Background: Polymethyl methacrylate (PMMA) is used in denture fabrication and considered as the most reliable material for the construction of removable prosthodontic appliances. The material is far from ideal in fulfilling the mechanical requirements and the effect of autoclave processing has not been fully determined. The purpose of this study was to evaluate the effect of addition of salinized (ZrO2) Nano fillers in percentages 3%, 5% and 7% by weight on some properties of heat cured acrylic processed the by autoclave and compare it with 0% (control) group . Materials and methods: The silanized(ZrO2) Nano-particles was added to PMMA powder by weight in three different percentages 3%, 5% and 7%, mixed by probe ultra-sonication machine.Two hundred specimens were constructed and processed by autoclave and divided into 5 groups according to the test (each group consist of 40 specimens ) and each group was subdivided into 4 sub-groups according to the percentage of added (ZrO2) nano-particles( with 10 specimens for each subgroups) . The tests conducted were transverse strength, hardness (shore D), Impact strength test, surface morphology and apparent porosity. AFM can provide 3D image of the specimen the homogeneity of nanostructure film, roughness of surface and crystallite size. Scanning electron microscope SEM of control and salinized Nano ZrO2 reveal the Nano fillers distribution and it is shaped. Results: Highly significant increase in impact strength recorded when acrylic (vertex) mixed with 3%, 5% ZrO2 nano filler, while a non-significant reduction was observed with 7% ZrO2 addition in comparison to control. Non-significant improvement in transverse strength when 3% ZrO2 was added, 5% nano addition ZrO2 improved transverse strength significantly while 7% nano addition showed anon significant reduce when these groups compared to the control group .Anon significant reduction in the deformity was seen within 3% nano addition ZrO2 also 5% nano ZrO2 addition reduce the deformity significantly and significant increase was recorded when 7% nano addition ZrO2 was add and when these groups are compared to the control group. A significant increase in surface hardness was observed with the addition of (ZrO2) nano-particles to (PMMA) at the percentage of 3%, highly significant increase at 5% and 7% with addition of modified nano-ZrO2. A non-significant decrease in apparent porosity at 3% and highly significant decrease in apparent porosity at 5% and 7% with addition of modified nano-ZrO2 were observed. SEM results showed a good distribution of the modified nano-ZrO2 fillers at 3%, 5% and showed aggregation at 7% in the polymer matrix. Conclusion: The addition of modified nano-ZrO2 particles to acrylic resin cured by autoclave improved impact and transverse strength of denture base nano composite containing 5% of nano-ZrO2. And this strength decreases with further increase of nano-ZrO2 filler content. Also addition of modified nano-ZrO2 slightly increaseshardness, thesurface roughness and the apparent porosity also decrease by addition of nano ZrO2 percentage increase. Key words: Salinized (ZrO2) nano fillers, PMMA.
Background: Glass ionomer restorations are widely employed in the field of pediatric dentistry. There is a constant demand for a durable restoration that remains functional until exfoliation. This study aimed to measure and compare the effect of a novel coating material (EQUIA Forte Coat) on the microleakage of glass hybrid restoration (EQUIA Forte HT) in primary teeth. Material and method: Thirty cavitated (class-II) primary molars were allocated randomly into two groups based on the coat application; uncoated (control) and coated group (experimental). Cavities were prepared by the use of a ceramic bur (CeraBur) and restored with EQUIA Forte HT with or without applying a protective coat (EQUIA Forte Coat). Samples went through the
... Show MoreBackground: Glass ionomer restorations are widely employed in the field of pediatric dentistry. There is a constant demand for a durable restoration that remains functional until exfoliation. This study aimed to measure and compare the effect of a novel coating material (EQUIA Forte Coat) on the microleakage of glass hybrid restoration (EQUIA Forte HT) in primary teeth. Material and method: Thirty cavitated (class-II) primary molars were allocated randomly into two groups based on the coat application; uncoated (control) and coated group (experimental). Cavities were prepared by the use of a ceramic bur (CeraBur) and restored with EQUIA Forte HT with or without applying a protective coat (EQUIA Forte Coat). Samples went through the therm
... Show MoreThe tetradentate N2O2 Schiff base ligand, which is produced via the condensation reaction of 2-hydroxynaphthaldehyde with phthalohydrazide, is prepared in this work with a fair yield. The prepared ligand was characterized using a microanalysis technique (C.H.N), UV-vis, FTIR, 1H-,13C-NMR, mass spectrometry, and thermal gravimetric analysis (TGA). New complexes were synthesized by a reaction between ligand (N'1E,N'2Z)-N'1,N'2-bis((1-hydroxynaphthalen-2yl)methylene)phthalohydrazide and metal chloride of Co+2, Ni+2, and Zn+2 ions in absolute ethanol. The present complexes are also characterized by techniques such as C.H.N, UV-vis, FTIR, TGA, molar conductivity, atomic absorption, and magnetic moment measurements. The in vitro antimicro
... Show MoreCu-Al-Ni shape memory alloy specimens has been fabricated using powder metallurgy technique with tube furnace and vacuum sintering environment , three range of Nb powder weight percentage (0.3,0.6,0.9)% has been added. Micro hardness and sliding wear resist has been tested followed by X-ray diffraction, scanning electron microscope (SEM) and energy dispersive X-ray spectroscope (EDX) for micro structure observation. The experimental test for the samples has showed that the increase of Nb powder weight percentage in the master alloy has a significant effect on increasing the hardness and decreasing the wear resist therefore it will enhance the mechanical properties for this alloy.
in this paper the second order neutral differential equations are incestigated are were we give some new suffucient conditions for all nonoscillatory
The solidification process in a multi-tube latent heat energy system is affected by the natural convection and the arrangement of heat exchanger tubes, which changes the buoyancy effect as well. In the current work, the effect of the arrangement of the tubes in a multi-tube heat exchanger was examined during the solidification process with the focus on the natural convection effects inside the phase change material (PCM). The behavior of the system was numerically analyzed using liquid fraction and energy released, as well as temperature, velocity and streamline profiles for different studied cases. The arrangement of the tubes, considering seven pipes in the symmetrical condition, are assumed at different positions in the system, i
... Show MoreThe study was conducted at the College of Agricultural Engineering Sciences - University of Baghdad in 2022. It aimed to improve the growth of the European black Henbane plant (
PVC/Kaolinite composites were prepared by the melt intercalation method. Mechanical properties, thermal properties, flammability and water absorption percentage of prepared samples were tested. Mechanical characteristic such as tensile strength, elongation at break; hardness and impact strength (charpy type) were measured for all samples. It was found that the tensile strength and elongation at break of PVC composites decreased with increasing kaolinite loading. Also, the hardness of the composites increases with increase in filler content .The impact strength of the composites at the beginning increases at lower kaolinite loadings is due to the lack of kaolin adhesion to the matrix. However, at higher kaolin loadings. This severe agglom
... Show More