condensation with GuttaFlow® 2 as a sealer, Soft Core Regular with GuttaFlow® 2 as a sealer and singl
... Show MoreBackground: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets
... Show MoreInfertility can be detected when the couples have not completed pregnancy after a year or more of normal coitus. So, in order to treat infertility, there are many supported reproductive techniques are in practice. The success rate of these techniques depends upon the way by which preparation of the paternal semen sample. Over the past 30 years, the manual has been standard as providing global standards and has been used extensively by research and clinical laboratories throughout the world. The spermatozoa of all placental (eutherian) mammals, including humans, are in a protective, no labile formal at ejaculation and are incapable of fertilization even if they are placed in direct contact with an oocyte. Accordingly, they must undergo a sub
... Show MoreThe applications of Multilevel Converter (MLC) are increased because of the huge demand for clean power; especially these types of converters are compatible with the renewable energy sources. In addition, these new types of converters have the capability of high voltage and high power operation. A Nine-level converter in three modes of implementation; Diode Clamped-MLC (DC-MLC), Capacitor Clamped-MLC (CC-MLC), and the Modular Structured-MLC (MS-MLC) are analyzed and simulated in this paper. Various types of Multicarrier Modulation Techniques (MMTs) (Level shifted (LS), and Phase shifted (PS)) are used for operating the proposed Nine level - MLCs. Matlab/Simulink environment is used for the simulation, extracting, and ana
... Show MoreThe goal of the research is to find the optimization in the test of the appropriate cross-over design for the experiment that the researcher is carrying out (under assumption that there are carry-over effects of the treatments) to posterior periods after the application period (which is often assumed to be the first period). The comparison between the double cross-over design and the cross-over design with extra period. The similarities and differences between the two designs were studied by measuring the Relative Efficiency (RE) of the experiment.
In this study, the effect of ceramic coating on the performance and gases emission on diesel engine was investigated. A four-stroke, direct injected, single cylinder, diesel engine was tested at constant speed and at different load conditions without coating. Then, the inlet and exhaust valves faces were coated by about 500µm with ceramic materials. Ceramic layers were made of YttriaStabilized Zirconia (YSZ), and NiCrAl as a bond coat. The coating technique adapted in this work is the flame spray method. The engine with valves ceramiccoated research was tested for the same operation conditions of the engine (without coating). The results indicate a reduction in both fuel consumption by about 7.6% and particulate emissions by about (13
... Show More