Background: Alterations in the microhardness and roughness are commonly used to analyze the possible negative effects of bleaching products on restorative materials. This in vitro study evaluated the effect of in-office bleaching (SDI pola office +) on the surface roughness and micro-hardness of four newly developed composite materials (Z350XT –nano-filled, Z250XT-nano-hybrid, Z250-mico-hybrid and Silorane-silorane based). Materials and methods: Eighty circular samples with A3 shading were prepared by using Teflon mold 2mm thickness and 10mm in diameter. 20 samples for each material, 10 samples for base line measurement (surface roughness by using portable profillometer, and micro-hardness by usingDigital Micro Vickers Hardness Tester), and 10 samples for after bleaching measurement. The appropriate bleaching procedure was performed on the top surface of test groups for 90 minutes total bleaching period. Then surface roughness and hardness were tested at the end of the duration. Statistical analysis was carried out using ANOVA, LSD and t-test. Results: There was a highly significant increase in surface roughness of all tested groups after bleaching. There is a highly significant increase in micro-hardness for Z250, there is decrease in Micro-hardness for siloraneand Z250xt and there is a non-significant increase in micro-hardness of Z350xt. Conclusion: bleaching has a negative effect on surface roughness of all the tested materials, as surface roughness increased after bleaching. Micro-hardness is a material dependent, there is different reaction to bleaching depending on the resin, load and size of the fillers used in the materials. Nano-filled composite is the material that has better performance than the other tested materials, as it is the material that has the least affection by bleaching.
In this work, results from an optical technique (laser speckle technique) for measuring surface roughness was done by using statistical properties of speckle pattern from the point of view of computer image texture analysis. Four calibration relationships were used to cover wide range of measurement with the same laser speckle technique. The first one is based on intensity contrast of the speckle, the second is based on analysis of speckle binary image, the third is on size of speckle pattern spot, and the latest one is based on characterization of the energy feature of the gray level co-occurrence matrices for the speckle pattern. By these calibration relationships surface roughness of an object surface can be evaluated within the
... Show MoreCO2 laser (10.6 μm) is the most often used laser in the oral surgery due to its high absorption by water of the oral tissues. Several benefits of the use of CO2 laser have been reported for oral surgical procedures. This study aims to evaluate the effect of CO2 laser on soft and hard oral tissues (in vitro study). This study was done on fresh tissues from sheep’s head. CO2Surgical Laser with different operation modes was used; 0.2 mm spot size using different laser parameters on the tongue, and bone making holes, incisions and cutting. The depths and widths of holes and incisions were measured using endodontic file under magnification. The speed of incisions was calculated and the required time for cutting was measured using sport clo
... Show MoreIn vitro tests have been carried out to find out the efficacy of watery extracts of garlic Allium sativum and hot pepper Capsicum spp. against the trophozoites of Entamoeba histolytica cultivated in liver infusion agar media at 37 c . The doses of ( 0.01, 0.05 ,0.1, 0.5, 1 ml )of garlic and hot pepper watery extracts were added to certain number of E. histolotica trophozoits for exposure time of 24 hrs., the mortality percentage of trophozoites treated with garlic extract were ( 14.82 %, 31.05% ,46.16% , 64.29% , 92.7%) respectively , these percentages were very close to that obtained from the treatment with the hot peper extract which were (17.86%, 32% , 44% ,66.67% ,100%) respectively . Generally these results showed that the ga
... Show MoreThe wear behavior of alumina particulate reinforced A332 aluminium alloy composites produced by a stir casting process technique were investigated. A pin-on-disc type apparatus was employed for determining the sliding wear rate in composite samples at different grain size (1 µm, 12µm, 50 nm) and different weight percentage (0.05-0.1-0.5-1) wt% of alumina respectively. Mechanical properties characterization which strongly depends on microstructure properties of reinforcement revealed that the presence of ( nano , micro) alumina particulates lead to simultaneous increase in hardness, ultimate tensile stress (UTS), wear resistances. The results revealed that UTS, Hardness, Wear resistances increases with the increase in the percentage of
... Show MoreThis study is attempt to improve thermal isolation through measuring thermal conductivity composite of on polyester resin with fillers of (TiO2, ZnO, Acrylonitril, wood flour Coconut (Wf). The grain size of the fillers is 200 µm. The number of samples is (16) in addition to the virgin sample; these samples are prepared by cast molding method for polyester with filler volume fractions (5%, 10%, 15% and 20%). Shore hardness tests were used to measure the hardness and Lee disk method for thermal conductivity. The experimental results showed that the (20% ZnO) sample has the maximum value of thermal conductivity where (20% w.f) has minimum thermal conductivity .on the other hand (15% ZnO) sample give the maximum value of hardness where (20% w
... Show MoreOne of the most popular causes for implant infection is dental plaque bacteria. Previous studies have shown the bactericidal effect of CO2 laser irradiation on bacteria associated with soft tissue surrounding the implant materials. No published studies have examined the effect of irradiation by CO2 laser on Streptococcus oralis and Staphylococcus aureus.The aim of this study was to evaluate the bactericidal effect of CO2 laser on bacteria that are causing dental implant infections. This study was carried out on two isolates of bacterial species out of 25 samples, isolated from patients having soft tissue infections around the dental implant. These two pure isolates including Streptococcus oralis and Staphylococcus aureus were identified
... Show MoreBackground: The most common reason for re-making a maxillofacial prosthesis is the degradation of the mechanical properties of the silicone. Aim of this study: To assess some mechanical properties of VST-50F maxillofacial silicone reinforced with a composite of silicon dioxide nanoparticle and polyamide-6 microparticle before and after artificial aging. Material and Method: Preparing 240 samples tested for tear strength, tensile strength and elongation percentage, hardness, and roughness before and after aging. The Silicon dioxide was added in concentrations of 1% by weight and Polyamide-6 in the concentration of 0.25% and 0.5% by weight to the VST-50F RTV maxillofacial silicone. The one-way ANOVA and post hoc tests were used for inferentia
... Show MoreABSTRACT Background: This study measured the effects of three parameters pH value, length of immersion and type of archwire on metal ions released from orthodontic appliances. Materials and Methods: Ninety maxillary halves simulated fixed orthodontic appliances that were immersed in artificial saliva of different pH values (6.75, 5 and 3.5) during 28 day period. Three types of archwires were used: stainless steel, nickel titanium and thermal activated nickel titanium. The quantity of nickel and chromium ions was determined with the use of atomic force spectrophotometer while iron ions by spectrophotometer. Each orthodontic set was weighted two times, before the ligation and immersion in the artificial saliva and after 28 days at the end of
... Show More