Background: The bond strength of root canal sealers to dentin and gutta-percha seems to be an important property for maintaining the stability of root canal filling, which potentially influences both leakage and root strength. The objective of this, in vitro, study was to evaluate the shear bond strength of three different endodontic sealers (Gutta-Flow, AH Plus, Apexit Plus) to dentin, in the presence and absence of the smear layer and gutta percha. Material and Methods: After slicing off the occlusal 2mm of 60 extracted human maxillary premolar teeth, the exposed dentin served as the tested surfaces; the teeth were fixed with cold cure acrylic, and were divided into two groups according to the smear layer presence, group A without smear layer, when dentin surfaces were irrigated with EDTA 17% followed by distilled water then subdivided into 3 subgroups according to the type of sealer used; group B when dentin surfaces were washed with distilled water only, then subdivided into 3 subgroups. Thirty samples of gutta-percha were prepared and named as group C which was subdivided into 3 subgroups. Five mm long section of polyethylene tubes were placed on the dentin or gutta percha surfaces and filled with freshly mixed sealer. After one week, all the samples were tested for shear bond strength by the Instron Universal Testing Machine at a cross head speed of 0.5 mm/min. The data was calculated in MPa and was statistically analyzed Result: There was a highly significant difference in the shear bond strength (P < 0.05) in comparison among the tested groups, GuttaFlow showed non-significant difference in bond strength to dentin with and without smear layer, while AH Plus and Apexit Plus showed a high significant difference. Conclusions: AHPlus showed the highest shear bond strength in all the tested samples, while GuttaFlow was the least. Additionally, AH Plus and Apexit Plus shear bond strengths were affected by the smear layer removal, while GuttaFlow was not.
Background: Dental caries is one of the most significant problems in world health care. Restoring carious primary teeth is one of the major treatment goals for Children, and the light activated resin restoration materials like composite, resin-modified glass ionomer and polyacid-modified which was introduced in dentistry in 1970, widely used in clinical dentistry but its application increased dramatically in recent years because of its biocompatibility, color matching, good adhesive properties of its resemblance in physical and mechanical aspects to tooth. The aim of this study: To evaluate the microleakage of Polyacid-Modified Composite resin Compared to Flowable Hybrid Composite and Resin-Modified Glass ionomer cement. Materials and me
... Show MoreBackground: The bond strength of root canal sealers to dentin was important for maintaining the integrity of the seal in root canal filling in both static and dynamic situations. In a static situation, it should eliminate any space that allowed the percolation of fluids between the filling and the wall while in a dynamic situation; it was needed to resist dislodgement of the filling during subsequent manipulation. Materials and Methods: Forty mandibular premolars were selected for this study. All canals were instrumented using ProTaper rotary instruments. Instrumentation was done with copious irrigation of 5.25% sodium hypochlorite. Roots were randomly divided into four groups according to the type of cleaning and method of root canal irrig
... Show MoreCIGS nanoink has synthesized from molecular precursors of CuCl, InCl3, GaCl3 and Se metal heat up 240 °C for a half hour in N2-atmosphere to form CIGS nanoink, and then deposited onto substrates of soda-lime glass (SLG). This work focused on CIGS nanocrystals, indicates their synthesis and applications in photovoltaic devices (PVs) as an active light absorber layers. in this work, using spin-coating to deposit CIGS layers (75 mg/ml and 500 nm thickness), without selenization at high temperatures, were obtained up to 1.398 % power conversion efficiency (PCE) at AM 1.5 solar illumination. Structural formations of CIGS chalcopyrite structure were studied by using x ray diffraction XRD. The morphology and composition of CIGS were studied using
... Show MoreIn this paper, an experimental study was conducted to enhance the thermal performance of a double-pass solar air heater (SAH) using phase change material (PCM) for thermal storage at climatic conditions of Baghdad city - Iraq. The double-pass solar air heater integrated with thermal storage system was manufactured and tested to ensure that the air heating reserved after the absence of the sun. The rectangular cavity filled with paraffin wax was used as a latent heat storage and incorporated into the lower channel of solar air heater. Experiments were carried out to evaluate the charging and discharging characteristics of two similar designed solar air collectors with and without using phase change material at a constant
... Show MoreBackground: Maxillary first premolar with wide MOD cavity more susceptible to fracture. The aim of this study was to assess the influence of cavity design for cusp coverage on the fracture resistance of weakened maxillary first premolar restored with CAD/CAM hybrid ceramic versus nanohybide composite. Materials and Methods: Fifty six intact maxillary first premolars of approximately comparable sizes were divided into seven groups eight for each: Group A: Intact teeth (control group); Group B: teeth prepared for MOD inlay; Group C: teeth prepared for MOD onlay covering the lingual cusp; Group D: teeth prepared for MOD covering buccal and lingual cusps ,the previous three groups indirectly restored with nanohybrid composite (3M ESPE Z 250 X
... Show MoreBackground: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CA
... Show MoreThis paper presents the results of investigating the vibrational characteristics of oblate dish with and without framed structure . A finite element method, was applied to the dynamic analysis of oblate spheroidal shell. Different types of elements were considered in one dimension and two dimensions. It was found that the natural frequencies of oblate shells had two types of behavior against increasing the shell thickness and eccentricity, which are the membrane mode and bending mode –Since – the membrane modes natural frequencies tend to increase with the increasing the eccentricity of oblate, while the bending modes natural frequencies decrease with the increasing the eccentricity till reach the optimum eccentricity.
... Show More
Background:: Infertility is a very common condition affecting approximately 13-14% of couples in the reproductive age. In general population; about 85% of couples have achieved conception within a year. Intrauterine insemination is one of the procedure which have a role in the treatment of infertile couple.Objectives:is to confirm that the use of ovulation induction in the course of intrauterine insemination elevates the pregnancy success rate.Method:This study had been conducted between December 2013 till December 2014 in AL-Elwiyah maternity hospital and AL-Samaraii hospital / Baghdad.On history and clinical examination; the chosen couple had the following criteria; primary infertility for more than one year, no previous IUI trials, hu
... Show MoreNaturally available products have been used widely for centuries in handling human disease. The present study aimed to determine the effect of aluminum potassium sulfate addition into the soft liner on tensile strength and peel bond strength. The effect of aluminum potassium sulfate evaluated by two methods, first one include incorporation of KAL (SO4)2 into soft liner monomer in concentration (2%,3% by wt.) while the second method include immersion of soft liner specimens in solution of KAL(SO4)2 in concentration(5%,10% percent) during time periods (0,10 minutes). In conclusions, the results of current study encourage use KAL (SO4)2 within soft liner material