Background: The bonded orthodontic retainer constructed from multistrand wire and composite is an efficient esthetic retainer, which can be maintained long-term. Clinical failures of bonded orthodontic retainers, most commonly at the wire/composite interface, have been reported. This in vitro investigation aimed to evaluate the tensile forces of selected multistrand wires and composite materials that are available for use in the construction of bonded fixed retainers. Materials and Methods: The study sample includes 120 wires with three types of retainer wires (3 braided strands\ Orthotechnology, 8 braided strands\ G&H Orthodontics, 6 coaxial strands\ Orthoclassic wires), two types of adhesive (flowable\ Orthotechnology, non flowable\ G&H Orthodontics composites) and two thickness of the adhesive (1mm, 2mm). The samples were prepared for each composite in which a wire was embedded; then the composite was light cured for 40 seconds and the specimens were stored in artificial saliva at 37°C in the incubator for 24 hours. The ends of the wire were drawn up and tensile force was applied through Tinius-Olsen universal testing machine until the resin failed and the results were recorded in Newton (N). Results: Statistical analysis showed that there was a highly significant difference (P ≤ 0.01) among the mean values of tensile forces of the three types of retainer wires in each thickness of composite with exception of a non significant difference (P > 0.05) between (3 braided) and (8 braided) and a non significant difference (P > 0.05) between (3 braided) and (6 coaxial) in both thickness of composite, a highly significant difference (P ≤ 0.01) between the two thickness of both composite types in each wire type and a highly significant difference (P ≤ 0.01) between the two types of composite in each wire type of both thickness of composite. Conclusion: The result of this study revealed that the 8 braided strands retainer wire shows the highest values of tensile force among the tested retainer wires, the non flowable composite demonstrates a higher tensile force than the flowable composite and increasing the thickness of composite overlying the wire increased the force required to detach the wire from the composite.
Background: Ceramic veneers represent the treatment of choice in minimally invasive esthetic dentistry; one of the critical factors in their long term success is marginal adaptation. The aim of the present study is to evaluate the marginal gap of ceramic veneers by using two different fabrication techniques and two different designs of preparation. Material and methods: A typodont maxillary central incisor used in the preparation from which metal dies were fabricated, which were in turn used to make forty stone dies. The dies divided into four experimental groups, each group had ten samples: A1: prepared with butt-joint incisal reduction and restored with IPS e.max CAD, A2: prepared with overlapped incisal reduction and restored with IPS e.
... Show MoreChoosing an appropriate impression material is a challenge for many dentists, yet an essential component to provide an excellent clinical outcome and improve productivity and profit. The purpose of present study was to compare wettability, tear strength and dimensional accuracy of three elastomeric impression materials, with the same consistencies (light-body). Three commercially available light body consistency and regular set 3M ESPE Express polyvinylsiloxane (PVS), 3M ESPE Permadyne polyether (PE), and Identium (ID), impression materials were comparedTear strength test, contact angle test and linear dimensional accuracy were evaluated for three elastic impression material. Among the three experimental groups PE impression materia
... Show MoreBackground Obstructing dentinal tubules is a valuable approach for managing dentin hypersensitivity. Although various agents promote dentin remineralization, direct comparisons between theobromine, bioactive glass (BAG), and nano-hydroxyapatite (Nano-HAP) under simulated oral conditions remain limited. To fill this gap, this in vitro study aimed to evaluate and compare the effectiveness of these three treatments on exposed cervical dentin. The assessment focused on their chemical, morphological, and mechanical effects on dentin. Materials and methods Forty-eight human dentin slabs were obtained from the cervical portions of twelve sound premolar teeth. Baseline Raman spectroscopy and VMH tests were done to exclude outliers. All specimens we
... Show MoreBackground: The new concepts and technologies continue to change the dynamics of endodontic practices in the world. Rapid and significant changes in techniques, instrument design, and the type of metals used to manufacture endodontic instruments which have been made during the last few years in an attempt to overcome canal preparation errors. The purpose of this study is to measure and compare canal transportation and centering ability of Self Adjusting File with two rotary nickel-titanium (Ni-Ti) systems, ProTaper and BioRaCe at different levels. Material and Methods: Forty five distal roots of mandibular first molars with moderate curvature were selected using Schneider method. Roots were divided randomly into 3 groups of 15 each and were
... Show MoreThe research aims to conduct a comparative study between the events (800) m and (1500) m track in the types of muscular strength and to identify the differences between them among Iraqi sports club players. The sample represented the players participating in the Iraqi Athletics Championship for the period between (02/11/2023) and (04 /11/2023), and their number was (16) players (8) for each event, as the selection was made intentionally. The researchers used the descriptive approach to achieve the goal of the research and used the statistical package (SPSS) to process the data statistically. According to the results collected, it was found that there was superiority among the intermediate track players (800) m in explosive power and the s
... Show MoreBack ground: Glass ionomer materials lack resistance to wear and pressure and are susceptible to moisture during the initial stages of setting and dehydration. So this study was done to assess diametral tensile strength and microhardness of glass ionomer reinforced by different amounts of hydroxyapatite. Materials and methods: In this study a hydroxyapatite material was added to glass monomer cement at different ratios: 10%, 15%, 20%, 25% and 30% (by weight). The diametral tensile strength test described by the British standard specification for zinc polycarboxylate cement was used in this study and the microhardness test was performed using Vickers microhardness testing machine and the microhardness values were calculated and statistical c
... Show MoreBackground: The marginal seal is essential for sealant success because penetration of bacteria under the sealant might allow caries onset or progression. The aim of the present study was to estimate and compare the microleakage of pit and fissure sealant after various methods of occlusal surface preparation. Materials and methods: Thirty non-carious premolars extracted for orthodontic reasons were equally divided into three groups. In group one, occlusal fissures were opened with round carbide bur, in group two, occlusal surfaces of the teeth were cleaned with a dry pointed bristle brush and samples of group three were cleaned with a slurry of fine flour of pumice in water using rubber cup. Then fissures of all teeth were etched using 35% p
... Show More