Background: This study aimed to evaluate the effect of zirconia different surface treatments (primer, sandblast with 50μmAl2O3, Er,Cr:YSGG laser) on shear bond strength between zirconia surface and resin cement. Material and methods: Sixty presintered Y-TZP zirconia cylinder specimens (IPS e.max ZirCAD, Ivoclar vivadent) will be fabricated and sintered in high temperature furnace of (1500 C for 8 hours) according to manufacturer’s instructions to the selected size and shape of (5mm. in diameter and 6mm in height). All specimens were ground flat using 600.800.1000.1200, aluminum oxide abrasive paper to obtain a standardized surface roughness. Surface roughness values were then recorded in µm using surface roughness tester (profilometer) to obtain a standardized data base line for all samples. The specimens were then randomly divided into three main groups (n=20); group A: no surface treatment (control group), group B: specimens in this group treated with 50μm Al2O3 and group C: specimens in this group treated with Er,Cr:YSGG laser. Sixty sound human premolars were used in this study, after construction of acrylic blocks, the occlusal surface of the teeth were ground flat, with diamond cutting disk to obtain a flat dentine surface . Prior to cementation of zirconia cylinders to tooth specimens subgroups (A1,B1,C1) will receive a coat of metal/zirconia primer and left to react for three minutes, while the subgroups (A2,B2,C2) were left undisturbed. Bonding surface of zirconia cylinder was then luted with SpeedCEM self adhesive resin cement under a static load of 2Kg. placed on the vertical arm of the surveyor and allowed to auto cure for 4minutes.The final cemented specimens were then stored in distilled water at room temperature for 24hours. All specimens were subjected to shear loading force in a universal testing machine at crosshead speed of 1mm/min. The shear bond strength values were analyzed statistically with one-way ANOVA; the fractured surfaces of zirconia cylinders were examined with a stereo-microscope to observe the failure mode. Results: The air borne-particle of 50μm followed by primer application showed significantly the higher bond strength than other groups. Conclusion : Within the limitation of this study, the results showed that sandblasting the bonding surface of zirconium cylinders with 50μmAl2O3 produced the highest values of shear bond strength , also the use of primer enhanced shear bond strength as well. Keyword: zirconia surface treatments, shear bond strength.
This study aims to assess the accuracy of digital elevation model (DEM) created with utilization of handheld Global Positioning System (GPS) and comparing with Advanced Spaceborne Thermal Emission and Reflection Radiometer Global Digital Elevation Model (ASTER GDEM), version 2. It is known that the quality of the DEM is affected by both of accuracy of elevation at each pixel (absolute accuracy) and accuracy of presented morphology (relative accuracy). The University of Baghdad, Al Jadriya campus was selected as a study area to create and analysis the resulting DEM. Additionally, Geographic Information System (GIS) was used to visualize, analyses and interpolate GPS track points (elevation data) of the study area. In this
... Show MoreThis paper presents an experimental study of cooling photovoltaic (PV) panels using evaporative cooling. Underground (geothermal energy) water used to extract heat from it during cooling and cleaning of PV panels. An experimental test rig was constructed and tested under hot and dusty climate conditions in Baghdad. An active cooling system was used with auxiliary an underground water tank to provide cold water as a coolant over both PV surfaces to reduce its temperature. The cellulose pad has been arranged on the back surface and sprays cooling on the front side. Two identical PV panels modules used: without cooling and evaporative water cooling. The experiments are comprised of four cases: Case (I): backside cooling, Ca
... Show MoreThe challenge to incorporate usability evaluation values and practices into agile development process is not only persisting but also systemic. Notable contributions of researchers have attempted to isolate and close the gaps between both fields, with the aim of developing usable software. Due to the current absence of a reference model that specifies where and how usability activities need to be considered in the agile development process. This paper proposes a model for identifying appropriate usability evaluation methods alongside the agile development process. By using this model, the development team can apply usability evaluations at the right time at the right place to get the necessary feedback from the end-user. Verificatio
... Show MoreIn this work, an inventive photovoltaic evaporative cooling (PV/EC) hybrid system was constructed and experimentally investigated. The PV/EC hybrid system has the prosperous advantage of producing electrical energy and cooling the PV panel besides providing cooled-humid air. Two cooling techniques were utilized: backside evaporative cooling (case #1) and combined backside evaporative cooling with a front-side water spray technique (case #2). The water spraying on the front side of the PV panel is intermittent to minimize water and power consumption depending on the PV panel temperature. In addition, two pad thicknesses of 5 cm and 10 cm were investigated at three different water flow rates of 1, 2, and 3 lpm. In Case #1,
... Show MoreRecent years have witnessed an increase in the use of composite coatings for numerous applications, including aerospace, aircraft, and maritime vessels. These materials owe this popularity surge to the superior strength, weight, stiffness, and electrical insulation they exhibit over conventional substances, such as metals. The growing demand for such materials is accompanied by the inevitable need for fast, accurate, and affordable nondestructive testing techniques to reveal any possible defects within the coatings or any defects under coating. However, typical nondestructive testing (NDT) techniques such as ultrasonic testing (UT), infrared thermography (IRT), eddy current testing (ECT), and laser shearography (LS) have failed to p
... Show MoreObjective: The aim of this study was to formulate and in vitro evaluate fast dissolving oral film of practically insoluble bromocriptine mesylate to enhance its solubility and to improve its oral bioavailability by avoiding first pass effect as well as to produce an immediate release action of the drug from the film for an efficient management of diabetes mellitus type II in addition to an improvement of the patient compliance to this patient- friendly dosage form. Methods: The films were prepared by the solvent casting method using hydroxypropyl methylcellulose of grades (E3, E5, E15), polyvinyl alcohol (PVA), pectin and gelatin as film-forming polymers in addition to polyethene glycol 400 (PEG400), propylene glycol (PG) and glycerin were
... Show MoreThis research involves study effect of chloride ions in concentration range (0.01 – 0.50 mol.dm-3) on the corrosion behavior of Al-Zn alloy in basic media of 1x10-3 mol.dm-3 NaOH at pH=11 and four different temperatures in the range (298-313 K). Cathodic and anodic Tafel slopes (bc &ba) and transfer coefficients (αc & αa) were calculated and the results interprets according to the variation of the rate – determining steps. The results also indicate that the chloride ions are bonded chemically in the interface as an initial step of formation of different mixed oxohydroxy – and chloro complexes. Polarization resistance (Rp) is calculates
... Show MoreBackground: The miswak is a teeth cleaning twig made from a twig of the Salvadora persica tree (known as arak in Arabic).A traditional alternative to the modern toothbrush, it has a long, well-documented history and is reputed for its medicinal benefits. It also features prominently in Islamic hygienical jurisprudence. Materials and methods: Twenty maxillary first premolars were treated with the selected solutions which included siwak water extract (5%, 10%) and sodium fluoride 0.05% for 2minutes once daily for 20 days interval, deionized water was used as control negative. Then the concentration of the dissolved calcium ion in the etching solution of 2N HCL was measured. Results: The least amount of the dissolved calcium ion was registere
... Show More