Background: Dental implant surface technologies have been evolving rapidly to enhance a more rapid bone formation on their surface and improve implant therapy.Implant threads should be designed to increase surface contact areathat induced better stability. In addition, implant surface coating with Flaxseed was used to enhance bone formation at the bone-implant interface. Materials and methods: Ninety-six commercially pure titanium (CpTi) screws were implanted in rabbits' tibiae and divided into three groups as dual-threaded group, flaxseed-coated group and control group. All groups were evaluated mechanically, histologically and radiographically after each healing periods (2, 4, 6 and 8) weeks and the resulting data were statistically analyzed using ANOVA and t-test at 0.05 significance level. Results: Dual threaded implant recorded the highest value in removal torque testand it showed mature bone at 8 weeks period. Coated implant shows enhancement of osteoblast and it is the only modified implant that illustrates proliferating cartilage zone that later on degenerated and replaced by bone. Conclusion: Each modified implants shows different benefits whether a modification of the implant surface mechanically (dual-threaded) or by coating the implants with Flaxseed.
The long healing time of bone after tooth extraction in order to construct artificial teeth is uncomfortable to the patient because of aesthetic or masticatory problems in addition to the daily visit to dental clinic. The objective of this study was to evaluate the effect of 805 nm diode laser with long time intervals on repair of bone and skin incisions in rabbits through biochemical, radiological and histological findings. Eighteen New-Zealand rabbits were undergone surgical operations to make a cavity in the bone of the lower jaw, the rabbits were divided into two groups:- Group A (control group) containing nine rabbits. Group B (lased group) containing nine rabbits in which two cavities were done, one on the right side and the other
... Show MoreThe present study aimed to identify the therapeutic evaluation of chitosan extracted from the fungus cushroom and pure chitosan on glucose and lipid profile in the blood of 35 male rabbits with hyperlipidemia induced experimentally by cholesterol. The tests included estimation of glucose levels, total cholesterol, triglycerides, high-density lipoproteins, low-density lipoproteins, and very low-density lipoproteins. hyperlipidemia was induced in the male rabbits used in the study which was administered orally with cholesterol 150mg/kg body weight for a week. rabbits were divided into seven groups: control, cholesterol, pure chitosan, mushroom chitosan, cholesterol and pure chitosan, cholesterol and mushroom chitosan and cholestero
... Show MorePurpose: This study aimed to compare the stability and marginal bone loss of implants inserted with flapped and flapless approaches 8 weeks after surgery and 3 months after loading. Material and Methods: Thirty SLActive implants were inserted in 11 patients and early loaded with final restoration 8 weeks after healing period. The stability values determined by Osstell and the marginal bone loss measured by CBCT at the initial time (1st) and 8 weeks of the healing period (2nd) and 3 months after loading (3rd). Results: The overall survival rate was 100%. A significant increase in the 3rd implant stability value in the age of ˂ 40. A significant decrease in the 2nd implant stability value in both gender and traumatic zone with a flapless app
... Show MoreThe ongoing research to improve the clinical outcome of titanium implants has resulted in the implementation of multiple approaches to deliver osteogenic growth factors accelerating and sustaining osseointegration. Here we show the presentation of human bone morphogenetic protein 7 (BMP-7) adsorbed to titanium discs coated with poly(ethyl acrylate) (PEA). We have previously shown that PEA promotes fibronectin organization into nanonetworks exposing integrin- and growth-factor-binding domains, allowing a synergistic interaction at the integrin/growth factor receptor level. Here, titanium discs were coated with PEA and fibronectin and then decorated with ng/mL doses of BMP-7. Human mesenchymal stem cells were used to investigate cellular resp
... Show MoreThis study aimed to improve the microencapsulation technique using a type coating the encapsulation Layer by Layer, which provide the best protection for life Lactobacillus casei in the extrusion method and use the microencapsulation of materials of the protein concentrated by protein 80% and the coating with alginate and chitosan have the results showed the variation in the difference of the binding process encapsulation yield among the types of coating through. by studying of these the effect o stability of the bio probiotic free cell and the three types coated towards three different concentrations from bile salts 0, 0.3, 0.5 and 0.7% when the periods of time different of zero and two and three hours at incubation the recorded
... Show MoreIn this work, functionally graded materials were synthesized by centrifugal technique at different
volume fractions 0.5, 1, 1.5, and 2% Vf with a rotation speed of 1200 rpm and a constant rotation time, T
= 6 min . The mechanical properties were characterized to study the graded and non-graded nanocomposites
and the pure epoxy material. The mechanical tests showed that graded and non-graded added alumina
(Al2O3) nanoparticles enhanced the effect more than pure epoxy. The maximum difference in impact strength
occurred at (FGM), which was loaded from the rich side of the nano-alumina where the maximum value was
at 1% Vf by 133.33% of the sample epoxy side. The flexural strength and Young modulus of the fu
In this investigation, the mechanical properties and microstructure of Metal Matrix Composites (MMCs) of Al.6061 alloy reinforced by ceramic materials SiC and Al2O3 with different additive percentages 2.5, 5, 7.5, and 10 wt.% for the particle size of 53 µm are studied. Metal matrix composites were prepared by stir casting using vortex technique and then treated thermally by solution heat treatment at 530 0C for 1 hr. and followed by aging at 175 0C with different periods. Mechanical tests were done for the samples before and after heat treatment, such as impact test, hardness test, and tensile test. Also, the microstructure of the metal matrix composites was examine