Background: This study report the corrosion behavior of commercially pure titanium and Ti-6Al-4V alloy samples without coating and with hydroxyapatite, partial stabilized zirconia and mixture of partial stabilized zirconia and hydroxyapatite coating and comparison between them through electrochemical polarization tests in 37 0 C Hank's solution. Materials and methods: Electrophoretic deposition technique (EPD) was used to achieve the coating from each one of three types of the coating materials (HAP, PSZ and mixture of 50% HAP and 50%PSZ) on Cp Ti and Ti-6Al-4V alloy samples. The electrochemical corrosion test was performed when samples were exposed to Hank's solution prepared in the laboratory and the polarization potential, corrosion rate and the open circuit potential of the samples were measured. Results: The results indicated that the corrosion rate is significantly higher for Ti-6Al-4V than for Cp Ti .The three types of coating significantly reduced the corrosion rate for Cp Ti while did not for Ti-6Al-4V alloy .After coating the corrosion rate for Ti-6Al-4V remained significantly higher than the coated Cp Ti samples .The open circuit potential (OCP) for both Cp Ti and Ti-6Al-4V samples was in the following sequence PSZ > HAP> mixture of HAP and PSZ >uncoated. Conclusions: Cp Ti showed less corrosion rate than Ti-6Al-4V alloy with and without coating .Coating significantly decreased the corrosion rate of Cp Ti but did not for Ti-6Al-4V alloy.
Background: Coated archwires have been introduced to improve esthetics during orthodontic treatment. Theaim of the present study was to evaluate and compare the load–deflection characteristics and force levels of six brands of coated nickel titanium orthodontic archwires using palatal and gingival deflection. Materials and methods: Ten round wires (0.016 inch) and ten rectangular wires (0.019x0.025 inch) were obtained from each of six brands (G&H, Opal, Ortho Technology, Dany, Hubit and Astar Companies). The load-deflection properties of these archwires were evaluated by the modified bending test usinga readymade dental arch model in both palatal and gingival directions at 37°C temperature using a universal material testing machi
... Show MoreThe behavior corrosion inhibition of aluminum alloy (Al6061) in acidic (0.1 M HCl) and saline (3.5% NaCl) solutions was investigated in the absence and the presence of expired diclofenac sodium drug (DSD) as a corrosion inhibitor. The influence of temperature and was studied using electrochemical techniques. In addition, scanning electron microscopy (SEM) was used to study the surface morphology. The results showed that DSD acted as a powerful inhibitor in acidic solutions, while a moderate influence was observed with saline one. Maximum inhibition efficiency was 99.99 and 83.32% in acidic and saline solutions at 150 ppm of DSD, respectively. Corrosion current density that obtained using electrochemical technique was increased with temperat
... Show MoreThe investigation of the effect of tempering on thermal analysis of
Al-Ti-Si alloy and its composites with MgO and SiC particles was
performed. Thermal analysis was performed before and after
tempering by DSC scan. Optical microscopy was used to identify the
phases and precipitations that may be formed in base alloy and
composites. X-ray diffraction test indicated that the Al3Ti is the main
phase in Al-Ti-Si alloy in addition to form Al5Ti7Si12 phase. Some
chemical reactions can be occurred between reinforcements and
matrix such as MgO.Al2O3 in Al-Ti/MgO, and Al4C3 and Al(OH)3 in
Al-Ti/SiC composite. X-ray florescence technique is used to
investigate the chemical composition of the fabricated specimens.
H
This research involves study effect of chloride ions in concentration range (0.01 – 0.50 mol.dm-3) on the corrosion behavior of Al-Zn alloy in basic media of 1x10-3 mol.dm-3 NaOH at pH=11 and four different temperatures in the range (298-313 K). Cathodic and anodic Tafel slopes (bc &ba) and transfer coefficients (αc & αa) were calculated and the results interprets according to the variation of the rate – determining steps. The results also indicate that the chloride ions are bonded chemically in the interface as an initial step of formation of different mixed oxohydroxy – and chloro complexes. Polarization resistance (Rp) is calculates
... Show MoreBackground:In this study,TiO2 layer was thermally grown as a diffusion barrier on CP Ti substrate prior to electrophoretic deposition of HA coatings, to improve the coating’s compatibility also macro and micro pores in nano Hydroxyapatite dual coatings were created and their effect on the bond strength between the bone and implant was evaluated. Materials and methods: Electrophoretic Deposition technique (EPD) was used to obtain coatings for each one of four types of Hydroxyapatite(HA)on CP Ti screws (micro HA, nano HA, dual nano HA with micro pores, dual nano HA with macro pores) where carbon particles used as fugitive material to be removed by thermal treatment to create porosity.For examination of the changes occurred on the subs
... Show MoreAim: To evaluate the commercial pure titanium disks that structuring by laser in two design (dot and groove) each one with three different laser scan (5, 15 and 25) and comparing with titanium surface that not subjected to any surface structuring (control) through measuring the wettability test and surface roughness test. Materials and methods: Structuring on the surface of the commercial pure titanium (CP Ti) disks was performed via using fiber laser CNC machine in two design (dot and groove) in three different laser scans (5, 15 and 25), then the structuring disks analyzed with the control group by atomic force microscope and water contact angle test. Results: The results of this study showed that the surface roughness and the wettability
... Show MoreBackground: Synthetic hydroxyapatite,(Ca10(PO4)6(OH2) can directly bond to bones without infection and fibrous encapsulation, thus is regarded as bioactive and biocompatible. The aim of the study was the estimation of microarchitecture bone parameters include bone mass (gm/cm2) cortical bone width (mm), thread width (mm), marrow space star volume analysis (V*m) and osteoblast, osteocyte cell number. Materials and methods: Ninety-six (96) commercially pure titanium CpTi) used in this study, (48) implants were coated with HA by dipping coating and (48) implants were used as control. They were inserted in (32) Newzland white rabbits and followed for 2 & 6 weeks. Mechanical torque removal test and histomorphometric analysis of bone microarchit
... Show MoreThe present study was conducted to evaluate the effect of different inhibitors on the corrosion rate of aluminum in 50% (v/v) ethylene glycol solution at 80°C and pH 8.0 in which the electrochemical technique of linear sweep voltammetry was employed to characterize each inhibitor function and to calculate the corrosion rate from Tafel plots generated by a computer assisted potentiostat.
It is found that both sodium dichromate and borax reduces the corrosion rate by polarizing the anodic polarization curve while sodium phosphate, potassium phosphate, and sodium benzoate reduces the corrosion rate by polarizing both the anodic and cathodic polarization curve.
When inhibitor concentration increases from I g/l up
... Show MoreAbstract
Corrosion-fatigue occurs by the combined actions of cyclic loading and corrosive environment. The effect of shot peening on cumulative corrosion-fatigue life of 1100-H12 Al alloy was investigated. Before fatigue testing, specimens were submerged in 3.5%NaCl solution for 71 days. Constant fatigue tests were performed with and without corrosive environment. Cumulative corrosion-fatigue tests were also carried out in order to determine the fatigue life before and after shot peening. The constant fatigue life was significantly reduced due to corrosive environment and the endurance fatigue limit was reduced by 13% compared with dry fatigue. In case of shot peening the cumul
... Show More