Background: The demand for better esthetic during orthodontic treatment has increased nowadays, so orthodontists starting using esthetic arch wires, brackets and ligatures.Tooth colored brackets were introduced in different types of materials. Sapphire ceramic brackets are one type of esthetic brackets and their color stability remains the main concern for the clinicians and patients at the same time. The present study design to evaluate the effect of three different staining materials (pepsi, black tea and cigarette smoke) on the stainability of sapphire ceramic brackets bonded with three types of light cure orthodontic adhesives which include: Resilience, Enlight and Transbond. Materials and Methods: The sample consisted of three hundred sixty sapphire brackets. The brackets were divided according to bonding materials into three groups each group consist of one hundred twenty brackets, then each subgroup farther subdivided into four groups according to the material they were immersed (distilled water, black tea, Pepsi and cigarette smoke) with thirty brackets each, then Each group with ten brackets farther subdivided according to time interval of immersion in each media into three groups one day, seven days and fourteen days at 37°C in the incubator.A UV-Visible spectrophotometer (Shimadzu, UV -1800) was used to perform a light absorption test. Results: ANOVA and LSD post Hoc tests were used to identify the significant effects of the staining materials at a significance level P ≤ 0.05.It was found that the immersion time gradually influenced the color stability of the adhesive materials with sapphire brackets with the highest activity observed at fourteen days interval. The brackets bonded with Resilience light cure adhesive are the most type affected by staining materials, then followed by the brackets bonded with Transbond and finally the brackets bonded with Enlight light cure adhesive. For the staining materials it was found that the cigarette smoke is the most powerful staining material, followed by tea and finally pepsi. Conclusions: From the above result we can conclude that the type of adhesive must take in consideration when the esthetic brackets have been used.
Background: Mouthwashes used widely as ancillary to mechanical oral hygiene methods. Little information provided about the effect of mouthwashes on ions released from orthodontic brackets. Therefore, the present study has been established to evaluate the effect of different mouthwashes on the corrosion resistance and the biocompatibility of two brands of brackets. Materials and Methods: Eighty premolar stainless steel brackets were used (40 brackets from each brand). They were subdivided into four subgroups (n=10) according to immersion media (deionized distilled water, Corsodyl, Listerine and Silca herb mouthwashes). Each bracket was stored in a closely packed glass tube filled with 15ml of the immersion media and incubated for 45 days at
... Show MoreBackground: Separation and deboning of artificial teeth from denture bases present a major clinical and labortory problem which affect both the patient and the dentist. The optimal bond strength of artificial teeth with denture base reinforced with nanofillers and flexible denture bases and the effect of thermo cycling should be evaluated. This study was conducted to evaluate and compare the shear bond strength of artificial teeth (acrylic and porcelain) with denture bases reinforced by 5% Zirconium oxide nanofillers and flexible bases under the effect of different surface treatments and thermo cycling and comparing the results with conventional water bath cured denture bases. Material and methods: Two types of artificial teeth; acrylic and
... Show MoreBackground: Dental erosion is a common oral condition which results due to consumption of high caloric and low pH acidic food such as carbonated drinks and fruit juices. It is expected that these food types can cause irreversible damage to dental hard tissues and early deterioration of the dental restorations. So, this study aimed to evaluate and compare the erosive potential effects of orange fruit juice and Miranda orange drink on the microhardness of an orthodontic composite material. Materials and methods: Thirty discs with a thickness of 2 mm and a diameter of 10 mm were prepared from orthodontic bonding composite. The prepared discs were equally divided into three groups (n=10). Microhardness analysis was carried out both prior to
... Show MoreBackground: Information concerning the maximum bite force in human population is important to clinical orthodontics. Additionally, the influence of bite force on the vertical stability of any treatment result is important. The new position of the dentition should be compatible with the dynamics of the muscular and occlusal forces in all planes. This study was conducted to 1) to measure and compare maximum bite force, body height and weight among normal occlusion and malocclusion groups (cl I,cl II,cl III) in both gender 2) to evaluate the correlation between bite force and craniofacial morphology, body height and weight. Materials and Methods: The sample consists of 100 Iraqi adult subjects aged 18-25 years. It was classified in to four gr
... Show MoreBackground: Ceramic veneers represent the treatment of choice in minimally invasive esthetic dentistry; one of the critical factors in their long term success is marginal adaptation. The aim of the present study is to evaluate the marginal gap of ceramic veneers by using two different fabrication techniques and two different designs of preparation. Material and methods: A typodont maxillary central incisor used in the preparation from which metal dies were fabricated, which were in turn used to make forty stone dies. The dies divided into four experimental groups, each group had ten samples: A1: prepared with butt-joint incisal reduction and restored with IPS e.max CAD, A2: prepared with overlapped incisal reduction and restored with IPS e.
... Show MoreBackground: The microhardness of a composite resin is a vital parameter that is used to determine its clinical behavior. Measuring the microhardness of a composite resin has been used as an indirect method to assess its degree of conversion and extent of polymerization. The purpose of this in vitro study was to evaluate the effect of three curing distances (0, 2, and 4 mm) on the microhardness of the top and bottom surfaces of three types of flowable bulk-fill composite resins (smart dentin replacement, Opus bulk fill flow, and Tetric N). Material and method: Sixty-three specimens from the three types of composite resins (n=21) were fabricated using Teflon mold with a 4mm depth and a 5 mm internal diameter and cured for 20 seconds. For e
... Show MoreBackground: The marginal seal is essential for sealant success because penetration of bacteria under the sealant might allow caries onset or progression. The aim of the present study was to estimate and compare the microleakage of pit and fissure sealant after various methods of occlusal surface preparation. Materials and methods: Thirty non-carious premolars extracted for orthodontic reasons were equally divided into three groups. In group one, occlusal fissures were opened with round carbide bur, in group two, occlusal surfaces of the teeth were cleaned with a dry pointed bristle brush and samples of group three were cleaned with a slurry of fine flour of pumice in water using rubber cup. Then fissures of all teeth were etched using 35% p
... Show MoreBackground: Esthetic treatment is the options of patient seeking orthodontic treatment. Therefore this study was conducted to measure the concentration of Aluminum, Nickel, Chromium and Iron ions released from combination of monocrysralline brackets with different arch wires immersed in artificial saliva at different duration, to evaluate the corrosion point on different parts of the orthodontic appliances before and after immersion in artificial saliva, and to evaluate the corrosion potential of each group of the orthodontic appliances. Material and methods: Eighty orthodontic sets prepared. Each set represents half fixed orthodontic appliance, from the central incisor to the first molar, for the maxillary arch, each set consisted of molar
... Show MoreBackground: One of the major problems in endodontics is micro-leakage of root canal fillings which might contribute to the failure of endodontic treatment. To avoid this problem, a variety of sealers have been tested. The objective of this, in vitro, study was to evaluate the shear bond strength of four resin based sealers (AH plus, silver free AH26, RealSeal SE and Perma Evolution permanent root canal filling material) to dentin. Materials and Methods: Forty non-carious extracted lower premolars were used. The 2mm of the occlusal surfaces of teeth were sectioned, to expose the dentin surface. The exposed dentin surfaces of teeth were washed with 5ml of 2.5% NaOCl solution followed by 5ml of 17 % EDTA then rinsed by deionized water to remov
... Show More