Background: It may be an important prospective clinical use of manufacturing of porous implant for clinical situations, such as cases of limitation in bone height, low bone density .The small segment of porous implant an effective osseointegration allows increasing in contact area provided for small segmented porous provided by its surface configuration. This study was done to Fabricate porous titanium implants by powder technology, as well as the observation of removal torque values of porous titanium implants compared to smooth titanium implants. Materials and methods: Twenty porous titanium implants (3.2mm in diameter and 8mm in length) were manufactured by powder technology using commercially pure titanium powder of ≤75um particles size, with polyvinyl alcohol powder of 212-300um particle size, as a space holder, by volume ratio (70:30) % respectively. The mixed powder was compacted using punch and die set -specially designed for this study –under 20 bar then sintering at 900 ºC by the use of argon gas. Twenty smooth titanium implants were prepared of (3.2mm in diameter and 8mm in length) by lathing of commercially pure titanium rod as a control group. The implants were examined by X-ray diffraction (XRD) and scanning electron microscope (SEM), as well as estimation of porosity percentage. For each tibia of the 20 white New Zealand rabbits, one implant of each type (one porous in right, and the smooth in left tibia), were inserted through surgical procedure carried under serial condition. Mechanical test was performed to evaluate the bone-implant interface, after (2 and 6 weeks) healing periods . Results: Porous implants were obtained successfully by powder technology with 52% porosity and pore size 210um 17±. The porous implant showed significantly higher removal torque values when compared to smooth implants at the two different intervals of examination (2,6 weeks) , this proved to be statistically highly significant, also a highly significant difference was noticed for the means of the torque removal values in the same group at different implantation , with no evidence of clinical features of inflammatory reaction with both . Conclusions: Powder technology seemed to be particularly advantageous in fabrication of porous titanium. Porous implant show an increasing bone ingrowth compared with the smooth type represented by higher removal torque for both healing periods (2, 6) weeks . Key words: Porous titanium implant, powder technology, removal torque test.
Silybum marianum, from which silymarin (SM) is extracted, is a medicinal herb. In the Biopharmaceutics Classification System, it is of the class II type, meaning it is almost completely insoluble in water. It has a number of therapeutic properties, including anti-inflammatory as well as properties that promote wound healing.
This research target is to promote the dissolution and solubility of SM by employing a technique called solid dispersion and then incorporating the formula of solid dispersion into a topical gel that can be used for wound healing.
Solid dispersion is a technique used to enhance solubility and dissolve pharmaceuticals that are not water-soluble. This method is widely used because of its low cos
... Show MoreThe deposition process and investigation of the physical properties of tungsten trioxide (WO3) thin films before and after gamma irradiation are presented in this paper. The WO3 thin films were deposited, using the pulse laser deposition technique, on glass substrates at laser energies of 600mJ and 800mJ. After deposition, the samples were gamma irradiated with Co60. The structural and optical properties of polycrystalline WO3 thin films are presented and discussed before and after 5kGy gamma irradiation at the two laser energies. X-ray diffraction spectra revealed that all the films consisted of WO3 crystallized in the triclinic form; the dislocation density and lattice strain increased with the absorbed dosage of gamma
... Show MoreThis study was aimed to assess the efficiency of N.oleander to remove heavy metals such as Copper (Cu) from wastewater. A toxicity test was conducted outdoor for 65-day to estimate the ability of N.oleander to tolerate Cu in synthetic wastewater. Based on a previous range-finding test, five concentrations were used in this test (0, 50, 100, 300, 510 mg/l). The results showed that maximum values of removal efficiency was found 99.9% on day-49 for the treatment 50 mg/l. Minimum removal efficiency was 94% day-65 for the treatment of 510 mg/l. Water concentration was within the permissible limits of river conservation and were 0.164 at day-35 for the 50 mg/l treatment, decreased thereafter until the end of the observation, and 0.12 at d
... Show MoreRemoval of direct blue dye by electrocoagulation method has been investigated using aluminum electrode in a bench-scale electrochemical system. Current density, NaCl concentration, electrocoagulation time, and dye concentration has been studied as effecting parameters in color removal efficiency. Increasing of current density will increase the color removal efficiency and energy consumption as well. While increasing NaCl concentration increase the color removal efficiency but it decrease energy consumption. High dye concentration is needed for extra electrocaogolation time to reach the same efficiency that obtained with low dye concentration .With current applied 0.35 amps. and NaCl concentration of 2 g/l more
... Show MoreThis research aims at investigating pupils’ ability in using discourse markers which are identified in the English textbooks of secondary schools. Four texts are chosen from third intermediate class. The four texts are short stories of different topics.
This research hypothesizes that there are no statistical significant differences among Iraqi intermediate pupils’ ability in using textual
... Show More