Background: The aim of the study was to investigate the effect of surface treatments of zirconia (grinding and sandblast with 50μm, 100 μm) on shear bond strength between zirconia core and veneering ceramic. Material and methods: Twenty-eight presintered Y-TZP ceramic specimens (IPS e.max ZirCAD, Ivoclar vivadent) were fabricated and sintered according to manufacturer’s instructions. The core specimens were divided randomly in to 4 groups, group 1: no surface treatment, group2: zirconia specimens were ground with silicon carbide paper up to1200 grit under water cooling, group3: zirconia specimens were ground and sandblast with 100 μm alumina, group 4: zirconia specimens were ground and sandblast with 50 μm alumina. Surface roughness of specimens were analyzed by surface profilometer, then veneering ceramic (IPS e.max ceramic, Ivoclar vivadent) was applied on the specimens& fired according to manufacturer’s instructions. All specimens were subjected to shear force in a universal testing machine at a crosshead speed of 1mm/min. The shear bond strength values were analyzed with one-way ANOVA; the fractured surfaces were examined with a stereo-microscope to observe the failure mode. Results: The mean of shear bond strength values in MPa were 24.75 for group 4, (17.72) for group 3, (17.68) for group2, (14.61) for group 1.The airborne-particle abrasion with 50μm group showed significantly higher bond strength than other groups. The airborne-particle-abraded with 100 μm group was not significantly different from grinding group. Conclusion: With limit of this study, the sandblast with 50 μm alumina was enhance the SBS between zirconia &veneering ceramic, and zirconia-veneering ceramic bonding is not only influenced by surface roughness. But also may be other factors.
ZSM-5 zeolite was synthesis under hydrothermal conditions at 175oC. The synthesis parameters have been investigated to find optimum synthesis method. Firstly, the crystallization time has been investigated to find the optimum crystallization time. Also, the ageing time was studied. The morphology, structure, and composition of the synthesized ZSM-5 zeolite were characterized using scanning electron microscopy (SEM), pH meter, viscometer, and X-ray powder diffraction (XRD). The bulk Si/Al ratio of ZSM-5 zeolite was in the range of 9.5—11.7. The synthesized ZSM-5 zeolite with appropriate ageing time could adjust crystal size and degree of the crystallinity. The crystal size of ZSM-5 zeolite obtained at an agei
... Show MoreNiO0.99Cu0.01 films have been deposited using thermal evaporation
technique on glass substrates under vacuum 10-5mbar. The thickness
of the films was 220nm. The as -deposited films were annealed to
different annealing temperatures (373, 423, and 473) K under
vacuum 10-3mbar for 1 h. The structural properties of the films were
examined using X-ray diffraction (XRD). The results show that no
clear diffraction peaks in the range 2θ= (20-50)o for the as deposited
films. On the other hand, by annealing the films to 423K in vacuum
for 1 h, a weak reflection peak attributable to cubic NiO was
detected. On heating the films at 473K for 1 h, this peak was
observed to be stronger. The most intense peak is at 2θ = 37
Premature failure in asphalt concrete pavement has been the main concern for pavement construction companies and engineers in recent years because of the large rise in traffic volume and loads and the temperature extremes in the summer and winter. The use of modifiers in asphalt concrete mixtures has attracted much attention to increase the performance and lifespan of pavements. As nanotechnology developed, several researchers concentrated on how these materials can help increase pavement serviceability by minimizing rutting and moisture damage. This study evaluates the Hydrated Lime (HL) effect by two methods (wet and dry hydrated lime) on the durability of the warm mix asphalt. The first method, HL, has been supplemented to the as
... Show MoreRecently, some of Iraq's newly constructed asphalt concrete pavements showed premature failures with significant negative impacts on roadway safety and the economy. Using Nano hydrated lime (NHL) in pavement construction could be one of the possible steps to improve pavement durability. This article discusses how NHL affects the durability of hot mix asphalt. NHL was added in two methods to the asphalt concrete mixture for the wearing course. The first is the dry method, i.e., on the aggregate, whereas the second is the wet addition method, i.e., to the bitumen. The percentages were tried for each additional method; 1, 2, and 3% by weight of aggregate for the dry method and 0.5, 1, and 1.5% by weight of asphalt concrete for the wet
... Show MoreThis study was conducted to determine the effects of concentration of hydrochloric acids, temperature, and time on the hydrolysis of soya proteins (defatted soya flour) by determining the value of total protein nitrogen concentration, and amino nitrogen concentration of protein, peptides, and amino acids, and then calculated the hydrolysis rate of proteins.
The variables of the conditions of hydrolysis process was achieved in this study with the following range value of tests parameter:
- Concentration of HCl solution ranged between 1-7 N,
- Hydrolysis temperature ranged between 35-95 °C, and
- The time of hydroly
The main objective of the present research is to conduct a thorough investigation into the impact of construction joints on the structural performance of reinforced concrete deep beams. This study involves a series of experimental tests and the use of advanced numerical analysis techniques to gain a deeper understanding of the behavior of these beams in the presence of construction joints. The experimental component incorporates analysis findings from both previous and current research. Specifically, six reinforced concrete deep beam specimens featuring horizontal and inclined construction joints were utilized as simply being supported with two-point loading. The test findings indicate that the presence of a horizontal construction
... Show MoreAbstract
Magnetic abrasive finishing (MAF) process is one of non-traditional or advanced finishing methods which is suitable for different materials and produces high quality level of surface finish where it uses magnetic force as a machining pressure. A set of experimental tests was planned according to Taguchi orthogonal array (OA) L27 (36) with three levels and six input parameters. Experimental estimation and optimization of input parameters for MAF process for stainless steel type 316 plate work piece, six input parameters including amplitude of tooth pole, and number of cycle between teeth, current, cutting speed, working gap, and finishing time, were performed by design of experiment
... Show MoreOne of the most important problems facing the world today is the energy problem. The solution was in finding renewable energy sources such as solar energy. The solar energy applications in Iraq is facing many problems . One of the most important problems is the accumulation of dust on the solar panels surface which causes decreasing its performance sharply. In the present work, a new technique was presented by using two-axis solar tracking system to reduce the accumulated dust on the solar panel surface and compared it with the fixed solar panels which installed at tilt angles 30° and 45°. The results indicated that the maximum losses of the output power due to accumulation of dust on the fixed solar panels is about 31.4% and 23.1% res