Background: Oral squamous cell carcinoma is the most prevalent malignant neoplasm of the oral cavity which results from accumulated genetic and epigenetic alterations. It is not always inexorable and may be reversible if early intervention in the process can occur to prevent further genetic mutation and disease progression. The FHIT gene is a tumor suppressor gene located in FRA3B region which is the most active common fragile site, where DNA damage leading to aberrant transcripts and translocations frequently occur. The WWOX is a tumor suppressor gene that plays a central role in tumor suppression through transcriptional repression and apoptosis, with its apoptotic function the more prominent of the two. This study aimed to evaluate and compare the immunohistochemical expression of FHIT and WWOX in normal oral mucosa, oral epithelial dysplasia and oral squamous cell carcinoma and to correlate the expression of the mentioned markers with the clinicopathological features and to show the expression of studied markers with each other. Materials and methods: Fifty formalin-fixed, paraffin embedded tissue blocks (10 cases of normal oral mucosa, 19 cases of oral epithelial dysplasia, and 21 cases of oral squamous cell carcinoma) were included in this study. Immunohistochemical staining was performed using anti FHIT polyclonal antibody, and anti WWOX polyclonal antibody. Results: Positive IHC of FHIT was detected with high score in all cases of NOM, 16 cases (84%) of OED and 18 cases (86%) of OSCC. For WWOX expression positive IHC detected with high score in all cases (100%) of NOM, 14 cases (74%) of OED and 15 cases (71%) of OSCC. There was statistically highly significant correlation of both markers in OED and non significant correlation in OSCC, with significant differences among studied groups. Conclusions: These results signifying both markers cooperative tumor suppressive role and potential pathological transition from normal oral mucosa to dysplastic epithelium and subsequently cause malignant oral lesions.
The reinforced fiberglass in cement slurry reflects the effect on its properties compared to usual additives. Fiberglass is typically used in cement slurry design for one or another of the following goals: (Earth earthquake, bearing storage, and with differential stresses, to enhance cement durability and increase its compressive strength). The main goal is to use glass fiber and ground fiberglass to improve the tensile strength and moderate compressive strength significantly. On the other hand, the use of glass fibers led to a slight increase in the value of thickening time, which is a desirable effect. Eleven glass fiber samples and milled glass fiber were used to show these materials' effect on Iraqi cement with (0.125, 0.25, 0.5
... Show MoreCultivation of the green seaweed Enteromorpha compressa was performed under natural laboratory spring environmental conditions of temperature, light intensity and photoperiod to study the salinity tolerance of this intertidal green macroalga. Cultivation was carried out under artificial seawater (ASW) of different concentrations (18, 35, 53 and 106 g/l sea salt) compared to the control using natural seawater (NSW). Growth rate and pigment content of the cultivated alga were recorded at regular intervals during the experimental duration. Antioxidant activity of the crude ethanolic extract and its fractions (petroleum ether, chloroform, ethyl acetate and acetone) was performed against DPPH radical scavenging assay and compared to
... Show MoreBackground: White spot lesions (WSLs) are subsurface enamel demineralization manifested as white opacities which had an esthetic problem. The purpose of this in-vitro study was to evaluate the lesion depth improvement of WSLs following application of fluoride varnish, tooth mousse and resin infiltration (ICON). Materials and methods: Artificial WSLs were created on 120 premolar teeth using demineralization solution with pH (4-4.5). Samples randomly allocated into four groups; fluoride varnish, tooth mousse, ICON and untreated group. Groups were discolored in Cola and orange juice for 24 hours. Teeth were ground sectioned by longitudinal cutting then these sections examined and photographed under stereomicroscope at 12X magnification then an
... Show MoreIn this study, the modified size-strain plot (SSP) method was used to analyze the x-ray diffraction lines pattern of diffraction lines (1 0 1), (1 2 1), (2 0 2), (0 4 2), (2 4 2) for the calcium titanate(CaTiO3) nanoparticles, and to calculate lattice strain, crystallite size, stress, and energy density, using three models: uniform (USDM). With a lattice strain of (2.147201889), a stress of (0.267452615X10), and an energy density of (2.900651X10-3 KJ/m3), the crystallite was 32.29477611 nm in size, and to calculate lattice strain of Scherrer (4.1644598X10−3), and (1.509066023X10−6 KJ/m3), a stress of(6.403949183X10−4MPa) and (26.019894 nm).
The ceramic compound Mg1-xSixAl2O4 (x= 0, 0.1, 0.2, 0.3, 0.4) was prepared from nano powder of Al2O3 and MgO doped with Nano powder of SiO2 at different molar ratios. The specimens were prepared by standard chemical solid reaction technique and sintered at 1450 oC. Structure of the specimens was analyzed by using X-ray diffraction (XRD). The X-ray patterns of the specimens showed the formation of pure simple cubic spinel structure MgAl2O4 phase with space group of ̅ . The average grain size and surface topology were studied by atomic force microscopy. The results showed that the average grain size was about 73-90 nm. The DC electrical properties of the specimen were measured. The apparent density was found to increase and the porosity a
... Show MoreEffect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.
BACKGROUND: Volar Barton’s fracture is a shearing mechanism of injury that results in fracture and subluxation of distal end radius in which volar rim of the distal radius is displaced with hand and carpus. Open reduction and volar plate fixation ensure more stable change of displacement, preservation of reduction, and early mobilization. AIM: This study aims to assess the functional and radiological outcome results of volar Barton’s fracture treated by volar buttress plate using the demerit points system of Gartland and Werley. PATIENTS AND METHODS: This study is a prospective descriptive observational study on 32 patients who were treated with ORIF by volar buttress plate for isolated volar Barton’s fractures between Fe
... Show MoreSome transition metal ions (Cr +3, Co+2 , Ni+2,Cu+2, Zn+2,Ag + ,Cd+2 ) complexes of [(N, N- - Bis(2- hydroxy ethyl) Glycine] (Bicine) have been synthesized and characterized by FTIR ,UV-Visble spectroscopy, atomic absorption, magnetic susceptibility, conductivity measurements and study of the nature of the complexes formed in ethanolic solution following the moleratio method. From the results obtained the following general formola have been given for the prepared complexes [M m+ (Bicine)n]. XH2O
Oil is considered the most important source for providing the funds for the national economic sectors. The revenues of oil constitute %95 of the GPD. Therefore, the development of the remaining sectors depend on oil..
The Iraqi Oil Marketing Organization (SOMO) depended on the a unified price for all the buyers, That may not reflect the real value of market and did not contribute in marketing the type of heavy oil. Then, to what extent had SOMO been able to market the light and heavy crude oil in a way that contains the expected increase in the crude oil production.