Background: It may be an important prospective clinical use of manufacturing of porous implant for clinical situations, such as cases of limitation in bone height, low bone density .The small segment of porous implant an effective osseointegration allows increasing in contact area provided for small segmented porous provided by its surface configuration. This study was done to Fabricate porous titanium implants by powder technology, as well as the observation of removal torque values of porous titanium implants compared to smooth titanium implants. Materials and methods: Twenty porous titanium implants (3.2mm in diameter and 8mm in length) were manufactured by powder technology using commercially pure titanium powder of ≤75um particles size, with polyvinyl alcohol powder of 212-300um particle size, as a space holder, by volume ratio (70:30) % respectively. The mixed powder was compacted using punch and die set -specially designed for this study –under 20 bar then sintering at 900 ºC by the use of argon gas. Twenty smooth titanium implants were prepared of (3.2mm in diameter and 8mm in length) by lathing of commercially pure titanium rod as a control group. The implants were examined by X-ray diffraction (XRD) and scanning electron microscope (SEM), as well as estimation of porosity percentage. For each tibia of the 20 white New Zealand rabbits, one implant of each type (one porous in right, and the smooth in left tibia), were inserted through surgical procedure carried under serial condition. Mechanical test was performed to evaluate the bone-implant interface, after (2 and 6 weeks) healing periods . Results: Porous implants were obtained successfully by powder technology with 52% porosity and pore size 210um 17±. The porous implant showed significantly higher removal torque values when compared to smooth implants at the two different intervals of examination (2,6 weeks) , this proved to be statistically highly significant, also a highly significant difference was noticed for the means of the torque removal values in the same group at different implantation , with no evidence of clinical features of inflammatory reaction with both . Conclusions: Powder technology seemed to be particularly advantageous in fabrication of porous titanium. Porous implant show an increasing bone ingrowth compared with the smooth type represented by higher removal torque for both healing periods (2, 6) weeks . Key words: Porous titanium implant, powder technology, removal torque test.
MR Younus, Al-A'DAB, 2011
The purpose of this paper, is to study different iterations algorithms types three_steps called, new iteration,
Imidacloprid is systemic insecticide (1-[(6-chloro-3-pyridinyl) methyl]-N-nitro-2-imidazolidinimine) and the world’s most widely used has significant efficacy against a broad variety of pests and a unique mode of action by using it spreader and irrigation. The persistence of this pesticide in the soil means that it causes environmental damage that must be cleaned up. In this study collected and identified the best bacteria isolate that breakdown imidacloprid from the Plant Protection Director in Baghdad, which has been using neonicotinoid pesticides for years in their own greenhouse for pest control. Using high-performance liquid chromatography HPLC to measuring the residual concentrations of imidacloprid in MSM media at a concentration o
... Show MoreSimple, sensitive and economical spectrophotometric methods have been developed for the determination of cefixime in pure form. This method is based on the reaction of cefixime as n-electron donor with chloranil to give highly colored complex in ethanol which is absorb maximally at 550 nm. Beer's law is obeyed in the concentration ranges 5-250 µg ml-1 with high apparent molar absorptivities of 1.52×103 L.mole-1. cm-1.
Pesticide biodegradation can be accomplished by the technique of bioremediation, which makes use of microorganisms’ ability to degrade pesticide residues. This study aimed to separate and identify imidacloprid-biodegradable from botanical fields soil of greenhouses in the Plant Protection Directorate /Ministry of Agriculture in Baghdad, which has been using imidacloprid pesticides for many years. Using high-performance liquid chromatography, residual imidacloprid concentrations in MSM medium at a concentration of 25 mg/L after 21 days were measured to identify the best degrading bacterial isolates. Isolate No.37 the best bacterial isolate was able to degrade 63% of imidacloprid. was
Leishmaniasis is endemic ofIraq in both cutaneous and visceral form. The available tools for diagnosis and detection of Leishmaniaare nonspecific and may interfere with other species. In this study, Polymerase Chain Reaction (PCR) has been used to identify Iraqi isolate of visceral leishmaniasis (MHOM/ IQ/2005/MRU15) which a previously diagnosed by classical serological tests. PCR amplificationwas carried out using species-specific primers of Leishmania donovani. Four primer pairs of mini-circle DNA and ITS-1 were used.13A/13B, which is used to identify Leishmaniaas a genus, NM12, LITSR/L5.8S and BHUL18S, were used to detect the sub species of L. donovani.The result ofPCR
... Show Moreِabstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission) was studied and found to be at 772 nm, several process parameters were such as concentration of TiO2 , and the effect of distance from nozzle tip to the grounded collector (gap distance). The result of the lower concentration of, the smaller the diameter of nanofiber is. Increasing the gap distance will affect nanofibers diameter.