ABSTRACT Background: One of the major problems of all ceramic restorations is their probable fracture against the occlusal forces. The objective of this in vitro study was to evaluate the effect of two gingival finishing lines (90°shoulder and deep chamfer) on the fracture resistance of full contour CAD/CAM and heat press all-ceramic crowns. Materials and Methods: Thirty two maxillary first premolars were prepared to receive full contour CAD/CAM (zolid) and heat press (Cergo Kiss) ceramic crowns using a special paralleling device (Parallel-A-Prep). The teeth were divided into four groups according to the type of finishing line prepared. Each crown was cemented to its corresponding tooth using self-etch, self-adhesive dual cure resin cement. Following storage for 1 week in distilled water at room temperature, teeth were subjected to thermal cycling. Fracture resistance was determined using a universal testing machine, and the samples were investigated microscopically from the point of view of the origin of the failure. Statistical analysis was carried out using the one-way ANOVA and Student’s t-tests. Results: The mean values of fracture resistance for CAD/CAM group showed 1367.250+178.967 N for 90°shoulder margins and 1109.250+252.455 N for the deep chamfer margins. ANOVA test results revealed high significance between and within the groups. The mean values of fracture resistance for heat press group were 548.562+272.471 N for 90°shoulder margins and 247.912+96.995 N for the deep chamfer margins expressing statistical significance. Conclusions: The results of this study pointed to a relationship between the design of the cervical finishing line and the fracture strength of the full CAD/CAM crowns and the full heat press ceramic crowns. Both 90° shoulder and deep chamfer finishing lines are suitable for zolid crowns while the 90° shoulder is more suitable for the Cergo Kiss crowns than the deep chamfer preparation. Key words: Full contour, All-ceramic crowns, CAD/CAM, Heat press, Fracture strength.
This research aims to study the effect of microwave furnace heat on the mechanical properties and fatigue life of aluminum alloy (AA 2024-T3). Four conditions were used inside microwave furnace (specimens subjected to heat as dry for 30 and 60min. and specimens subjected to heat as wet (water) for 30 and 60 min.), and compared all results with original alloy (AA 2024-T3). Tensile, fatigue, hardness and surface roughness tests were used in this investigation. It is found that hardness of dry conditions is higher than wet conditions and it increases with increasing of time duration inside microwave furnace for dry and wet conditions. Also, tensile strength has the same behavior of hardness, but it increases with decreasing
... Show MoreThe semiconductor ZnO is one of II – VI compound group, it is prepare as thin films by using chemical spray pyrolysis technique; the films are deposited onto glass substrate at 450 °C by using aqueous zinc chloride as a spray solution of molar concentration 0.1 M/L. Sample of the prepared film is irradiating by Gamma ray using CS 137, other sample is annealed at 550°C. The structure of the irradiated and annealed films are analyzed with X-ray diffraction, the results show that the films are polycrystalline in nature with preferred (002) orientation. The general morphology of ZnO films are imaged by using the Atomic Force Microscope (AFM), it constructed from nanostructure with dimensions in order of 77 nm.
The optical properties o
Self- curing is the potential of lightweight aggregate to absorption great amount of water thru mixing which prominently can moves to the paste during hydration process. Self- curing empowers a water to be distributes more evenly act out the cross section. Whereas, the external curing water is only able to penetrate several millimetres into concrete with low water cement ratio. Brick dust accumulates in the demolish site creates serious environmental contamination. This study investigates the effect of brick dust recovered from construction site on the Properties of mortar cured in three curing conditions. Mortar in this study produced using BD as cement additive with (2, 4, 6, and 8) % by weight of cement. BD was used a
... Show MoreThe research aims to evaluate Evaluation of the investments Iraqi fund for External development through the application of financial tools to a number of companies of the Iraqi Fund for External Development, and from the point of view to achieve the best returns from investment and the feasibility of the investments of the Iraqi Fund for External Development and the research community represents the Iraqi Fund for External Development and the amount of (28) A company, while the research sample is (4) companies (the Arab Petroleum Transportation Services Company, the Arab Iraqi Company for Livestock Development, the Bauhaus Company for prefabricated buildings and mineral installations, the Arab Fisheries Company) that were chosen
... Show MoreBackground: The surface properties of the titanium alloy plays a significant role in the bond of the dental implant with living bone and modification of the implant surface could enhance osseointegration. This study was aimed to investigate the effect of different durations of heat treatment on the surface properties of titanium alloy for dental implants. Materials and methods: Twenty disks of (Ti-6Al-4V) alloy were prepared. The sample was divided into four test groups to study the effect of different duration of heat treatment to the surface topography; surface chemistry, titanium oxide layer thickness, blood contact angle, & blood drop diameter of titanium alloy samples were investigated to evaluate the effect of different durations of
... Show MoreIn this study, the investigation of flavorings used in 567 model of local food products and imported in our local markets through information contents cards media shoddy standard Iraqi has been found that foods that appeal to children of sugar confectionery and Crapt and other barely Atkhalo of flavorings used that lead tohealth risks
In this paper the full stable Banach gamma-algebra modules, fully stable Banach gamma-algebra modules relative to ideal are introduced. Some properties and characterizations of these classes of full stability are studied.