Background: Alterations in the microhardness and roughness are commonly used to analyze the possible negative effects of bleaching products on restorative materials. This in vitro study evaluated the effect of in-office bleaching (SDI pola office +) on the surface roughness and micro-hardness of four newly developed composite materials (Z350XT –nano-filled, Z250XT-nano-hybrid, Z250-mico-hybrid and Silorane-silorane based). Materials and methods: Eighty circular samples with A3 shading were prepared by using Teflon mold 2mm thickness and 10mm in diameter. 20 samples for each material, 10 samples for base line measurement (surface roughness by using portable profillometer, and micro-hardness by usingDigital Micro Vickers Hardness Tester), and 10 samples for after bleaching measurement. The appropriate bleaching procedure was performed on the top surface of test groups for 90 minutes total bleaching period. Then surface roughness and hardness were tested at the end of the duration. Statistical analysis was carried out using ANOVA, LSD and t-test. Results: There was a highly significant increase in surface roughness of all tested groups after bleaching. There is a highly significant increase in micro-hardness for Z250, there is decrease in Micro-hardness for siloraneand Z250xt and there is a non-significant increase in micro-hardness of Z350xt. Conclusion: bleaching has a negative effect on surface roughness of all the tested materials, as surface roughness increased after bleaching. Micro-hardness is a material dependent, there is different reaction to bleaching depending on the resin, load and size of the fillers used in the materials. Nano-filled composite is the material that has better performance than the other tested materials, as it is the material that has the least affection by bleaching.
Roughness length is one of the key variables in micrometeorological studies and environmental studies in regards to describing development of cities and urban environments. By utilizing the three dimensions ultrasonic anemometer installed at Mustansiriyah university, we determined the rate of the height of the rough elements (trees, buildings and bridges) to the surrounding area of the university for a radius of 1 km. After this, we calculated the zero-plane displacement length of eight sections and calculated the length of surface roughness. The results proved that the ranges of the variables above are ZH (9.2-13.8) m, Zd (4.3-8.1) m and Zo (0.24-0.48) m.
This study included prepared samples of epoxy reinforced by the novolac , aluminum , glass powder and epoxy reinforced by aluminum , glass powder and epoxy alone .They are used as reinforced materials of volum fraction amounting 40% . The mechanical properties inclouded ( tensile , compressive and wear) where the wear test inclouded different applied loads (5,10,15) . From the results showed the epoxy reinforced by aluminum and glass powder has higher compressive strength (56.91) Mpa and higher tensile strength (132.2) Mpa .But the epoxy alone has higher wear rate and the epoxy reinforced by aluminum and glass powder which have higher elasticity of modulus from the tensile test (315.7) Mpa
Reliability analysis methods are used to evaluate the safety of reinforced concrete structures by evaluating the limit state function 𝑔(𝑋𝑖). For implicit limit state function and nonlinear analysis , an advanced reliability analysis methods are needed. Monte Carlo simulation (MCS) can be used in this case however, as the number of input variables increases, the time required for MCS also increases, making it a time consuming method especially for complex problems with implicit performance functions. In such cases, MCS-based FORM (First Order Reliability Method) and Artificial Neural Network-based FORM (ANN FORM) have been proposed as alternatives. However, it is important to note that both MCS-FORM and ANN-FORM can also be time-con
... Show MoreAbstract
Magnetic abrasive finishing (MAF) is one of the advanced finishing processes, which produces a high level of surface quality and is primarily controlled by a magnetic field. This paper study the effect of the magnetic abrasive finishing system on the material removal rate (MRR) and surface roughness (Ra) in terms of magnetic abrasive finishing system for eight of input parameters, and three levels according to Taguchi array (L27) and using the regression model to analysis the output (results). These parameters are the (Poles geometry angle, Gap between the two magnetic poles, Grain size powder, Doze of the ferromagnetic abrasive powder, DC current, Workpiece velocity, Magnetic poles velocity, and Finishi
... Show MoreBackground: The demand for better esthetic during orthodontic treatment has increased nowadays, so orthodontists starting using esthetic arch wires, brackets and ligatures.Tooth colored brackets were introduced in different types of materials. Sapphire ceramic brackets are one type of esthetic brackets and their color stability remains the main concern for the clinicians and patients at the same time. The present study design to evaluate the effect of three different staining materials (pepsi, black tea and cigarette smoke) on the stainability of sapphire ceramic brackets bonded with three types of light cure orthodontic adhesives which include: Resilience, Enlight and Transbond. Materials and Methods: The sample consisted of three hundre
... Show MoreIn this work the interaction of plasma jet with water and hydrogen peroxide liquids used for assisted teeth bleaching by plasma jet had been study. A homemade plasma jet system was used. The plasma jet supply by 15 W electrical power generated by high voltage power supply of 9.6 kV peak to peak and frequency of 33 kHz .this power supply generate high electric field on electrodes that would be enough to ionize the argon gas. Some important agents were study such as the effect of the Ar gas flow rates on the length of the plasma jet, the influence of plasma jet on some properties of water and two hydrogen peroxide concentrations 25 % and 30 % like pH, conductivity and liquid temperature for different exposure time. The liquids temperature
... Show MoreBackground: Fracture of different types of acrylic denture base is a common problem associated with dental prosthesis. Studies suggested that the repair strength may be improved by several means including surface treatment with chemical agents. The aim of the study was to evaluate the effect of surface treatment with acrybond-bonding agent and monomer on fractured denture base in respect to transverse, tensile and shear bond strength and evaluation of the mode of failure by light microscope. Materials and methods: Two hundred seventy specimens were prepared and divided into 3 groups according to the material used (regular conventional, rapid simplified and high impact) heat cure acrylic. The specimen in each groups were prepared specificall
... Show MoreA particulate composite material was prepared by adding the Titanium dioxide (TiO2) with a particle size of (75-150) µm to Epoxy resin at weight percentage of (10%,20%,30%,40%,50%).The following some mechanical properties were studied,fracture toughness, hardness.casting preparation methods were used in this study includes preparing plate of matrix and composites. specimens were prepared according to ASTM for the Mechanical properties tests. After that Another samples were heat treated for three and six hour at 65C?. Fracture toughness (Kic) represent for stress intensity factor results were showed that the curve of three hours aging increases in fracture toughness (Kic) for composites but for six hours aging increases fracture tough
... Show MoreBackground: This study was conducted to assess the effects of various beverages on the shear bond strength of light-cured orthodontic composite used to bond stainless steel orthodontic brackets on human teeth and to determine the site of bonding failure of this material. Materials and Methods: Fifty extracted human premolars were selected and randomly divided into five equal groups each with 10 teeth according to the beverage type (Control, One Tiger, Milk, Green tea and Coffee). After bonding, the teeth were immersed in specific beverages for 5 minutes twice daily with equal intervening intervals then washed and stored in distilled water at 37º C for the reminder of the day. The process was carried out for 30 days. The samples were then
... Show More