Background: In recent years, the immediate loading of dental implants has become more accepted as a standard protocol for the treatment of the edentulous area. Success in implant dentistry depends on several parameters that may improve phenomenon of osseointegration and new bone formation in close contact with the implant. The aim of study was to evaluate the effect of strontium chloride coating of screw shape commercially pure titanium dental implant osseointegration at bone - implant interface by histomorphometric analysis and compare with hydroxyapatite coating at 2 time periods (2 weeks and 6 weeks). Materials and methods: Electrophoretic Deposition Technique (EPD) was used to obtain a uniform coating layer on commercially pure titanium screws. The tibia of 4 white New Zealand rabbits was chosen as implantation sites. Each tibia of rabbit received two screws, one strontium chloride coated and one hydroxyapatite coated and a total 30 histological sections were obtained for each coating material in each period of time. Histomorphometric analysis was performed to measure new bone formed ratio between implant and original bone, after 2 and 6 weeks healing periods. Results: There was increased in new bone formation ratio for the strontium chloride coated implants than hydroxyapatite coated implants and over the two periods of time. There was an increase in the new bone formation ratio at bone-implant interface with time. Conclusion: Coating commercially pure titanium implant with strontium chloride was more efficient in increasing osseointegration at bone implant interface than hydroxyapatite , which was demonstrated by higher new bone formation and maturation at the two periods of time 2 weeks and 6 weeks after implantation. Keywords: Histomorphometric, commercially pure titanium, strontium chloride, hydroxyapatite.
Aim: To evaluate the wettability and microhardness of Zirconium (ZrO2) dental material when coated with different concentrations of Faujasite. Materials and methods: 30 circular disks produced from ZrO2, then each group is classified into 10 control groups, 10 coated groups with 3% Faujasite, and 10 coated groups with 7% faujasite by electro-spun tool to study variable properties in hardness and water contact angle of implant materials. Results: This study stated the high hardness in 7% of faujasite concentration for ZrO2, in addition, the contact angle decreased gradually until reach 0 ᵒ in 7% concentration of faujasite with ZrO2 Conclusion: Water contact angle (WCA) declined till disappeared in (7% wt.) of faujasite coated with the Z
... Show MoreBackground: Dental implant considers a unique treatment option for the replacement of missing dentition. The new trend of implants is looking for materials which accelerate bone formation in bone implant interface and enhance osseointegration to provide immediate loading directly after placement and decrease the time period which is disturbs patients and uncomfortable. The aim of the study was to evaluate the effect of nano zirconium oxide (ZrO2) and nano hydroxyapatite (Hap) mixture coating of screw shaped commercially pure titanium (cpTi) implants on bond strength at the bone implant interface with torque removal test and histological analysis in comparison with non coated implants. Materials and methods: Forty screws were machined from c
... Show MoreIn this research, the study of thermal treating by laser, plasma glow discharge and tubular furnace on Ti-6Al-4V alloy coated with hydroxyapatite by methods of dip coating and electrophoretic deposition .A group of samples was coated by dip coating and another group was coated by electrophoretic deposition. The first group was treated by pulse laser 10 (mJ) as energy for samples from both coating with uniform distributed pulses on every single sample surface, The second thermal treating was made by plasma glow discharge in a locally made system with argon atmosphere, 600 Volt , and 6 cm distance between the electrodes, The third treating was made by tubular furnace in air atmosphere and 400 °C for 1 hour duration. T
... Show MoreObjective: Evaluation of the poly ether keton keton polymer (PEKK) coating material on the commercial pure titanium disks (CP Ti) with or without laser surface structuring. Design: In vitro experimental study of PEKK polymer coated material on the CP Ti disks with or without laser surface structuring. Materials and methods: coating the surface of the commercial pure titanium (CP Ti) disks with PEKK polymer was performed via using frictional mode CO2 laser, then the samples disks analyzed by using FESEM. Results: the FESEM reveal good adherence and distribution of the PEKK coated material over the CP Ti substrate by using the frictional mode CO2 laser at 2 watt and 6 ms pulse duration. Conclusion: the frictional mode CO2 laser considered an
