Background: This study aimed to evaluate the effect of zirconia different surface treatments (primer, sandblast with 50μmAl2O3, Er,Cr:YSGG laser) on shear bond strength between zirconia surface and resin cement. Material and methods: Sixty presintered Y-TZP zirconia cylinder specimens (IPS e.max ZirCAD, Ivoclar vivadent) will be fabricated and sintered in high temperature furnace of (1500 C for 8 hours) according to manufacturer’s instructions to the selected size and shape of (5mm. in diameter and 6mm in height). All specimens were ground flat using 600.800.1000.1200, aluminum oxide abrasive paper to obtain a standardized surface roughness. Surface roughness values were then recorded in µm using surface roughness tester (profilometer) to obtain a standardized data base line for all samples. The specimens were then randomly divided into three main groups (n=20); group A: no surface treatment (control group), group B: specimens in this group treated with 50μm Al2O3 and group C: specimens in this group treated with Er,Cr:YSGG laser. Sixty sound human premolars were used in this study, after construction of acrylic blocks, the occlusal surface of the teeth were ground flat, with diamond cutting disk to obtain a flat dentine surface . Prior to cementation of zirconia cylinders to tooth specimens subgroups (A1,B1,C1) will receive a coat of metal/zirconia primer and left to react for three minutes, while the subgroups (A2,B2,C2) were left undisturbed. Bonding surface of zirconia cylinder was then luted with SpeedCEM self adhesive resin cement under a static load of 2Kg. placed on the vertical arm of the surveyor and allowed to auto cure for 4minutes.The final cemented specimens were then stored in distilled water at room temperature for 24hours. All specimens were subjected to shear loading force in a universal testing machine at crosshead speed of 1mm/min. The shear bond strength values were analyzed statistically with one-way ANOVA; the fractured surfaces of zirconia cylinders were examined with a stereo-microscope to observe the failure mode. Results: The air borne-particle of 50μm followed by primer application showed significantly the higher bond strength than other groups. Conclusion : Within the limitation of this study, the results showed that sandblasting the bonding surface of zirconium cylinders with 50μmAl2O3 produced the highest values of shear bond strength , also the use of primer enhanced shear bond strength as well. Keyword: zirconia surface treatments, shear bond strength.
This research presents a particular designing strategy for a free form of surfaces, constructed by the lofting design method. The regarded surfaces were created by sliding a B-spline curves (profile curves), in addition to describing an automatic procedure for selective identification of sampling points in reverse engineering applications using Coordinate Measurement Machine. Two models have been implemented from (Ureol material) to represent the different cases of B-spline types to clarify its scope of application. The interior data of the desired surfaces was designed by MATLAB software, which then were transformed to UG-NX9 software for connecting the sections that were designed in MATLAB program and obtaining G-code programs for the
... Show MoreIn this work, a Photonic Crystal Fiber (PCF) sensor based on the Surface Plasmon Resonance (SPR) technology was proposed. A thin layer of gold (Au) was deposited on a D-shaped Photonic Crystal Fiber (PCF), which was coated with plasmonic chemically stable gold material with a thickness of 40nm. The performance parameters like sensitivity including wavelength sensitivity and amplitude sensitivity and resolution were evaluated by simulation using COMSOL software. The proposed sensor was created by using the finite element approach, it is numerically examined. The results show that the surface of D-shaped Photonic Crystal Fiber coated with Au behaves as a sensor to detect the refractive index (IR) of toxic metal ions. The impacts of the str
... Show MoreI
In this study, optical fibers were designed and implemented as a chemical sensor based on surface plasmon resonance (SPR) to estimate the age of the oil used in electrical transformers. The study depends on the refractive indices of the oil. The sensor was created by embedding the center portion of the optical fiber in a resin block, followed by polishing, and tapering to create the optical fiber sensor. The tapering time was 50 min. The multi-mode optical fiber was coated with 60 nm thickness gold metal. The deposition length was 4 cm. The sensor's resonance wavelength was 415 nm. The primary sensor parameters were calculated, including sensitivity (6.25), signal-to-noise ratio (2.38), figure of merit (4.88), and accuracy (3.2)
... Show MoreFree water surface constructed wetlands (FSCWs) can be used to complement conventional waste water treatment but removal efficiencies are often limited by a high ratio of water volume to biofilm surface area (i.e. high water depth). Floating treatment wetlands (FTWs) consist of floating matrices which can enhance the surface area available for the development of fixed microbial biofilms and provide a platform for plant growth (which can remove pollutants by uptake). In this study the potential of FTWs for ammoniacal nitrogen (AN) removal was evaluated using experimental mesocosms operated under steady-state flow conditions with ten different treatments (two water depths, two levels of FTW mat coverage, two different plant densities and
... Show MoreThis paper aims to study the rate of star formation (SFR) in luminous infrared galaxies at different wavelengths using distance measurement techniques (dl, dm) and to know which methods are the most accurate to determine the rate of star formation as we present through this research the results of the statistical analysis (descriptive statistics) for a sample of luminous infrared galaxies. The data used in this research were collected from the NASA Extragalactic Database (NED) and HYPERLEDA, then used to calculate the star formation rate and indicate the accuracy of the distance methods used (dl, dm). Two methods were tested on Hα, OII, FIR, radio continuum at 1.4 GHz, FUV, NUV, and total (FUV + FIR). The results showed that the dl
... Show MoreThe present study aimed to investigate the histology of the testis in golden hamster during 1, 28 and 60 day of old. Tissue samples were processed, sectioned and subjected to specific stains to reveal histological details. Observation of one day old showed the testicle enclosed by undifferentiated thin layer of testicle capsule which consisted of undifferentiated myoblasts and fibroblasts small size seminiferous tubules appeared, one layer of spermatogonium cells (Type-A) which revealed mitotic figures, at 28 day old the capsule was consisted of thick outer fibromuscular layer and thick inner vascular layer that revealed encouraged blood vessels and cells, Spermatogonial cells type-A & B appeared as large
... Show MoreThis study aims to investigate the adequacy of composite cellular beams with lightweight reinforced concrete deck slab as a structural unit for harmonic loaded buildings. The experimental program involved three fixed-ends supported beams throughout 2140 mm. Three concrete types were included: Normal Weight Concrete (NWC), Lightweight Aggregate Concrete (LWAC), and Lightweight Fiber Reinforced Aggregate Concrete (LWACF). The considered frequencies were (5, 10, 15, 20, 25, and 30) Hz. It was indicated that the harmonic load caused a significant influence on LWAC response (64% greater than NWC) and lattice cracks were observed, especially at 30 Hz. As for LWACF slab, no cracks appeared,
The nephrotoxicity induced by methotrexate is a severe condition that greatly affects its therapeutic potential and has a significant inflammatory component. Fimasartan is an angiotensin receptor blocker that offers organ-protective effects and may be useful in mitigating renal injury. The present study explored the anti-inflammatory potential of two doses of fimasartan against methotrexate-mediated nephrotoxicity. Albino rats were intraperitoneally administered a single methotrexate (20 mg/kg). Intraperitoneal treatment with fimasartan (5 or 10 mg/kg/day) was initiated on day two after methotrexate injection and continued for seven consecutive days. Methotrexate significantly increased serum urea, creatinine, and NGAL concentrations. It al
... Show More