Background: This study was conducted to assess the effect of sonic activation and bulk placement of resin composite in comparison to horizontal incremental placement on the fracture resistance of weakened premolar teeth. Materials and method: Sixty sound human single-rooted maxillary premolars extracted for orthodontic purposes were used in this study. Teeth were divided into six groups of ten teeth each: Group 1 (sound unprepared teeth as a control group), Group 2 (teeth prepared with MOD cavity and left unrestored), Group 3 (restored with SonicFill™ composite), Group 4 (restored with Quixfil™ composite), Group 5 (restored with Tertic EvoCeram® Bulk Fill composite) and Group 6 (restored with Universal Tetric EvoCeram® composite using horizontal incremental layering technique). Standardized class II MOD cavity was prepared in all teeth except (group 1).After finishing the restorative procedure of each group according to the manufacturer's instructions, all teeth were stored in deionized distilled water in an incubator at 37°C for seven days.All specimens were subjected to compressive axial loading until fracturein a universal testingmachine.Specimens were examined by a stereomicroscope at a magnification of (20X) to evaluate the mode of fracture . Results: The results of this study revealed that the control group exhibited the highest fracture resistance compared to all prepared teeth groups (restored or unrestored) and the differences were statistically highly significant (P<0.01), except with group 3 (which was restored with SonicFill™ composite) where the difference was statistically significant only (P < 0.05).Additionally the results of this study revealed that the prepared unrestored teeth (Group 2) exhibited the lowest fracture resistance compared to all restored groups and the differences were statistically highly significant (P<0.01). Meanwhile, among the restored teeth groups, teeth restored with SonicFill™ composite (group 3) exhibited the highest fracture resistance as compared with all other restored groups and the difference was statistically highly significant (P<0.01). On the other hand, no statistically significant differences in fracture resistance were found among groups 4, 5 and 6, which were restored with Quixfil™ composite, Tetric EvoCeram® Bulk Fill composite and Universal Tetric EvoCeram® composite, respectively (P > 0.05). Group 3and Group 5 showed mostly mixed mode of failure, while Group 4 showed mostly adhesive mode of failure. On the other hand Group 6 teeth showed different modes of failure. Conclusions: SonicFill™ composite can be considered as a viable treatment modality for the restoration of weakened maxillary premolar teeth. On the other hand, the time-consuming incremental layering technique can be substituted with bulk filling, using bulk fill materials (Quixfil™ and Tetric EvoCeram® Bulk Fill) for reinforcement ofweakened maxillary premolars.
Gingivitis, the initial stage of periodontal disease, is characterised by inflammation driven by dental biofilm and associated with oxidative stress. Matcha tea, a powdered green tea rich in antioxidants, has shown potential health benefits. This study aimed to investigate the effect of Matcha tea consumption on clinical periodontal parameters and salivary antioxidant levels in patients with gingivitis.
A randomised controlled clinical trial was conducted with 41 participants diagnosed with gingivitis.
Neuron-derived neurotrophic factor [NENF], a human plasma neurotrophic factor, also increases neurotrophic activity in conjunction with Parkinson's disease-related proteins in Neudesin. Although Neudesin (neuron-derived neurotrophic secreted protein) is a member of the membrane-associated progesterone receptor (MAPR) protein subclass, it is not evolutionary related to the other members of the same family. The expression of Neudesin is found in both brain and spinal cord from embryonic stages to adulthood, as w Neudesin levels in Parkinson's patients with osteoporosis disease and Parkinson's patients without osteoporosis disease, as well as the relationship between Neudesin levels, Anthropometric and Clinical Features (Age, Gender, BMI) and
... Show MoreThe present work deals with five species of parasitic Hymenoptera belonging to Pteromalidae, Eupelmidae and Eurytornidae which have been reared from brachid beetles. A new species, Eurytoma irakensis is described and the species, Bruchocida orientalis Crawford is recorded for the first time from Iraq.
The adsorption of copper ions onto produced activated carbon from banana peels (with particle size 250 µm) in a single component system with applying magnetic field has been studied using fixed bed adsorber. The fixed bed breakthrough curves for the copper ions were investigated. The adsorption capacity for Cu (II) was investigated. It was found that 1) the exposure distance (E.D) and strength of magnetic field (B), affected the degree of adsorption; and 2) experiments showed that removal of Cu ions and accumulative adsorption capacity of adsorbent increase as the exposure distance and strength of magnetic field increase.
In this work, two groups of nanocomposite material, was prepared from unsaturated polyester resin (UPE), they were prepared by hand lay-up method. The first group was consisting of (UPE) reinforced with individually (ZrO2) nanoparticles with particle size (47.23nm). The second group consists of (UPE) reinforced with hybrid nanoparticles consisting of zirconium oxide and yttrium oxide (70% ZrO2 + 30% Y2O3) with particles size (83.98nm). This study includes the effect of selected volume fraction (0.5%, 1%, 1.5%, 2%, 2.5%, 3%) for both reinforcement nano materials. Experimental investigation was carried out by analyzing the thermo-physical properties like thermal conductivity, thermal diffusivity and specific heat for the polymeric composit
... Show MoreThis study is concerned with the effect of adding two kinds of ceramic materials on the mechanical properties of (Al-7%Si- 0.3%Mg) alloy, which are zirconia with particle size (20μm > P.S ≥ 0.1μm) and alumina with particle size (20μm > P.S ≥ 0.1μm) and adding them to the alloy with weight ratios (0.2, 0.4, 0.6, 0.8 and 1%). Stirring casting method has been used to make composite material by using vortex technique which is used to pull the particles to inside the melted metals and distributed them homogenously.
After that solution treatment was done to the samples at (520ºC) and artificial ageing at (170ºC) in different times, it has been noticed that the values of hardness is increased with the aging time of the o
... Show More