... Show MoreBackground: Dental implant surface technologies have been evolving rapidly to enhance a more rapid bone formation on their surface and improve implant therapy.Implant threads should be designed to increase surface contact areathat induced better stability. In addition, implant surface coating with Flaxseed was used to enhance bone formation at the bone-implant interface. Materials and methods: Ninety-six commercially pure titanium (CpTi) screws were implanted in rabbits' tibiae and divided into three groups as dual-threaded group, flaxseed-coated group and control group. All groups were evaluated mechanically, histologically and radiographically after each healing periods (2, 4, 6 and 8) weeks and the resulting data were statistically analy
... Show MoreDue to the advantages over other metallic materials, such as superior corrosion resistance, excellent biocompatibility, and favorable mechanical properties, titanium, its alloys and related composites, are frequently utilized in biomedical applications, particularly in orthopedics and dentistry. This work focuses on developing novel titanium-titanium diboride (TiB2; ceramic material) composites for dental implants where TiB2 additions were estimated to be 9 wt.%. In a steel mold, Ti-TiB2 composites were fabricated using a powder metallurgy technique and sintered for five hours at 1200 °C. Microstructural and chemical properties were analyzed by energy dispersive X-ray spectroscopy (EDX), scanning electron microscopy (SEM), and X-ra
... Show MoreIn this research we investigated the corrosion behavior of the commertialy pure titanium and Ti-6Al-4V alloy that coated with hydroxyapatite by electrochemical deposition with applied voltage (6,9,12) Volt from aqueous solution containing Ca(NO3)2.H2O =7.0 gm/l , (NH4)2HPO4 =3.5 gm/l , Na(NO3)2 = 8.5 gm/l in order to improve the bonding strength of hydroxyapetite and medical metals and alloys and increasing the biocompatibility. The coating layer morphology was investigated by XRD, Optical microscope , and SEM tests, the corrosio tests was made by use senthesys simulated body fluid (SBF) , and we found that the propreate voltage for coatint on Ti was 9 Volt and for Ti-6Al-4Vwas12Volt.
Electrophoretic Deposition (EPD) process offers various advantages like the fabrication of the ceramic coatings and bodies with dense packing, good sinterability and homogenous microstructure. The variables namely (applied potential, deposition time and sintering temperature) affected the development of hydroxyapatite (HAP) coatings. The coating weight and thickness were found to increase with the increase in applied potential or coating time. Sintering temperature was found to affect in change phases of the metal, furthermore the firing shrinkage of the HAP coating on a constraining metal substrate leads to serve cracking. XRD Characterization indicates the formation of a contamination free phase pure, and the optical micrographs show th
... Show MoreThis research focuses on improvement of the corrosion behaviour of commercial pure titanium (Ti) grade II when exposed to Hank’s solution through different surface treatments. The disc shape of titanium samples were constructed to be divided according to their surface treatment. The first experimental group the Ti sample was exposed to computer numerical control (CNC) fiber laser machine. Whereas, the other experimental group the Ti sample was only coated with Polyetherketon keton (PEKK) by using carbon dioxide (CO2) laser technique while the last experimental group the Ti sample was treated with CNC fiber laser followed by PEKK coating by using CO2 laser technique. All were compared with the untreated control group. The electrochemical a
... Show MorePurpose This study investigated periodontal ligament (PDL) restoration in osseointegrated implants using stem cells. Methods Commercial pure titanium and zirconium oxide (zirconia) were coated with beta-tricalcium phosphate (β-TCP) using a long-pulse Nd:YAG laser (1,064 nm). Isolated bone marrow mesenchymal cells (BMMSCs) from rabbit tibia and femur, isolated PDL stem cells (PDLSCs) from the lower right incisor, and co-cultured BMMSCs and PDLSCs were tested for periostin markers using an immunofluorescent assay. Implants with 3D-engineered tissue were implanted into the lower right central incisors after extraction from rabbits. Forty implants (Ti or zirconia) were subdivided according to the duration of implantation (healing period: 45 o
... Show More