Background: Adjustment of any premature occlusal contact of any zirconia restoration requires its polishing or glazing in order to restore the smoothness of the restoration. The objective of this in vitro study was to evaluate the effects of different polishing systems and glazing on the surface roughness of full-contour zirconia. Material and methods: Forty disks (diameter: 8 mm, thickness: 6.4 mm) were prepared from pre-sintered full-contoured zirconia block; they were colored and sintered in a high-temperature furnace at 1500˚C for 8 hours. The specimens were then leveled and finished using grinding and polishing machine and adjusted using diamond disk. The specimens were then randomly divided into four groups (n=10), group I involves samples that were polished using (karat diamond polishing set, Vita zahnfabrik, Germany), group II involves samples that were polished with (zirconia polishing kit, SMEdent, Shanghai, China), group III involves samples that were polished with (OptraFine® diamond polishing system, Ivoclar Vivadent, Germany), while group IV involves samples that were glazed using glazing medium (VITA Akzent Glaze AKZ 25, Vita zahnfabrik, Germany). Surface roughness values (Ra) (in µm) of all the specimens were recorded at each stage of surface treatment of zirconia disks (leveling and finishing, adjustment of the samples and polishing / glazing) using surface roughness tester. Statistical analysis was carried out using one-way ANOVA and LSD tests. Results: The results showed that the glazing group recorded the lowest surface roughness mean value, followed by (OptraFine® polishing system), then (zirconia polishing kit) and finally (karat polishing set) which showed the highest mean of surface roughness. For all groups, there was a statistically very high significant difference of (Ra) value before and after adjustment of the samples. Moreover, there was a statistically very high significant difference in (Ra) value when comparing the adjusted samples with the polished and glazed ones. Karat polishing set group showed a statistically highly significant difference with zirconia polishing kit group (P<0.01). Both, karat polishing set and zirconia polishing kit groups showed a statistically very highly significant difference (P<0.001) with (OptraFine® polishing system) and glazing groups. On the other hand, no statistically significant difference was found between glazing and (OptraFine® polishing system) groups (P>0.05). Conclusions: Adjusting full-contour zirconia with diamond bur or disk resulted in a significant increase in (Ra) that necessitates its polishing or glazing to restore the surface smoothness. Furthermore, both glazing and OptraFine® polishing system provided the best surface smoothness, so glazing can be substituted with chairside polishing using OptraFine® polishing system.
Vascular patterns were seen to be a probable identification characteristic of the biometric system. Since then, many studies have investigated and proposed different techniques which exploited this feature and used it for the identification and verification purposes. The conventional biometric features like the iris, fingerprints and face recognition have been thoroughly investigated, however, during the past few years, finger vein patterns have been recognized as a reliable biometric feature. This study discusses the application of the vein biometric system. Though the vein pattern can be a very appealing topic of research, there are many challenges in this field and some improvements need to be carried out. Here, the researchers reviewed
... Show MoreWhile conservative access preparations could increase fracture resistance of endodontically treated teeth, it may influence the shape of the prepared root canal. The aim of this study was to compare the prepared canal transportation and centering ability after continuous rotation or reciprocation instrumentation in teeth accessed through traditional or conservative endodontic cavities by using cone-beam computed tomography (CBCT).
Forty extracted intact, matured, and 2-rooted human maxillary first premolars were selected for this
In this research, nanocomposites of poly(methyl methacrylate) (PMMA) and a mixture of nano silica (SiO2) and nano zirconia (ZrO2) were prepared in different weight percentages of the nano fillers to improve some of the properties of PMMA resin to be used as a denture base material. The nano filles were surface modified with a coupling agent and added to the PMMA in different amounts. Impact strength, transverse strength, hardness and roughness were tested for both control and experimental groups. The results indicate that PMMA/silica/zirconia nanocomposites, prepared with 5% by weight of both types of fillers, had a slight increase in impact s
Background: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three
... Show MoreBackground: The aim of this study was to evaluate the effect of thermo cycling and different pH of artificial saliva (neutral, acidic, basic) on impact and transverse strength of heat cure acrylic resin reinforced of with 5% silanated ZrO2 nano fillers. Materials and methods: 120 samples were prepared, 60 samples for impact strength test and another 60 samples for transverse strength test, for each test, samples were divided into two major groups (before and after thermo cycling), then each of these major groups were further subdivided into 3 subgroups according to the pH of prepared artificial saliva (neutral, acidic, basic). Charpy impact device was used for impact strength test and Flexural device was used for transverse strength test. R
... Show MoreThis research studies the rheological properties ( plastic viscosity, yield point and apparent viscosity) of Non-Newtonian fluids under the effect of temperature using different chemical additives, such as (xanthan gum (xc-polymer), carboxyl methyl cellulose ( High and low viscosity ) ,polyacrylamide, polyvinyl alcohol, starch, Quebracho and Chrome Lignosulfonate). The samples were prepared by mixing 22.5g of bentonite with 350 ml of water and adding the additives in four different concentrations (3, 6, 9, 13) g by using Hamilton Beach mixer. The rheological properties of prepared samples were measured by using Fan viscometer model 8-speeds. All the samples were subjected to Bingham plastic model. The temperature range studi
... Show More