Background: This study was conducted to assess the effect of sonic activation and bulk placement of resin composite in comparison to horizontal incremental placement on the fracture resistance of weakened premolar teeth. Materials and method: Sixty sound human single-rooted maxillary premolars extracted for orthodontic purposes were used in this study. Teeth were divided into six groups of ten teeth each: Group 1 (sound unprepared teeth as a control group), Group 2 (teeth prepared with MOD cavity and left unrestored), Group 3 (restored with SonicFill™ composite), Group 4 (restored with Quixfil™ composite), Group 5 (restored with Tertic EvoCeram® Bulk Fill composite) and Group 6 (restored with Universal Tetric EvoCeram® composite using horizontal incremental layering technique). Standardized class II MOD cavity was prepared in all teeth except (group 1).After finishing the restorative procedure of each group according to the manufacturer's instructions, all teeth were stored in deionized distilled water in an incubator at 37°C for seven days.All specimens were subjected to compressive axial loading until fracturein a universal testingmachine.Specimens were examined by a stereomicroscope at a magnification of (20X) to evaluate the mode of fracture . Results: The results of this study revealed that the control group exhibited the highest fracture resistance compared to all prepared teeth groups (restored or unrestored) and the differences were statistically highly significant (P<0.01), except with group 3 (which was restored with SonicFill™ composite) where the difference was statistically significant only (P < 0.05).Additionally the results of this study revealed that the prepared unrestored teeth (Group 2) exhibited the lowest fracture resistance compared to all restored groups and the differences were statistically highly significant (P<0.01). Meanwhile, among the restored teeth groups, teeth restored with SonicFill™ composite (group 3) exhibited the highest fracture resistance as compared with all other restored groups and the difference was statistically highly significant (P<0.01). On the other hand, no statistically significant differences in fracture resistance were found among groups 4, 5 and 6, which were restored with Quixfil™ composite, Tetric EvoCeram® Bulk Fill composite and Universal Tetric EvoCeram® composite, respectively (P > 0.05). Group 3and Group 5 showed mostly mixed mode of failure, while Group 4 showed mostly adhesive mode of failure. On the other hand Group 6 teeth showed different modes of failure. Conclusions: SonicFill™ composite can be considered as a viable treatment modality for the restoration of weakened maxillary premolar teeth. On the other hand, the time-consuming incremental layering technique can be substituted with bulk filling, using bulk fill materials (Quixfil™ and Tetric EvoCeram® Bulk Fill) for reinforcement ofweakened maxillary premolars.
Water contamination is a pressing global concern, especially regarding the presence of nitrate ions. This research focuses on addressing this issue by developing an effective adsorbent for removing nitrate ions from aqueous solutions. two adsorbents Chitosan-Zeolite-Zirconium (Cs-Ze-Zr composite beads and Chitosan-Bentonite-Zirconium Cs-Bn-Zr composite beads were prepared. The study involved continuous experimentation using a fixed bed column with varying bed heights (1.5 and 3 cm) and inlet flow rates (1 and 3 ml/min). The results showed that the breakthrough time increased with higher bed heights for both Cs-Ze-Zr and Cs-Bn-Zr composite beads. Conversely, an increase in flow rate led to a decrease in breakthrough time. Notab
... Show MoreObjective: The present work was undertaken to investigate the impact of sub inhibitory concentration of gentamicin on hla gene expression in methicillin resistant Staphylococcus aureus isolates. Methods: The bacterial isolates used in this study represent 33 MRSA strains, previously isolated form patients visiting several hospitals in Baghdad. Gentamicin, vancomycin, and oxacillin MIC were determined using broth dilution method. Microtiter plate method was adopted to investigate the biofilm forming capacity. Alpha hemolysin was detected by culturing MRSA isolates on rabbit blood agar. Furthermore, hla gene was detected in MRSA isolates using conventional PCR technique; while, qRT-PCR method was performed to assay the hla expression in plank
... Show MoreThe dielectric constant of most polymers is very low; the addition of TiO2 particles into the polymers provides an attractive and promising way to reach a high dielectric constant. Polymer-based materials with a high dielectric constant show great potential for energy storage applications. Four samples were prepared, one of them was polyurethane (PU) and the other were PU with different weight percent (wt %) of TiO2 (0.1, 0.2, 0.3) powder AFM test was used to distinguish the nanoparticles. The result shows that the most shape of these nanoparticles are spherical and the roughness average is 0.798 nm. The dielectric properties were measured for all samples before and after the exposure to the UV radiation. The result illustrates that the
... Show More200 samples collected Adrar of patients with urinary tract infection were investigating the types of bacteria most local isolates showed high resistance to antibiotics penicillin c ??????? Amoxicillin Beracelin
The nanostructured MnO2 /carbon fiber (CF) composite electrode was prepared using the anodic electrodeposition process. The crystal structure and morphology of MnO2 particles were determined with X-ray diffraction and field-emission scanning electron microscopy. The electrosorptive properties of the prepared electrode were investigated in the removal of cadmium ions from aqueous solution, and the effect of pH, cell voltage, and ionic strength was optimized and modeled using the response surface methodology combined with Box–Behnken design. The results confirm that the optimum conditions to remove Cd(II) ions were: pH of 6.03, a voltage of 2.77 V, and NaCl concentration of 3 g/L. The experimental results showed a good fit for the Freundli
... Show MoreABSTRACT Background: Bracket rebonding is a common problem in orthodontics which may result in many drawbacks. The aims of this study were to evaluate the effects of application of two enamel protective agents “Icon†and “ProSeal†on shear bond strength before and after rebonding of stainless steel orthodontic brackets using conventional orthodontic adhesive and to assess the site of bond failure. Materials and methods: Fifty sound extracted human upper first premolar teeth were selected and randomly divided into two equal groups; the first time bonding and the rebonding groups (n=30). Each group was subdivided into control, Icon and ProSeal subgroups. The enamel protective agents were applied after etching (precondi
... Show MoreBackground: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive res
... Show More