Background: Change in palatal vault shape and Reinforcement of high impact acrylic denture base resin may in turn affect the dimensional accuracy of acrylic resin and affecting the fitness of the denture. The aim of study is to evaluate the effect of fiber reinforcement for high-impact acrylic resin denture base with different palatal vault shapes on linear dimensional change and effect of palatal vault shapes on linear dimensional changes of non-reinforced and fiber reinforced high impact denture base acrylic resin Material and method: Three different palatal vault shapes were prepared on standard casts using CNC (computer numerical control) machine. 60 samples of heat polymerized high impact acrylic resin maxillary denture base were fabricated onto each definitive cast according to manufacturer instruction. Samples divided into three main experimental groups represented the three different palatal vault shapes (20 samples for each main group); 1st rounded 2nd U-shaped and the 3rd groups V-shaped. Each main group divided into two subgroups (10 samples for each subgroup) representing non fiber reinforced high impact acrylic group as a control and the fiber reinforced high impact acrylic. The measurements of linear dimensional changes of denture bases done at two stages, 1st 24 hour after polymerization and 2nd measurement done after one month storage in distilled water at room temperature. Results and conclusion: Linear dimensional changes of high impact acrylic denture base not affected by glass fiber reinforcement p-value in all reference lines ≥ 0.05, while topographical change in maxillary vault shapes effects on the linear dimensional changes in woven glass fiber reinforced high impact acrylic denture base p-value < 0.05. Key words: High impact acrylic resin, topographical change in vault, woven glass fiber reinforcement.
Background: Polymethylmethacrylate (PMMA) has relatively unsatisfactory mechanical properties such as low flexural strength and impact strength also dimensional instability. Material and method: Zirconium silicate nanoparticles were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 1% and 1.5% by weight then mixed with powder using conventional procedure, (150) samples were prepared and divided into three groups, each group consisted of (50) samples, the first group prepared from PMMA without addition (control), another group with the addition of 1% wt Zrsio4 nanoparticles (experimental) and the third one with 1.5% wt Zrsio4 nanoparticles (experimental). Each group
... Show MoreBackground: Polymethyl methacrylate (PMMA) is used in denture fabrication and considered as the most reliable material for the construction of removable prosthodontic appliances. The material is far from ideal in fulfilling the mechanical requirements and the effect of autoclave processing has not been fully determined. The purpose of this study was to evaluate the effect of addition of salinized (ZrO2) Nano fillers in percentages 3%, 5% and 7% by weight on some properties of heat cured acrylic processed the by autoclave and compare it with 0% (control) group . Materials and methods: The silanized(ZrO2) Nano-particles was added to PMMA powder by weight in three different percentages 3%, 5% and 7%, mixed by probe ultra-sonication machine.
... Show MoreBackground: Fluoridated acrylic resin material can present more stable properties when compared with conventional one.The most widely used fluoride –containing substance added to dental resin materials is sodium fluoride (Naf). This study evaluated the effect of Naf in different concentration to the acrylic resin denture base material and its effect on tensile strength ,modules of elasticity with long –term water immersion (after 4 months immersion in de-ionized water) Materials and methods: Eighty specimens from dumbbells shaped metal pattern for tensile strength test were preparedaccording to ISO 527: 1993 plastic –Determination tensile properties ,in dimensions(60mm, 12mm, 3 ± 0.2mm) length, width and depth respec
... Show More
Background: Polymethyl methacrylate (PMMA) is the most commonly used material in denture fabrication. The material is far from ideal in fulfilling the mechanical requirement. The purpose of this study was to evaluate the effect of addition of 3% wt of treated (silanized) Titanium oxide Nano filler on some physical and mechanical properties of heat cured acrylic denture base material. Materials and methods: 100 specimens were constructed, 50 specimens were prepared from heat cure PMMA without additives (control) and 50 specimens were prepared from heat cure PMMA with the addition of TiO2 Nano fillers. Each group was divided into 5 sub groups according to the test performed which was mixed by probe ultra-sonication machine. Results: A highly
... Show MoreBackground: Separation and deboning of artificial teeth from denture bases present a major clinical and labortory problem which affect both the patient and the dentist. The optimal bond strength of artificial teeth with denture base reinforced with nanofillers and flexible denture bases and the effect of thermo cycling should be evaluated. This study was conducted to evaluate and compare the shear bond strength of artificial teeth (acrylic and porcelain) with denture bases reinforced by 5% Zirconium oxide nanofillers and flexible bases under the effect of different surface treatments and thermo cycling and comparing the results with conventional water bath cured denture bases. Material and methods: Two types of artificial teeth; acrylic and
... Show MoreBackground: Poly propylene fibers with and without silane treatment have been used to reinforce heat cure denture base acrylic but, some mechanical properties like transverse strength, impact strength, tensile strength, hardness, wear resistance and wettability. Which are related to the clinical use of the prosthesis are not evaluated yet. The aim of the study is to identify the influence of incorporation of treated and untreated fibers on these properties Materials and methods: Eighty four heat cure acrylic specimens were constructed by conventional flasking technique. They were divided into six groups according to the tests and each group was subdivided into two subgroups control and experimental groups (seven samples for each subgroup
... Show MoreBackground: Recently, Poly propylene fibers with and without plasma treatment have been used to reinforce heat cure denture base acrylic but, so far some of properties like tensile strength , wettability and wear resistance not evaluated yet, the aim of the study is to clarify the influence of incorporation of treated and untreated fibers on these properties. Materials and methods: Twenty one specimens were fabricated for every tested property(tensile strength, wear resistance and wettability) that classified into three groups(control, untreated poly propylene fibers reinforced specimens and Oxygen plasma treated group)and for each test sevens amples were used(n=7). Tensile strength was tested using Instron universal testing machine, wear
... Show MoreThis paper displays the effect of uncoated and coated chopped carbon fibers with alumina Al2O3 or Tri calcium phosphate (TCP) on the impact strength of acrylic poly methyl methacrylate (PMMA) denture base resin. To improve bonding between carbon fibers and coating materials powders, the surface of carbon fibers has been treated with Para amino benzoic acid (C9H10N2O3) and poly vinyl alcohol (PVA) was also used. The morphology of the coating layers has been examined by field emission scanning electron microscope (FE-SEM). From the results, PMMA reinforced with uncoated chopped carbon fiber has high impact strength value but still have bad aesthetic. Samples prepared b
... Show MoreThis work aims to investigate the tensile and compression strengths of heat- cured acrylic resin denture base material by adding styrene-butadiene (S- B) to polymethyl methacrylate (PMMA). The most well- known issue in prosthodontic practice is fracture of a denture base. All samples were a blend of (90%, 80%) PMMA and (10%, 20%) S- B powder melted in Oxolane (Tetra hydro furan). These samples were chopped down into specimens of dimensions 100x10x2.5mm to carry out the requirements of tensile tests. The compression strength test specimens were shaped into a cylinder with dimensions of 12.7mm in diameter and 20mm in length. The experimental results show a significant increase in both tensile and compression strengths when compared to cont