Background: The bonded orthodontic retainer constructed from multistrand wire and composite is an efficient esthetic retainer, which can be maintained long-term. Clinical failures of bonded orthodontic retainers, most commonly at the wire/composite interface, have been reported. This in vitro investigation aimed to evaluate the tensile forces of selected multistrand wires and composite materials that are available for use in the construction of bonded fixed retainers. Materials and Methods: The study sample includes 120 wires with three types of retainer wires (3 braided strands\ Orthotechnology, 8 braided strands\ G&H Orthodontics, 6 coaxial strands\ Orthoclassic wires), two types of adhesive (flowable\ Orthotechnology, non flowable\ G&H Orthodontics composites) and two thickness of the adhesive (1mm, 2mm). The samples were prepared for each composite in which a wire was embedded; then the composite was light cured for 40 seconds and the specimens were stored in artificial saliva at 37°C in the incubator for 24 hours. The ends of the wire were drawn up and tensile force was applied through Tinius-Olsen universal testing machine until the resin failed and the results were recorded in Newton (N). Results: Statistical analysis showed that there was a highly significant difference (P ≤ 0.01) among the mean values of tensile forces of the three types of retainer wires in each thickness of composite with exception of a non significant difference (P > 0.05) between (3 braided) and (8 braided) and a non significant difference (P > 0.05) between (3 braided) and (6 coaxial) in both thickness of composite, a highly significant difference (P ≤ 0.01) between the two thickness of both composite types in each wire type and a highly significant difference (P ≤ 0.01) between the two types of composite in each wire type of both thickness of composite. Conclusion: The result of this study revealed that the 8 braided strands retainer wire shows the highest values of tensile force among the tested retainer wires, the non flowable composite demonstrates a higher tensile force than the flowable composite and increasing the thickness of composite overlying the wire increased the force required to detach the wire from the composite.
Background: Denture fracture is one of the most common problems encountered by the patients and prosthodontists. The objective of present study was to evaluate the transverse strength of nylon denture base resin repaired by using conventional heat polymerized, autopolymerized and visible light cure {VLC} resins, surface treatment that used for repair and adjustment of insufficient nylon denture bases and in case of addition of artificial teeth. As these corrective procedures are common chair side procedures in dental clinic. Materials and methods: One hundred twenty nylon specimens were prepared by using metal patterns with dimension of (65x10x2.5 mm) length, width, and thickness respectively for transverse strength test while for tensile b
... Show MoreThis study aimed to incorporate hydroxyapatite nanoparticles (nHA) or amorphous calcium phosphate nanoparticles (nACP) into a self-etch primer (SEP) to develop a simplified orthodontic bonding system with remineralizing and enamel preserving properties.
nHA and nACP were incorporated into a commercial SEP (Transbond™ plus) in 7% weight ratio and compared with the plain SEP as a control. Shear bond strengths (SBS), enamel damage, and adhesive remnant index (ARI) scores were evaluated at 24 h
This study aimed to incorporate hydroxyapatite nanoparticles (nHA) or amorphous calcium phosphate nanoparticles (nACP) into a self-etch primer (SEP) to develop a simplified orthodontic bonding system with remineralizing and enamel preserving properties.
nHA and nACP were incorporated into a commercial SEP (Transbond™ plus) in 7% weight ratio and compared with the plain SEP as a control. Shear bond strengths (SBS), enamel damage, and adhesive remnant index (ARI) scores were evaluated at 24 h
This study aims to investigate the adequacy of composite cellular beams with lightweight reinforced concrete deck slab as a structural unit for harmonic loaded buildings. The experimental program involved three fixed-ends supported beams throughout 2140 mm. Three concrete types were included: Normal Weight Concrete (NWC), Lightweight Aggregate Concrete (LWAC), and Lightweight Fiber Reinforced Aggregate Concrete (LWACF). The considered frequencies were (5, 10, 15, 20, 25, and 30) Hz. It was indicated that the harmonic load caused a significant influence on LWAC response (64% greater than NWC) and lattice cracks were observed, especially at 30 Hz. As for LWACF slab, no cracks appeared,
This research presents an experimental investigation on the influence of metakaolin replacement percentage upon some properties of different concrete types. Three types of concrete were adopted (self- compacted concrete, high performance concrete and reactive powder concrete) all of high sulphate (SO3) percentage from the fine aggregate weight, 0.75%. Three percentages of metakaolin replacement were selected to be studied (5, 7 and 10) %. Three types of concrete properties (compressive, flexural and splitting tensile strength) were adopted to achieve better understanding for the influence of adding metakaolin.. The output results indicated that the percentage of metakaolin had a different level of positive effect on the compressive strength
... Show MoreThe present work aimed to study the effect of Grave's disease on the different tissues and organs of the body by using Wayne Thyrotoxicosis Diagnostic Index (WTDI) and Basel Metabolic Index (BMI). To reach such aim, (35) patients were involved (25 females and 10 males). A control group of (15) healthy individuals (10 females and 5 males) was selected for comparison , as well as , the following: 1- Wayne Thyrotoxicosis Diagnostic Index (WTDI) applied on patient group and control group under the supervision of specialist medical team , this index include (19) sign and symptom , the appearance of one of them may be lead to the others. The sings and symptoms of the index appear only on the patients. There is no Significant di
... Show MoreIn this study, dead and live anaerobic biomass was used in biosorption of Pb(II), Cr(III) and Cd(II) ions from a synthetic wastewater. The biosorption was investigated by batch adsorption experiments. It was found that, the biosorption capacities were significantly affected by biosorbent dosage. The process follows Langmuir isotherm (regression coefficient 0.995, 0.99 and 0.987 for Pb(II), Cr(III) and Cd(II) ions, respectively, onto dead anaerobic biomass) model with uniform distribution over the biomass surface. The experimental uptake capacity was 51.56, 29.2 and 28 mg/g for Pb(II), Cr(III) and Cd(II), respectively, onto dead anaerobic biomass, compared with 35, 13.6 and 11.8 mg/g for Pb(II), Cr(III) and Cd(II), respectively, onto live
... Show MoreBackground: The microhardness of a composite resin is a vital parameter that is used to determine its clinical behavior. Measuring the microhardness of a composite resin has been used as an indirect method to assess its degree of conversion and extent of polymerization. The purpose of this in vitro study was to evaluate the effect of three curing distances (0, 2, and 4 mm) on the microhardness of the top and bottom surfaces of three types of flowable bulk-fill composite resins (smart dentin replacement, Opus bulk fill flow, and Tetric N). Material and method: Sixty-three specimens from the three types of composite resins (n=21) were fabricated using Teflon mold with a 4mm depth and a 5 mm internal diameter and cured for 20 seconds. For e