Background: Ceramic veneers represent the treatment of choice in minimally invasive esthetic dentistry; one of the critical factors in their long term success is marginal adaptation. The aim of the present study is to evaluate the marginal gap of ceramic veneers by using two different fabrication techniques and two different designs of preparation. Material and methods: A typodont maxillary central incisor used in the preparation from which metal dies were fabricated, which were in turn used to make forty stone dies. The dies divided into four experimental groups, each group had ten samples: A1: prepared with butt-joint incisal reduction and restored with IPS e.max CAD, A2: prepared with overlapped incisal reduction and restored with IPS e.max CAD. B1: prepared with butt-joint incisal reduction restored with IPS e.max press. B2: prepared with overlapped incisal reduction and restored with IPS e.max press. The marginal gap was measured with direct view technique using digital microscope at a magnification of 230x. Measurements were recorded for four surfaces for each sample and the maximum value was taken to represent that sample. Results: The data were analyzed with two-way ANOVA and independent samples t-tests. These tests revealed highly significant effects of both the preparation design and the technique of fabrication on the marginal gap (p=0.00), with CAD/CAM veneers, group A1 recorded the least marginal gap and pressing group, B2 showed the highest gap values. There was no significant effect of the interaction between the two parameters on the marginal gap. Conclusion: the CAD/CAM veneers with butt joint incisal reduction produced the most accurate margins while the least favorable combination was the pressable ceramic veneers with overlapped incisal reduction.
This work presents a completely new develop an analyzer, named NAG-5SX1-1D-SSP, that is simple, accurate, reproducible, and affordable for the determination of cefotaxime sodium (CFS) in both pure and pharmaceutical drugs. The analyzer was designed according to flow injection analysis, and conducted to turbidimetric measurements. Ammonium cerium nitrate was utilized as a precipitating agent. After optimizing the conditions, the analysis system exhibited a linear range of 0.008-27 mmol. L-1 (n=29), with a limit of detection of 439.3 ng/sample, a limit of quantification of 0.4805 mg/sample, and a correlation coefficient of 0.9988. The repeatability of the responses was assessed by performing six successive injections of CFS at concentra
... Show MoreThe reaction oisolated and characterized by elemental analysis (C,H,N) , 1H-NMR, mass spectra and Fourier transform (Ft-IR). The reaction of the (L-AZD) with: [VO(II), Cr(III), Mn(II), Co(II), Ni(II), Cu(II), Zn(II), Cd(II) and Hg(II)], has been investigated and was isolated as tri nuclear cluster and characterized by: Ft-IR, U. v- Visible, electrical conductivity, magnetic susceptibilities at 25 Co, atomic absorption and molar ratio. Spectroscopic evidence showed that the binding of metal ions were through azide and carbonyl moieties resulting in a six- coordinating metal ions in [Cr (III), Mn (II), Co (II) and Ni (II)]. The Vo (II), Cu (II), Zn (II), Cd (II) and Hg (II) were coordinated through azide group only forming square pyramidal
... Show More